journal article·2002-06

Sensitization behavior of type 308 stainless steel weld metals after postweld heat treatment and low-temperature aging and its relation to microstructure

Ikuhisa Hamada, Kiyoshi Yamauchi

Publisher page

Abstract

Type 308 weld metal overlaid on a low-alloy steel by a submerged arc welding (SAW) process using wide strip electrodes can become sensitized by not only postweld heat treatments (PWHTs) at around 600 °C but also low-temperature aging (LTA) at 500 °C for 24 hours after PWHT. A slow strain-rate test (SSRT) in oxygenated, high-temperature pure water revealed that type 308 SAW weld metals after PWHT were susceptible to intergranular stress corrosion cracking (IGSCC) when sensitized such that the intergranular corrosion (IGC) rate in the modified ASTM A262E test exceeds 1 µm/h. The effect of microstructure (ferrite phase distribution) on the sensitization behavior was evaluated using a microstructural parameter NLβ−γ. Though mostly useful, the average NLβ−γ was not always accurate in distinguishing IGC-susceptible, SAW overlay weld metals. However, local NLβ−γ, newly introduced to deal with a rather large fluctuation in ferrite distribution within SAW overlay weld metals, was partly able to explain the IGC susceptibility of a theoretically resistant heat with a high average NLβ−γ. The beneficial effect of surface remelting by plasma arc on the IGC resistance was described.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. A.G. Vinckier and A.W. Pense: WRC Bulletin, 1974, No. 197.
2. Japanese Industrial Standard (JIS), G 0575, “Copper Sulfate-Sulfuric Acid Test for Stainless Steels.”
3. T.M. Devine, Jr.: Metall. Trans. A, 1980, vol. 11A, pp. 791–800.10.1007/BF02661208 ↗
4. H. Menendez and T.M. Devine: Corrosion, 1990, vol. 49, pp. 410–18.10.5006/1.3585125 ↗
5. J.N. Kass, J.C. Lemaire, R.B. Davis, J.E. Alexander, and J.C. Danko: Corrosion, 1980, vol. 36, pp. 686–98.10.5006/0010-9312-36.12.686 ↗
6. M.J. Povich: Corrosion, 1978, vol. 34(2), pp. 60–65.10.5006/0010-9312-34.2.60 ↗
7. M.J. Povich and P. Rao: Corrosion, 1978, vol. 34(8), pp. 269–75.10.5006/0010-9312-34.8.269 ↗
8. F. Uberti, S. Bonato, G. Buzzanca, and R. Pascali: Corrosion 88, NACE, Houston, TX, 1988, pp. 295/1–295/12.
9. Specification for Base Stainless Steel Welding Electrodes and Rods, ASME Section II, SFA-5.9, ASME, New York, NY, 1989.
10. S. Hattori, J. Kuniya, Y Mori, R. Sasaki, K. Masaoka, and H. Itow: Proc. 100th Conf. of The Iron and Steel Institute of Japan, The Iron and Steel Institute of Japan, Tokyo, 1980, Paper No. A-213.
11. I. Hamada, G. Nakao, K. Yamauchi, and T. Maruyama: Predictive Methods for Assessing Corrosion Damage to BWR Piping and PWR Steam Generators, NACE, Houston, TX, 1978, pp. 174–78.
12. I. Hamada and K. Yamauchi: Corrosion, 2002, vol. 58, pp. 82–93.10.5006/1.3277307 ↗
13. K. Nishimoto, H. Mori, and Y. Nakao: Iron Steel Inst. Jpn. Int., 1995, vol. 35(10), pp. 1265–71.10.2355/isijinternational.35.1265 ↗