journal article·2005-05

Effect of different mo contents on tensile and corrosion behaviors of CD4MCU cast duplex stainless steels

Younghwan Jang, Sangshik Kim, Jehyun Lee

Publisher page

Abstract

The tensile and corrosion behaviors of CD4MCU cast duplex stainless steels with different Mo contents of 0, 2, and 4 pct, respectively, were examined in the present study. The polarization and the in-situ slow-strain-rate (SSR) tests were conducted in a 3.5 pct NaCl+5 pct H2SO4 aqueous solution to quantify the resistances to pitting corrosion and stress corrosion cracking (SCC) with different Mo contents. The addition of Mo, which is a strong ferrite stabilizer, affected the microstructure of the present alloy and, eventually, the tensile and corrosion behaviors in a complex manner. The tensile properties of CD4MCU cast duplex stainless steel, for example, were found to be determined by the volume fraction of hard ferritic phase, the presence of the second precipitates of soft austenitic phase in the ferrite matrix, and the shape of the austenitic phase. The addition of 2 pct Mo was detrimental to the corrosion properties of CD4MCU cast duplex stainless steel due to the significant increase in the volume fraction of ferritic phase. With the addition of 4 pct Mo, however, the resistances to pitting corrosion and SCC recovered to those of the specimen without Mo. The relationship between the microstructural evolution and the tensile and corrosion behavior of CD4MCU cast duplex stainless steels with different Mo contents was discussed based on the micrographic and fractographic observations.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. J.H. Huang and C.J. Altstetter: Metall. Mater. Trans. A, 1995, vol. 26A, pp. 1079–85.10.1007/BF02670603 ↗
2. ASM Specialty Handbook Stainless Steels, J.R. Davis, ed., ASM INTERNATIONAL, Materials Park, OH, 1996, pp. 32–34.
3. H.D. Solomon and T.M. Devine, Jr.: in Duplex Stainless Steels, R.A. Lula, ed., ASM, Metals Park, OH, 1983, pp. 693–756.
4. J.I. Son, S.S. Kim, J.H. Lee, and B.H. Choi: Metall. Mater. Trans. A, 2003, vol. 34A, pp. 1617–25.10.1007/s11661-003-0307-6 ↗
5. J.I. Son, S.S. Kim, J.H. Lee, and B.H. Choi: J. Kor. Inst. Met. Mater., 2002, vol. 40, pp. 723–29.
6. Y.H. Park and Z.H. Lee: Mater. Sci. Eng. A, 2001, vol. 297, pp. 78–84.10.1016/S0921-5093(00)01263-6 ↗
7. J.I. Son, S.S. Kim, J.H. Lee, and B.H. Choi: J. Kor. Inst. Met. Mater., 2003, vol. 41, pp. 155–60.
8. J. Sakai, I. Matsushima, Y. Kamemura, M. Tanimura, and T. Osuka: in Duplex Stainless Steels, R.A. Lula, ed., ASM, Metals Park, OH, 1983, pp. 211–31.
9. C.J. Park, J.S. Kim, and H.S. Kwon: J. Kor. Inst. Met. Mater., 1999, vol. 37, pp. 1390–98.
10. S.B. Kim, K.W. Paik, and Y.G. Kim: Mater. Sci. Eng. A, 1998, vol. 247, pp. 67–74.10.1016/S0921-5093(98)00473-0 ↗
11. A. Poznansky, C.S. Nalbone, and J.D. Crawford: in Duplex Stainless Steels, R.A. Lula, ed., ASM, Metals Park, OH, 1983, pp. 431–44.
12. K. Sugimoto and Y. Sawada: Corr. Sci., 1977, vol. 17, pp. 425–45.10.1016/0010-938X(77)90032-4 ↗
13. C.R. Clayton and Y.C. Lu: J. Electrochem. Soc., 1986, vol. 133, pp. 2465–73.10.1149/1.2108451 ↗
14. M.U. Macdonald and D.D. Macdonald: J. Electrochem. Soc., 1989, vol. 136, pp. 961–67.10.1149/1.2096894 ↗
15. J.S. Kim, C.J. Park, and H.S. Kwon: Bull. Kor. Inst. Met. Mater., 1999, vol. 12, pp. 635–57.
16. Russel D. Kane: Slow Strain Rate Testing for the Evaluation of Environmentally Induced Cracking, ASTM, Baltimore, MD, 1993.