Effects of Oxides on Tensile and Charpy Impact Properties and Fracture Toughness in Heat Affected Zones of Oxide-Containing API X80 Linepipe Steels
Source abstract
Abstract
This study is concerned with effects of complex oxides on acicular ferrite (AF) formation, tensile and Charpy impact properties, and fracture toughness in heat affected zones (HAZs) of oxide-containing API X80 linepipe steels. Three steels were fabricated by adding Mg and O2 to form oxides, and various HAZ microstructures were obtained by conducting HAZ simulation tests under different heat inputs. The no. of oxides increased with increasing amount of Mg and O2, while the volume fraction of AF present in the steel HAZs increased with increasing the no. of oxides. The strengths of the HAZ specimens were generally higher than those of the base metals because of the formation of hard microstructures of bainitic ferrite and granular bainite. When the total Charpy absorbed energy was divided into the fracture initiation and propagation energies, the fracture initiation energy was maintained constant at about 75 J at room temperature, irrespective of volume fraction of AF. The fracture propagation energy rapidly increased from 75 to 150 J and saturated when the volume fraction of AF exceeded 30 pct. At 253 K (−20 °C), the total absorbed energy increased with increasing volume fraction of AF, as the cleavage fracture was changed to the ductile fracture when the volume fraction of AF exceeded 45 pct. Thus, 45 vol pct of AF at least was needed to improve the Charpy impact energy, which could be achieved by forming a no. of oxides. The fracture toughness increased with increasing the no. of oxides because of the increased volume fraction of AF formed around oxides. The fracture toughness did not show a visible correlation with the Charpy absorbed energy at room temperature, because toughness properties obtained from these two toughness testing methods had different significations in view of fracture mechanics.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fatigue and fracture mechanics · Microstructure and Mechanical Properties of Steels · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. K.T. Corbett, R.R. Bowen, and C.W. Petersen: Int. J. Offshore Polar Eng., 2004, vol. 14, pp. 75–80.
2. R. Denys: Pipeline Technology, vols. I & II, Elsevier, Amsterdam, 2000.
3. Y.T. Shin and H.W. Lee: Met. Mater. Int., 2012, vol. 18, pp. 863–67.10.1007/s12540-012-5018-3 ↗
4. D.P. Fairchild, M.L. Macia, S.D. Papka, C.W. Petersen, J.H. Stevens, S.T. Barbas, N.V. Bangaru, J.Y. Koo, and M.J. Luton: Proceedings of the International Pipe Dreamer’s Conference, Yokohama, 2002, pp. 307–21.
5. T. Koseki, H. Kato, M. Tsutsumi, K. Kasai, and J. Inoue: Int. J. Mater. Res., 2008, vol. 99, pp. 347–51.10.3139/146.101643 ↗
6. J.-S. Byun, J.-H. Shim, Y.W. Cho, and D.N. Lee: Acta Mater., 2003, vol. 51, pp. 1593–1606.10.1016/S1359-6454(02)00560-8 ↗
7. S.S. Babu: Curr. Opin. Solid State Mater., 2004, vol. 8, pp. 267–78.10.1016/j.cossms.2004.10.001 ↗
8. J.-H. Shim, Y.J. Oh, J.Y. Suh, Y.W. Cho, J.-D. Shim, J.S. Byun, and D.N. Lee: Acta Mater., 2001, vol. 49, pp. 2115–22.10.1016/S1359-6454(01)00134-3 ↗
9. S.Y. Shin, K. Oh, K.B. Kang and S. Lee, Mater. Sci. Technol., 2010, vol. 26, pp. 1049–58.10.1179/174328409X425218 ↗
10. T. Maki: Mater. Jpn., 1997, vol. 36, pp. 937–40.10.2320/materia.36.937 ↗
11. J.M. Gregg and H.K.D.K. Bhadeshia: Acta Mater., 1997, vol. 45, pp. 739–48.10.1016/S1359-6454(96)00187-5 ↗
12. M. Enomoto: Met. Mater., 1998, vol. 4, pp. 115–23.10.1007/BF03026028 ↗
13. F.J. Barbaro, P. Krauklis, and K.E. Easterling: Mater. Sci. Technol., 1989, vol. 5, pp. 1057–68.10.1179/mst.1989.5.11.1057 ↗
14. H.K.D.H. Bhadeshia: Bainite in Steels, 2nd ed., IOM Communications Ltd., London, 2001.
15. Y.T. Shin, H.S. Shin, H.W. Lee: Met. Mater. Int., 2012, vol. 18, pp. 1037–40.10.1007/s12540-012-6017-0 ↗
16. S.Y. Shin, K. Oh, K.B. Kang, and S. Lee: ISIJ Int., 2009, vol. 49, No. 8, pp. 1191–99.10.2355/isijinternational.49.1191 ↗
