journal article·2002-06

Infrared repair brazing of 403 stainless steel with a nickel-based braze alloy

R. K. Shiue, S. K. Wu, C. M. Hung

Publisher page

Abstract

Martensitic stainless steel (403SS) is extensively used for intermediate and low-pressure steam turbine blades in fossil-fuel power plants. The purpose of this investigation is to study the repair of shallow cracks on the surface of 403SS steam turbine blades by infrared repair brazing using rapid thermal cycles. A nickel-based braze alloy (NICROBRAZ LM) is used as filler metal. The braze alloy after brazing is primarily comprised of borides and an FeNi3 matrix with different amounts of alloying elements, especially B and Si. As the brazing temperature increases, more Fe atoms are dissolved into the molten braze. Some boron atoms diffuse into the 403SS substrate primarily via grain boundary diffusion and form B-Cr-Fe intermetallic precipitates along the grain boundaries. The LM filler metal demonstrates better performance than 403SS in both microhardness and wear tests. It is also noted that specimens brazed in a vacuum have less porosity than those brazed in an Ar atmosphere. The shear strength of the joint is around 300 MPa except for specimens brazed in short time periods, e.g., 5 seconds in Ar flow and 30 seconds in vacuum. The fractographs mainly consist of brittle fractures and no ductile dimple fractures observed in the scanning electron microscope (SEM) examination.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. M.C. Balmforth and J.C. Lippold: Weld. J., 1998, vol. 77, pp. 1s-7s.
2. R.B. Corbit and S.M. French: Weld. J., 1997, vol. 76, pp. 51–55.
3. D. Armstrong: Weld. World, 1993, vol. 31, pp. 426–27.
4. C.E. Chang: Trans. Geothermal Res., 1989, vol. 13, pp. 569–74.
5. M.K. Lee: J. Nucl. Mater., 1998, vol. 254, pp. 42–48.10.1016/S0022-3115(97)00348-6 ↗
6. J.S. Dubey: J. Nucl. Mater., 1998, vol. 254, pp. 271–74.10.1016/S0022-3115(98)00007-5 ↗
7. P.R. Sreenivasan, S.K. Ray, S.L. Mannan, and P. Rodriguez: J. Nucl. Mater., 1996, vol. 228, pp. 338–45.10.1016/0022-3115(95)00225-1 ↗
8. Y. Fu, A.W. Batchelor, N.L. Loh, and K.W. Tan: Wear, 1998, vol. 219, pp. 169–76.10.1016/S0043-1648(98)00184-7 ↗
9. C.V. Cooper, K. Marchev, and B.C. Giessen: Surf. Coat. Technol., 1998, vol. 99, pp. 229–33.10.1016/S0257-8972(97)00533-1 ↗
10. B.H. Olesen, R. Avci, and Z. Lewandowski: Corr. Sci., 2000, vol. 42, pp. 211–27.10.1016/S0010-938X(99)00071-2 ↗
11. J. Vollmar and E. Roeder: Int. J. Fatigue, 1996, vol. 18, p. 422.
12. R. Li and M.G.S. Ferreira: Corr. Sci., 1996, vol. 38, pp. 317–27.10.1016/0010-938X(96)00130-8 ↗
13. E. Stagno, M.R. Pinasco, M.G. Ienco, G. Palombarini, and G.F. Bocchini: J. Alloy Compounds, 1997, vol. 247, pp. 172–79.10.1016/S0925-8388(96)02604-7 ↗
14. V. Shanov and W. Tabakoff: Surf. Coat. Technol., 1996, vol. 86, pp. 88–93.10.1016/S0257-8972(96)02965-9 ↗
