journal article·2002-09

Direct observation of the crystal-growth transition in undercooled silicon

Zengyun Jian, Kosuke Nagashio, Kazuhiko Kuribayashi

Publisher page

Abstract

Using an electromagnetic levitation facility with a laser heating unit, silicon droplets were highly undercooled in the containerless state. The crystal morphologies on the surface of the undercooled droplets during the solidification process and after solidification were recorded live by using a high-speed camera and were observed by scanning electron microscopy. The growth behavior of silicon was found to vary not only with the nucleation undercooling, but also with the time after nucleation. In the earlier stage of solidification, the silicon grew in lateral, intermediary, and continuous modes at low, medium, and high undercoolings, respectively. In the later stage of solidification, the growth of highly undercooled silicon can transform to the lateral mode from the nonlateral one. The transition time of the sample with 320 K of undercooling was about 535 ms after recalescence, which was much later than the time where recalescence was completed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Solidification and crystal growth phenomena · Metallic Glasses and Amorphous Alloys · Phase-change materials and chalcogenides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. G. Devaud and D. Turnbull: Acta Metall., 1987, vol. 35, pp. 765–69.10.1016/0001-6160(87)90202-1 ↗
2. Y. Shao and F. Spaepen: J. Appl. Phys., 1996, vol. 79, pp. 2981–85.10.1063/1.361222 ↗
3. D. Li and D.M. Herlach: Phys. Rev. Lett., 1996, vol. 77, pp. 1801–04.10.1103/PhysRevLett.77.1801 ↗
4. D. Li and D.M. Herlach: Europhys. Lett., 1996, vol. 34, pp. 423–28.10.1209/epl/i1996-00473-7 ↗
5. D. Li and D.M. Herlach: J. Mater. Sci., 1997, vol. 32, pp. 1467–42.
6. S.E. Battersby, R.F. Cochrane, and A.M. Mullis: J. Mater. Sci., 1999, vol. 34, pp. 2049–56.10.1023/A:1004547423857 ↗
7. C.F. Lau and H.W. Kui: Acta Metall., 1991, vol. 39, pp. 323–27.10.1016/0956-7151(91)90311-N ↗
8. C.F. Lau and H.W. Kui: Acta Metall., 1993, vol. 41, pp. 1999–2005.10.1016/0956-7151(93)90370-8 ↗
9. C.F. Lau and H.W. Kui: Acta Metall., 1994, vol. 42, pp. 3811–16.10.1016/0956-7151(94)90446-4 ↗
10. T. Aoyama, Y. Takamura, and K. Kuribayashi: Metall. Mater. Trans. A, 1999, vol. 30A, pp. 1333–39.10.1007/s11661-999-0282-7 ↗
11. T. Aoyama, Y. Takamura, and K. Kuribayashi: Metall. Mater. Trans., 1999, vol. 30A, pp. 3013–16.10.1007/s11661-999-0140-7 ↗
12. T. Aoyama, Y. Takamura, and K. Kuribayashi: Acta Mater. Metall. A, 2000, vol. 48, pp. 3739–44.10.1016/S1359-6454(00)00164-6 ↗
13. R.P. Liu, T. Volkmann, and D.M. Herlach: Acta Metall., 2001, vol. 49, pp. 439–44.
14. T. Aoyama, Y. Takamura, and K. Kuribayashi: Jpn. J. Appl. Phys., 1998, vol. 37, pp. L687-L690.10.1143/JJAP.37.L687 ↗
15. H. Watanabe, M. Susa, H. Fukuyama, and K. Nagata: High Temp.-High Pressures, 1999, vol. 31, pp. 587–93.10.1068/htwu124 ↗
16. K. Kuribayashi and T. Aoyama: J. Cryst. Growth, 2002, vols. 237–339, pp. 1840–43.10.1016/S0022-0248(01)02105-4 ↗
17. Z.Y. Jian and K. Kuribayashi: The Institute of Space and Astronautical Science, Kanagawa, Japan, unpublished research, 2002.