Effect of Phosphorus and Strontium Additions on Formation Temperature and Nucleation Density of Primary Silicon in Al-19 Wt Pct Si Alloy and Their Effect on Eutectic Temperature
Source abstract
Abstract
The influence of P and Sr additions on the formation temperature and nucleation density of primary silicon in Al-19 wt pct Si alloy has been determined, for small volumes of melt solidified at cooling rates ( dot{T} ) of ~0.3 and 1 K/s. The proportion of ingot featuring primary silicon decreased progressively with increased Sr addition, which also markedly reduced the temperature for first formation of primary silicon and the number of primary silicon particles per unit volume ( ar{N}v . ) When combined with previously published results, the effects of amount of P addition and cooling rate on ( ar{N}v ) are in reasonable accord with ( {{ar{N}v } mathord{left/ {vphantom {{ar{N}v } {dot{T}}}} ight. kern- ulldelimiterspace} {dot{T}}} = left( {pi / 6f} ight) 1/ 2 ) 109 [250 − 215 (wt pct P)0.17]−3, where ( ar{N}v ) is in mm−3, ( dot{T} ) is in K/s, and f is volume fraction of primary silicon. Increased P addition reduces the eutectic temperature, while increased Sr appears to generate a minimum in eutectic temperature at about 100 ppmw Sr.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Solidification and crystal growth phenomena · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. N. Tenekedjiev and J.E. Gruzleski: Cast Met., 1990, vol. 3 (2), pp. 96–105.10.1080/09534962.1990.11819026 ↗
2. J.L. Jorstad: AFS Trans., 1996, vol. 104, pp. 669–71.
3. R.J. Donahue: Adv. Mater. Proc., 2002, vol. 160 (2), p. 11.
4. J. Cissé, G.F. Bolling, and H.W. Kerr: Metall. Trans. B, 1975, vol. 6B, pp. 195–97.10.1007/BF02825695 ↗
5. M. Faraji, I. Todd, and H. Jones: J. Mater. Sci., 2005, vol. 40, pp. 6363–65.10.1007/s10853-005-3103-4 ↗
6. S. Terai: Sumitomo Met., 1958, vol. 10 (3), pp. 40–51.
7. P.B. Crosley and L.F. Mondolfo: AFS Trans., 1966, vol. 74, pp. 53–64.
8. G.A. Colligan and M.A. Gunes: AFS Trans., 1973, vol. 81, pp. 359–65.
9. N. Tenekedjiev, D. Argo, and J.E. Gruzleski: AFS Trans., 1989, vol. 97, pp. 127–36.
10. J. Chang, I. Moon, and C. Choi: J. Mater. Sci., 1998, vol. 33, pp. 5015–23.10.1023/A:1004463125340 ↗
11. W.J. Kyffin, W.M. Rainforth, and H. Jones: Mater. Trans., 2001, vol. 42, pp. 2098–2101.10.2320/matertrans.42.2098 ↗
12. Z.-H. Zhang, X.-F. Bian, Y. Wang, and X.-F. Liu: Trans. Nonferrous Met. Soc. China, 2001, vol. 11 (3), pp. 374–77.
13. X. Song, X. Bian, X. Qi, X. Liu, J. Zhang, B. Wang, and L. Zhu: J. Univ. Sci. Technol. Beijing, 2004, vol. 11 (1), pp. 81–84.
14. K. Nogita, S.D. McDonald, and A.K. Dahle: Phil. Mag., 2004, vol. 84, pp. 1683–96.10.1080/14786430310001659803 ↗
15. F.C. Robles Hernandez and J.H Sokolowski: J. Alloys Compd., 2006, vol. 426, pp. 205–12.10.1016/j.jallcom.2006.09.039 ↗
16. N. Nafisi, J. Hedjazi, S.M.A. Boutorabi, and R. Ghomashci: Light Metals 2004, Proc. Symp., A.T. Tobereaux, ed., Charlotte, NC, Mar. 14–18, 2004, TMS, Warrendale, PA, 2004, pp. 851–56.
17. D.C. Jenkinson and L.M. Hogan: J. Cryst. Growth, 1975, vol. 28, pp. 171–87.10.1016/0022-0248(75)90233-X ↗
18. L. Clapham and R.W. Smith: J. Cryst. Growth, 1988, vol. 92, pp. 263–70.10.1016/0022-0248(88)90458-7 ↗
19. K. Nogita, H. Yasuda, K. Yoshida, K. Oesugi, A. Takeuchi, Y. Suzuki, and A.K. Dahle: Scripta Mater., 2006, vol. 55, pp. 787–90.10.1016/j.scriptamat.2006.07.029 ↗
20. C.I. Simensen, Ø. Nielsen, F. Hillion, and J. Voje: Metall. Mater. Trans. A, 2007, vol. 38A, pp. 1448–51.10.1007/s11661-007-9165-y ↗
21. M.H. Kim, Y.M. Hong, and H.Y. Cho: Metall. Mater. Int., 2004, vol. 10, pp. 513–20.10.1007/BF03027412 ↗
22. Y.H. Cho, H.-C. Lee, K.H. Oh, and A.K. Dahle: Metall. Mater. Trans. A, 2008, vol. 39A, pp. 2435–48.10.1007/s11661-008-9580-8 ↗
23. W.J. Kyffin, W.M. Rainforth, and H. Jones: J. Mater. Sci., 2001, vol. 36, pp. 2667–72.10.1023/A:1017904627733 ↗
24. P. Mandal, A. Saha, and M. Chakraborty: AFS Trans., 1991, vol. 99, pp. 643–51.
25. J. Sulzer: Mod. Cast., 1961, vol. 39 (1), pp. 38–43.
26. J. Kaneko, M. Sugamata, and K.-I. Aoki: J. Jpn. Inst. Met., 1978, vol. 42, pp. 966-7210.2320/jinstmet1952.42.10_966 ↗
27. Trans. Jpn. Inst. Met., 1979, vol. 20, pp. 733-41.10.1536/ihj.20.733 ↗
28. B. Closset and J.E. Gruzleski: AFS Trans., 1981, vol. 89, pp. 801–08.
29. L. Bäckerud, G. Chai, and J. Tamminen: Solidification Characteristics of Aluminum Alloys, Foundry Alloys, AFS/Skanaluminum, Stockholm, 1990, vol. 2, pp. 33–38.
30. M. Faraji and L. Katgerman: Int. Foundry Res., 2009, vol. 61 (2), in press.
31. S.G. Shabestari and S. Ghodrat: Mater. Sci. Eng. A, 2007, vol. 467, pp. 150–58.10.1016/j.msea.2007.05.022 ↗
32. M. Djurdjevic, H. Jiang, and J. Sokolowski: Mater. Charact., 2001, vol. 46, pp. 31–38.10.1016/S1044-5803(00)00090-5 ↗
33. L. Heusler, and W. Schneider: J. Light Met., 2002, vol. 2, pp. 17–26.10.1016/S1471-5317(02)00009-3 ↗