Microstructure and sliding-wear behavior of tungsten-reinforced W-Ni-Si metal-silicide in-situ composites
Source abstract
Abstract
W-Ni-Si metal-silicide-matrix in-situ composites reinforced by tungsten primary grains were fabricated using a water-cooled copper-mold laser-melting furnace by the LASMELT process. Main constitutional phases of the W/W-Ni-Si in-situ composites are the tungsten primary phase, peritectic W2Ni3Si, and the remaining W2Ni3Si/Ni31Si12 eutectics, depending on the alloy compositions. The sliding-wear resistance of the W/W-Ni-Si intermetallic composites was evaluated at room temperature and 600 °C. Wear mechanisms of the W/W2Ni3Si in-situ composites were discussed based on morphology observations of the worn surface and wear debris. Results show that the W/W-Ni-Si composites have excellent wear resistance under both room- and high-temperature sliding-wear-test conditions, because of the high yield strength and toughness of the tungsten-reinforcing phase and the high hardness and the covalent-dominated intermetallic atomic bonds of the W2Ni3Si and Ni31Si12 metal silicides. Tungsten-reinforcing grains played the dominant role in resisting abrasive-wear attacks of microcutting, plowing, and brittle spalling during the sliding-wear process, while the W2Ni3Si and Ni31Si12 metal silicides are responsible for the excellent adhesive wear resistance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced materials and composites · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. J.J. Petrovic and A.K. Vasudevan: Mater. Sci. Eng. A, 1999, vol. A261, pp. 1–5.10.1016/S0921-5093(98)01043-0 ↗
2. C.T. Liu, J. Stringer, J.N. Mundy, L.L. Horton, and P. Angelini: Intermetallics, 1997, vol. 5, pp. 579–96.10.1016/S0966-9795(97)00045-9 ↗
3. J.H. Westbrook and R.L. Fleischer: Intermetallic Compounds, John Wiley & Sons, New York, 1994, vol. 2, pp. 211–35.
4. A.A. Sharif, A. Misra, J.J. Petrovic, and T.E. Mitchell: Intermetallics, 2001, vol. 9, pp. 869–73.10.1016/S0966-9795(01)00084-X ↗
5. R. Mitra and V.V.R. Rao: Metal. Mater. Trans. A, 1998, vol. 29A, pp. 1665–75.10.1007/s11661-998-0089-y ↗
6. F.W. Crossman and A.S. Yue: Metall. Trans. A, 1971, vol. 2, pp. 1545–55.10.1007/BF02913876 ↗
7. A. Tomasi, R. Ceccato, M. Nazmy, and S. Gialanella: Mater. Sci. Eng. A, 1997, vols. A239-240, pp. 877–81.10.1016/S0921-5093(97)00678-3 ↗
8. T. Takasugi, S. Watanabe, and O. Izumi: Acta Metall, 1989, vol. 37, pp. 3425–32.10.1016/0001-6160(89)90214-9 ↗
9. T. Takasugi, D. Shindo, O. Izumi, and M. Hirabayashi: Acta Metall., 1990, vol. 38, pp. 747–52.10.1016/0956-7151(90)90026-D ↗
10. M.E. Reiss, C.M. Esber, D. Van Heerden, A.J. Gavens, M.E. Williams, and T.P. Weihs: Mater. Sci. Eng. A, 1999, vol. 261, pp. 217–22.10.1016/S0921-5093(98)01069-7 ↗
11. J. Kajuch, J.D. Rigney, and J.J. Lewandowski: Mater. Sci. Eng. A, 1991, vol. A155, pp. 59–66.
12. F. Chu, D.J. Thoma, K.J. McClellan, and P. Peralta: Mater. Sci. Eng. A, 1999, vol. A261, pp. 44–52.10.1016/S0921-5093(98)01048-X ↗
