Kinetics of low-temperature pack aluminide coating formation on alloy steels
Source abstract
Abstract
The kinetics of pack aluminide coating formation and growth on alloy steels was studied in the temperature range of 550 °C to 700 °C. The pack Al content was varied from 1 to 10 wt pct and aluminizing time from 1 to 16 hours. The halide salts AlCl3 and NH4Cl were studied as activators. In the AlCl3 activated packs, it was observed that all the coatings consisted of a single Fe2Al5 layer with an abrupt coating/substrate interface and varying the pack chemical compositions and processing conditions affected the growth rate of the layer thickness but not the microstructure of the coating. In these packs, it was revealed that the growth kinetics of the layer thickness (h in µm) that accounts for the effects of temperature (T in K), time (t in hours), and pack Al content (W in wt pct) can be described byh=75,141.8 exp (−8820.8/T)W1/2 t 1/2. In the NH4Cl activated packs, it was shown that coating formation and dissolution took place simultaneously at 650 °C. However, increasing Al content in this type of packs will increase the coating formation rate, making it possible to form a sufficient coating layer.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · High-Temperature Coating Behaviors · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. R. Mevrel, D. Duret, and R. Pichoir:Mater. Sci. Technol., 1986, vol. 2 (3), pp. 201–06.10.1179/mst.1986.2.3.201 ↗
2. G.W. Goward and D.H. Boone:Oxid. Met., 1971, vol. 3 (5), pp. 475–95.10.1007/BF00604047 ↗
3. Z.D. Xiang, J.S. Burnell-Gray, and P.K. Datta:J. Mater. Sci., 2001, vol. 36, pp. 5673–82.10.1023/A:1012534220165 ↗
4. Z.D. Xiang and P.K. Datta:J. Mater. Sci., 2003, vol. 38(18), pp. 3721–28.10.1023/A:1025915812928 ↗
5. S.R. Levine and R.M. Caves:J. Electrochem. Soc., 1974, vol. 121 (8), pp. 1051–64.10.1149/1.2401976 ↗
6. T.H. Wang and L.L. Seigle:Mater. Sci. Eng., A, 1989, vol. A108, pp. 253–63.10.1016/0921-5093(89)90428-0 ↗
7. B.K. Gupta and L.L. Seigle:Thin Solid Films, 1980, vol. 73, pp. 365–71.10.1016/0040-6090(80)90501-5 ↗
8. R. Sivakumar and L.L. Seigle:Metall. Trans. A, 1976, vol. 7A, pp. 1073–79.10.1007/BF02656589 ↗
9. D.C. Tu and L.L. Seigle:Thin Solid Films, 1982, vol. 95, pp. 47–65.10.1016/0040-6090(82)90581-8 ↗
10. S.C. Kung and R.A. Rapp:J. Electrochem. Soc., 1988, vol. 135 (3), pp. 731–41.10.1149/1.2095732 ↗
11. H.C. Akuezue and J. Stringer: inDiffusion Analysis and Applications, A.D. Romig and M.A. Dayananda, eds., TMS, Warrendale, PA, 1989, pp. 337–60.
12. H.M. Soliman, K.E. Mohamed, M.E. Abd El-Azim, and F.H. Hammad:J. Mater. Sci. Technol., 1997, vol. 13, pp. 383–88.
13. L. Levin, A. Ginzburge, L. Klinger, T. Werber, A. Katsman, and P. Schaaf:Surf. Coating Technol., 1998, vol. 106, pp. 209–13.10.1016/S0257-8972(98)00529-5 ↗
14. P.J. Ennis, A. Zielinska-Lipiec, O. Wachter, and A. Czyrska-Filemonowicz:Acta Mater., 1997, vol. 45 (12), pp. 4901–07.10.1016/S1359-6454(97)00176-6 ↗
15. S. Saroja, P. Parameswaran, M. Vijayalakshmi, and V.S. Raghunathan:Acta Mater., 1995, vol. 43, pp. 2985–3000.10.1016/0956-7151(95)00022-N ↗
16. D.V. Thornton and K.H. Meyer: inAdvanced Heat Resistant Steels for Power Generation, R. Viswanathan and J.W. Nutting, eds., IOM Communications Ltd., London, 1999, pp. 349–65.
17. Z.D. Xiang and P.K. Datta:Surf. Coating Technol., 2004, vol. 184, pp. 108–15.10.1016/j.surfcoat.2003.10.046 ↗
18. S. O’Dell, J. Charles, M. Vlot, and V. Randle:Mater. Sci. Technol., 2004, vol. 20, pp. 251–56.10.1179/026708304225011289 ↗
19. R. Jha, C.W. Haworth, and B.B. Argent:CALPHAD, 2001, vol. 25 (4), pp. 651–65.10.1016/S0364-5916(02)00015-9 ↗