15. H.M. Shalaby, J.A. Begley, and D.D. Macdonald: Br. Corr. J., 1994, vol. 29, pp. 43–52.10.1179/000705994798268024 ↗
16. J.S. Dubey, S.L. Wadekar, and J.K. Chakravartty: J. Nucl. Mater., 1998, vol. 254, pp. 271–74.10.1016/S0022-3115(98)00007-5 ↗
17. J.G. Gonzalez and Rodriguez: Mater. Lett., 2000, vol. 43, pp. 208–14.10.1016/S0167-577X(99)00261-X ↗
18. B. Miao, D.C. Northwood, L.C. Lim, and M.A. Lai: Mater. Sci. Eng. A-Struct., 1993, vol. 171, pp. 21–33.10.1016/0921-5093(93)90389-V ↗
19. H.M. Shalaby, J.A. Begley, and D.D. Macdonald: Corrosion, 1996, vol. 52, pp. 262–74.10.5006/1.3293638 ↗
20. L. Albertin, P.K. Liaw, M.G. Burke, and R.L. Frohlich: Scripta Mater., 1991, vol. 25, pp. 2445–50.10.1016/0956-716X(91)90047-5 ↗
21. W.R. Oates and A.M. Saitta: Welding Handbook Volume 4, American Welding Society, Miami, FL, 1998, pp. 233–332.
22. D.L. Olson, T.A. Siewert, S. Liu, and G.R. Edwards: ASM Handbook vol. 6, Welding, Brazing, and Soldering, ASM INTERNATIONAL, Materials Park, OH, 1993, pp. 431–55.10.31399/asm.hb.v06.9781627081733 ↗
23. D.N. French: Metallurgical Failures in Fossil Fired Boilers, John Wiley & Sons, Inc., New York, NY, 1993, pp. 242–76.
24. S.J. Lee, S.K. Wu, and R.Y. Lin: Acta Mater., 1998, vol. 46, pp. 1283–95.10.1016/S1359-6454(97)00298-X ↗
25. T.Y. Yang, S.K. Wu, and R.K. Shiue: Intermetallics, 2001, vol. 9, pp. 341–47.10.1016/S0966-9795(01)00011-5 ↗
26. S.J. Lee and S.K. Wu: Intermetallics, 1999, vol. 7, pp. 11–21.10.1016/S0966-9795(98)00004-1 ↗
27. R.K. Shiue, S.K. Wu, J.M. O, and J.Y. Wang: Metall. Mater. Trans. A, 2000, vol. 31A, pp. 2527–36.10.1007/s11661-000-0197-9 ↗
28. M. Schwartz: Brazing: For the Engineering Technologist, Chapman & Hall, New York, NY, 1995, pp. 8–55.
29. G. Humpston and D.M. Jacobson: Principles of Soldering and Brazing, ASM INTERNATIONAL, Materials Park, OH, 1993, pp. 71–110.
30. M. Roulin, J.W. Luster, G. Karadeniz, and A. Mortensen: Weld. J., 1999, vol. 78, pp. 151s-55s.
31. R.E. Lee: Scanning Electron Microscopy and X-Ray Microanalysis, Prentice Hall, New York, NY, 1993, pp. 130–4.
32. P. Villars, A. Prince, and H. Okamoto: Handbook of Ternary Alloy Phase Diagrams, ASM INTERNATIONAL, Metals Park, OH, 1995, pp. 5508–13.
33. A. Rabinkin, E. Wenski, and A. Ribaudo: Weld. J., 1998, vol. 77, pp. 66s-75s.
34. A. Rabinkin, E. Wenski, and A. Ribaudo: Weld. World, 1998, vol. 41, pp. 466–78.
35. X. Wu, R.S. Chandel, S.H. Pheow, and H. Li: Mater. Sci. Eng. A-Struct., 2000, vol. A288, pp. 84–90.10.1016/S0921-5093(00)00839-X ↗
36. S.K. Tung, L.C. Lim, and M.O. Lai: Scripta Mater., 1996, vol. 34, pp. 763–69.10.1016/1359-6462(95)00577-3 ↗
37. P.J. Blau: ASM Handbook, vol. 18, Friction, Lubrication, and Wear Technology, ASM INTERNATIONAL, Materials Park, OH, 1992, pp. 184–90.
38. H. Chandler: Heat Treater’s Guide: Practices and Procedures for Irons and Steels, ASM INTERNATIONAL, Metals Park, OH, 1995, pp. 763–65.