17. W. Cha, K. Oh, and J.Y. Cho: Kor. Patent No. 10-2010-0102442, 2010.
18. I. Tamura, H. Sekine, T. Tanaka, and C. Ouchi: Thermomechanical Processing of High-Strength Low-Alloy Steels, Butterworth & Co. Ltd., London, UK, 1988, pp. 80–100.10.1016/B978-0-408-11034-1.50007-6 ↗
19. S. Vervynckt, P. Thibaux, and K. Verbeken: Mater. Int., 2012, vol. 18, pp. 37–46.10.1007/s12540-012-0005-2 ↗
20. S. Kim and C. Lee: Met. Mater. Int., 2012, vol. 18, pp. 857–62.10.1007/s12540-012-5017-4 ↗
21. M. Diaz-Fuentes, A. Iza-Mendia, and I. Gutierrez: Metall. Mater. Trans. A, 2003, vol. 34A, pp. 2505–16.10.1007/s11661-003-0010-7 ↗
22. ASTM Standard E8/E8M-11: Standard Test Methods for Tension Testing of Metallic Materials, Annual Book of ASTM Standards, ASTM, West Conshohocken, PA, 2011.
23. ASTM Standard E23-12c: Standard Test Method for Notched Bar Impact Testing of Metallic Materials, Annual Book of ASTM Standards, ASTM, West Conshohocken, PA, 2012.
24. ASTM Standard E2298-09: Standard Test Method for Instrumented Impact Testing of Metallic Materials, Annual Book of ASTM Standards, ASTM, West Conshohocken, PA, 2009.
25. ASTM Standard E1921-12: Standard Test Method for Determination of Reference Temperature, T o , for Ferritic Steels in the Transition Range, Annual Book of ASTM Standards, ASTM, West Conshohocken, PA, 2012.
26. C.H. Lee, H.K.D.H. Bhadeshia, and H.-C. Lee: Mater. Sci. Eng., 2003, vol. A360, pp. 249–57.10.1016/S0921-5093(03)00477-5 ↗
27. G. Krauss and S.W. Thompson: ISIJ Int., 1995, vol. 35, pp. 937–45.10.2355/isijinternational.35.937 ↗
28. S.S. Sohn, S.Y. Han, S.Y. Shin, J. Bae, K. Kim, N.J. Kim, H.S. Kim, and S. Lee: Mater. Int., 2012, vol. 18, pp. 597–606.10.1007/s12540-012-4005-z ↗
29. D. Hull and D.J. Bacon: Introduction to Dislocations, 5th ed., Elsevier Ltd., Amsterdam, 2011.
30. Y. Ohomori, H. Ohtani, and T. Kunitake: Met. Sci., 1974, vol. 8, pp. 357–66.10.1179/msc.1974.8.1.357 ↗
31. A.P. Green and B.B. Hundy: J. Mech. Phys. Solids, 1956, vol. 4, pp. 128–44.10.1016/0022-5096(56)90085-0 ↗
32. J.M. Alexander and T.J. Komoly: J. Mech. Phys. Solids, 1962, vol. 10, pp. 265–75.10.1016/0022-5096(62)90043-1 ↗
33. H. Couque, R.J. Asaro, J. Duffy, and S.H. Lee: Metall. Trans. A, 1988, vol. 19A, pp. 2179–2206.10.1007/BF02645043 ↗
34. S.Y. Shin, K. Oh, S. Lee, and N. J. Kim: Met. Mater. Int., 2011, vol. 17, pp. 29–40.10.1007/s12540-011-0205-1 ↗
35. W.M. Garrison Jr., A.L. Wojcieszynski: Mater. Sci. Eng., vol. 464, 2007, pp. 321-29.10.1016/j.msea.2007.02.015 ↗
36. S. Kim, S. Lee, Y.-R. Im, H.-C. Lee, S.-J. Kim, and J.H. Hong: Metall. Mater. Trans. A, 2004, vol. 35A, pp. 2027–37.10.1007/s11661-004-0151-3 ↗
37. S. Lee, B.C. Kim, and D. Kwon: Metall. Trans. A., 1993, vol. 24A, pp. 1133–41.10.1007/BF02657244 ↗
38. R.O. Ritchie, J.F. Knott, and J.R. Rice: J. Mech. Phys. Solids, 1973, vol. 21, pp. 395–410.10.1016/0022-5096(73)90008-2 ↗
39. D. Horsley: Eng. Fract. Mech., vol. 70, 2003, pp. 547–52.10.1016/S0013-7944(02)00136-4 ↗