13. J.A. Hawk and D.E. Alman: Mater. Sci. Eng. A, 1997, vols. A239–240, pp. 899–906.10.1016/S0921-5093(97)00681-3 ↗
14. H.M. Wang and G. Duan: Mater. Sci. Eng. A, 2002, vol. A336, pp. 117–23.10.1016/S0921-5093(01)01970-0 ↗
15. G. Duan and H.M. Wang: Acta Materiae Compositae Sinica, 2002, vol. 19, pp. 32–36.
16. G. Duan and H.M. Wang: Scripta Mater, 2002, vol. 46, pp. 107–11.10.1016/S1359-6462(01)01208-8 ↗
17. H.M. Wang, G. Duan, L.Y. Zhang, and W.J. Xi: Proc. SPIE, 2002, vol. 4915, pp. 162–66.10.1117/12.482880 ↗
18. J.W. Newkirk and J.A. Hawk: Wear, 2001, vol. 251, pp. 1361–137.10.1016/S0043-1648(01)00768-2 ↗
19. C.T. Liu, J.H. Zhu, M.P. Brady, and C.G. McKamey: Intermetallics, 2000, vol. 8, pp. 1119–29.10.1016/S0966-9795(00)00109-6 ↗
20. J. Przybylowicz and J. Kusinski: Surf. Coating Technol., 2000, vol. 125, pp. 13–18.10.1016/S0257-8972(99)00563-0 ↗
21. G. Sauthoff: Intermetallics, 2000, vol. 8, pp. 1101–09.10.1016/S0966-9795(00)00045-5 ↗
22. J.H. Schneibel, C.T. Liu, D.S. Eaton, and D.S. Carmichael: Mater. Sci. Eng. A, 1999, vol. 261, pp. 78–83.10.1016/S0921-5093(98)01051-X ↗
23. K. Sadananda, C.R. Feng, R. Mitra, and S.C. Deevi: Mater. Sci. Eng. A, 1999, vol. A261, pp. 223–38.10.1016/S0921-5093(98)01070-3 ↗
24. K. Badrinarayana, A.L. McKelvey, and K.T. Venkateswara: Metall. Mater. Trans. A, 1996, vol. 27A, pp. 3781–89.10.1007/BF02595627 ↗
25. J. Kajuch, J.D. Rigney, and J.J. Lewandowski: Mater. Sci. Eng. A, 1991, vol. A155, pp. 59–66.
26. J.H. Schneibel, C.T. Liu, D.S. Easton, and C.A. Carmichael: Mater. Sci. Eng. A, 1999, vol. A261, pp. 78–83.10.1016/S0921-5093(98)01051-X ↗
27. T.A. Cruse and J.W. Newkirk: Mater. Sci. Eng. A, 1997, vol. A239-240, pp. 410–18.10.1016/S0921-5093(97)00611-4 ↗
28. P. Villars, A. Prince, and H. Okamoto: Handbook of Ternary Alloy Phase Diagrams, ASM INTERNATIONAL, New York, NY, 1995, vol. 10, p. 13030.
29. H.M. Wang, L.Y. Zhang, W.J. Xi, and L.Q. Zhang: China Patent No. 02121496.4.
30. H.M. Wang, D.Y. Luan, and L.Y. Zhang: Scripta Mater., 2003, in press.
31. Handbook of Rare Metallic Materials and Applications, The Metallurgical Industry Press, Beijing, 1974, pp. 337–39.
32. ASM Handbook, vol. 2, Refractory Metals and Alloys, ASM INTERNATIONAL, Materials Park, OH, 1990, pp. 557–85.10.31399/asm.hb.v02.a0001079 ↗
33. The Chinese Encyclopedia of Metallurgy, The Metallurgical Industry Press, Beijing, 2001, pp. 608–10.
34. M.B. Peterson, S.J. Calabrase, and S.Z. Li: J. Mater. Sci. Technol., 1994, vol. 10, pp. 313–20.
35. T.F.J. Quinn and J.L. Sullivan: Wear, 1984, vol. 94, pp. 175–83.10.1016/0043-1648(84)90053-X ↗
36. H.E. Sliney: Lubric. Eng., 1994, vol. 50, pp. 571–76.