journal article·2003-08

Effect of N addition on tensile and corrosion behaviors of CD4MCU cast duplex stainless steels

Jinil Son, Sangshik Kim, Jehyun Lee, Byunghak Choi

Publisher page

Abstract

The effect of N addition on the microstructure, tensile, and corrosion behaviors of CD4MCU (Fe-25Cr-5Ni-2.8Cu-2Mo) cast duplex stainless steel was examined in the present study. The slow strain rate tests were also conducted at a nominal strain rate of 1 × 10−6/s in air and 3.5 pct NaCl+5 pct H2SO4 solution for studying the stress corrosion cracking (SCC) behavior. It was observed that the volume fraction of austenitic phase in CD4MCU alloy varied from 38 to 59 pct with increasing nitrogen content from 0 to 0.27 wt. pct. The tensile behavior of CD4MCU cast duplex stainless steels, which tended to vary significantly with different N contents, appeared to be strongly related to the volume changes in ferritic and austenitic phases, rather than the intrinsic N effect. The improvement in the resistance to general corrosion in 3.5 pct NaCl+5 pct H2SO4 aqueous solution was notable with 0.13 pct N addition. The further improvement was not significant with further N addition. The resistance to SCC of CD4MCU cast duplex stainless steels in 3.5 pct NaCl+5 pct H2SO4 aqueous solution, however, increased continuously with increasing N content. The enhancement in the SCC resistance was believed to be related to the volume fraction of globular austenitic colonies, which tended to act as barriers for the development of initial pitting cracks in the ferritic phase into the sharp ones.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. J.A. Jimenez, M. Carsi, G. Frommeyer, and O.A. Ruano: Key Eng. Mater., 2000, vol. 171 (4), pp. 389–94.10.4028/www.scientific.net/KEM.171-174.389 ↗
2. J.S. Kim, C.J. Park, and H.S. Kwon: Bull. Kor. Inst. Met. Mater., 1999, vol. 12, pp. 634–57.
3. A.J. Sedriks: NACE, 1986, vol. 42, pp. 376–89.10.5006/1.3584918 ↗
4. J.H. Huang and C.J. Altstetter: Metall. Mater. Trans. A, 1995, vol. 26A, pp. 1079–85.10.1007/BF02670603 ↗
5. H. Hanninen, J. Romu, R. Ilola, J. Tervo, and A. Laitinen: J. Mater. Pro. Technol., 2001, vol. 117, pp. 424–30.10.1016/S0924-0136(01)00804-4 ↗
6. J.O. Nilson and A. Wilson: J. Mater. Sci. Technol., 1993, vol. 9, pp. 545–54.10.1179/mst.1993.9.7.545 ↗
7. T. Kudo, H. Tsuge, and T. Moroishi: NACE, 1989, vol. 45, pp. 831–38.10.5006/1.3584990 ↗
8. S. Mark Wilhelm and R.D. Kane: NACE, 1984, vol. 40, pp. 431–39.10.5006/1.3593951 ↗
9. J.W. Simmons: Mater. Sci. Eng., 1996, vol. A207, pp. 159–69.10.1016/0921-5093(95)09991-3 ↗
10. K.N. Adhe, V. Kain, K. Madangopal, and H.S. Gadiyar: J. Mater. Eng. Performance, 1996, vol. 5 (4), pp. 500–06.10.1007/BF02648847 ↗
11. J. Wang, P.J. Uggowitzer, R. Magdowski, and M.O. Speidel: Scripta. Metall. Mater., 1999, vol. 40, pp. 123–29.10.1016/S1359-6462(98)00396-0 ↗
12. Russel D. Kane: Slow Strain Rate Testing for the Evaluation of Environmentally Induced Cracking, ASTM, Baltimore, MD, 1993.
13. J.E. Truman, M.J. Coleman, and K.R. Pirt: Br. Corr. J., 1997, vol. 12, pp. 236–45.10.1179/000705977798318973 ↗
14. K. Osozawa and N. Okato: Passivity and Its Breakdown on Iron and Iron Base Alloys, R. Staehle and H. Okada, eds., NACE, Houston, TX, 1976.
15. E. Owczarek and T. Zakroczymski: Acta Metall. Mater., 2000, vol. 48, pp. 3059–70.10.1016/S1359-6454(00)00122-1 ↗
16. T. Suzuki, H. Hasegawa, and M. Watanabe: Nippon Kinzaku Gakaishi, 1968, vol. 32, pp. 1171–81.