This work investigated the effect of nominal boron additions of 0.1, 0.4, and 1 wt pct on the intermediate-temperature (455 °C to 565 °C) tensile and tensile-creep deformation behavior of as-cast Ti-6Al-2Sn-4Zr-2Mo-0.1Si (wt pct) for applied stresses between 138 and 600 MPa. A 0.1 wt pct boron addition resulted in a refinement of the as-cast grain size from 550 to 75 μm. Additional boron additions resulted in a less dramatic refinement of the as-cast grain size. Boron additions stabilized the orthorhombic TiB phase where the average TiB-phase volume percents were 0.7, 2.3, and 5.4 for the Ti-6Al-2Sn-4Zr-2Mo-0.1Si-0.1B (wt pct), Ti-6Al-2Sn-4Zr-2Mo-0.1Si-0.4B (wt pct), and Ti-6Al-2Sn-4Zr-2Mo-0.1Si-1B (wt pct) alloys, respectively. Overall, the boron additions did not have a dramatic effect on the creep behavior of Ti-6Al-2Sn-4Zr-2Mo-0.1Si, though the Ti-6Al-2Sn-4Zr-2Mo-0.1Si-1B (wt pct) alloy exhibited lower minimum creep rates than the baseline Ti-6Al-2Sn-4Zr-2Mo-0.1Si (wt pct) alloy. The sequence of surface deformation events during the elevated-temperature tensile deformation was characterized using in-situ experiments performed inside a scanning electron microscope. The TiB whisker microcracking occurred at stresses well below the global yield stress. Multiple and extensive TiB cracking occurred after global yielding. The α + β phase slip occurred after TiB whisker cracking.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. W.F. Smith: Structure and Properties of Engineering Alloys, McGraw-Hill, Inc., New York, NY, 1993.
2. R.W. Hayes, G.B. Viswanathan, and M.J. Mills: Acta Mater., 2002, vol. 50, pp. 4953–63.10.1016/S1359-6454(02)00279-3 ↗
3. S.R. Seagle, G.S. Hall, and H.B. Bomberger: Met. Eng. Q., 1975, vol. 15, pp. 48–54.
4. S. Ankem and S.R. Seagle: Titanium Science Technology Oberursel, Duetsche Gesellschaft fur Metallkunde, Oberursel, Germany, 1985, pp. 2411–18.
5. C. Quesne, C. Duong, F. Charpentier, J. Fries, and P. Lacombe: J. Less Common Met., 1979, vol. 68, pp. 133–42.10.1016/0022-5088(79)90049-3 ↗
6. K.E. Thiehsen, M.E. Kassner, J. Pollard, D.R. Hiatt, and B.M. Bristow: Metall. Trans. A, 1993, vol. 24A, pp. 1819–26.10.1007/BF02657856 ↗
7. C.J. Boehlert, S. Tamirisakandala, and D.B. Miracle: Ti 2007 Sci. Technol., 2007, vol. 1, pp. 697–700.
8. C.J. Boehlert and W. Chen: Mater. Trans., 2009, in print.
9. T. Saito: J. Met., 2004, vol. 56, pp. 33–36.
10. C.F. Yolton and J.H. Moll: in Titanium 1995, P.A. Blenkinsop, W.J. Evans, and H.M. Flowers, eds., The University Press, Cambridge, United Kingdom, 1996, vol. 1, pp. 2755–62.
11. S. Gorsse and D.B. Miracle: Acta Mater., 2003, vol. 51, pp. 2427–42.10.1016/S1359-6454(02)00510-4 ↗
12. S. Tamirisakandala, R.B. Bhat, J.S. Tiley, and D.B. Miracle: Scripta Mater., 2005, vol. 53, pp. 1421–26.10.1016/j.scriptamat.2005.08.020 ↗
13. S. Tamirisakandala, R.B. Bhat, D.B. Miracle, S. Boddapati, R. Bordia, R. Vanover, and V.K. Vasudevan: Scripta Mater., 2005, vol. 53, pp. 217–22.10.1016/j.scriptamat.2005.03.038 ↗
14. W.O. Soboyejo, W. Shen, and T.S. Srivatsan: Mech. Mater., 2004, vol. 36, pp. 141–59.10.1016/S0167-6636(03)00036-X ↗
15. K.B. Panda and K.S. Ravi Chandran: Acta Mater., 2006, vol. 54, pp. 1641–57.10.1016/j.actamat.2005.12.003 ↗
16. C.J. Boehlert, C.J. Cowen, S. Tamirisakandala, D.J. McEldowney, and D.B. Miracle: Scripta Mater., 2006, vol. 55, pp. 465–68.10.1016/j.scriptamat.2006.05.008 ↗
17. I. Sen, S. Tamirisakandala, D.B. Miracle, and U. Ramamurty: Acta Mater., 2007, vol. 55, pp. 4983–93.10.1016/j.actamat.2007.05.009 ↗
18. C.J. Boehlert, S. Tamirisakandala, W.C. Curtin, and D.B. Miracle: Scripta Mater., 2009, in print.
19. K.S.R Chandran, K.B. Panda, and S.S. Sahay: J. Met., 2004, vol. 56 (5), pp. 42–48.
20. D.X. Li, D.H. Ping, Y.X. Lu, and H.Q. Ye: Mater. Lett., 1993, vol. 16, pp. 322–26.10.1016/0167-577X(93)90201-8 ↗
21. C.J. Cowen and C.J. Boehlert: Metall. Mater. Trans. A, 2007, vol. 38A, pp. 26–34.10.1007/s11661-006-9004-6 ↗
22. J.P. Quast and C.J. Boehlert: Metall. Mater. Trans. A, 2007, vol. 38A, pp. 529–36.10.1007/s11661-006-9074-5 ↗
23. C.J. Boehlert, S.C. Longanbach, and T.R. Bieler: Phil. Mag., 2008, vol. 88, pp. 641–64.10.1080/14786430801944836 ↗
24. Y. Komizo, H. Terasaki, M. Ikeda, F. Nishino, and K. Toudai: Ti 2007 Sci. Technol., 2007, vol. 1, pp. 741–44.
25. R.W. Evans and B. Wilshire: Creep of Metals and Alloys, The Institute of Metals, New York, NY, 1985.
26. W. Chen and C.J. Boehlert: Mater. Sci. Eng. A, 2008, vol. 494, pp. 132–38.10.1016/j.msea.2008.04.004 ↗
27. J.R. Porter, J.A. Hall, J.C. Chesnutt, and C.G. Rhodes: “Advanced Ti-Based MMC Development,” Interim Report WL-TR-95-4034, Wright Patterson Air Force Base, Dayton, OH, 1995.
28. P.R. Smith, A. Rosenberger, and M.J. Shepard: Scripta Metall., 1999, vol. 41 (2), pp. 221–28.10.1016/S1359-6462(99)00162-1 ↗
29. R. Boyer, G. Welsch, and E.W. Collings: Materials Properties Handbook: Titanium Alloys, ASM INTERNATIONAL, Materials Park, OH, 1994, p. 337.
30. J.A. Vreeling, V. Ocelik, and J.T.M. De Hosson: Acta Mater., 2002, vol. 50, pp. 4913–24.10.1016/S1359-6454(02)00366-X ↗
31. A.B. Kloosterman, B.J. Kooi, and J.T.M. De Hosson: Acta Mater., 1998, vol. 46, pp. 6205–17.10.1016/S1359-6454(98)00265-1 ↗