Effects of Isothermal Aging on the Microstructure Evolution and Pitting Corrosion Resistance of Lean Duplex Stainless Steel UNS S32003
Source abstract
Abstract
UNS S32003 materials were aged at temperatures in the range of 873 K to 1173 K (600 °C to 900 °C) for 30 minutes and 2 hours. Nitrides were found to precipitate along the ferrite/austenite phase boundaries and within the ferrite phase. The precipitation kinetics was the fastest at 1073 K (800 °C), at which temperature the Cr-depleted zones were observed to be in the vicinity of the precipitates. Precipitation and resultant Cr-depleted zone led to the highest pitting susceptibility of the UNS S32003, aged at 1073 K (800 °C), when tested in 0.6 mol/L NaCl solution. To observe the precipitation evolution, the UNS S32003 specimens were aged at 973 K (700 °C) for different time periods for up to 120 hours. Within aging time up to 24 hours at 973 K (700 °C), only nitrides precipitates were observed and an intermetallic phase was observed after 120 hours of aging along with an increase in the percentage of precipitates. Pitting potential dropped with increasing aging time and metastable pitting rate increased with longer aging time period, both indicating a negative effect of aging on pitting corrosion resistance of the lean duplex stainless steel UNS S32003.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. A. Bhattacharya and P. M. Singh, J. Fail. Anal. Prev. 2007, vol. 7, pp. 371-377.10.1007/s11668-007-9069-6 ↗
2. V. Muthupandi, P. Srinivasan, S. K. Seshadri, S. Sundaresan, Mater. Sci. Eng. A 2003, 358, 9-16.10.1016/S0921-5093(03)00077-7 ↗
3. R. Badji, M. Bouabdallah, B. Bacroix, C. Kahloun, B. Belkessa and H. Maza, Materials Characterization 2008, vol. 59, pp. 447-53.10.1016/j.matchar.2007.03.004 ↗
4. N Leif, Welding in the World 2012, 56, 65-76.10.1007/BF03321351 ↗
5. L. Zhang, W. Zhang, Y. Jiang, B. Deng, D. Sun and J. Li, Electrochim. Acta 2009, vol. 54, pp. 5387-92.10.1016/j.electacta.2009.04.023 ↗
6. Y. Yang, H. Tan, Z. Zhang, Z. Wang, Y. Jiang, L. Jiang and J. Li, CORROSION 2012, vol. 69, pp. 167-73.10.5006/0717 ↗
7. L. He and P.M. Singh, In CORROSION 2017, (NACE International: New Orleans, Louisiana, USA, 2017), p 8.
8. D. C. dos Santos and R. Magnabosco, Metall. Mater. Trans. A 2016, vol. 47, pp. 1554-65.10.1007/s11661-016-3323-z ↗
9. J. Michalska and M. Sozańska, Mater. Charact. 2006, vol. 56, pp. 355-62.10.1016/j.matchar.2005.11.003 ↗
10. I. Calliari, M. Pellizzari, M. Zanellato and E. Ramous, J. Mater. Sci. 2011, vol. 46, p. 6916.10.1007/s10853-011-5657-7 ↗
11. H. Sieurin, R. Sandström, Mater. Sci. Eng. A 2007, 444, 271-76.10.1016/j.msea.2006.08.107 ↗
12. A. Bhattacharya and P. M. Singh, Metall. Mater. Trans. A 2009, vol. 40, pp. 1388-99.10.1007/s11661-009-9833-1 ↗
13. M. E. Wilms, V. J. Gadgil, J. M. Krougman and F. P. Ijsseling, Corros. Sci. 1994, vol. 36, pp. 871-81.10.1016/0010-938X(94)90176-7 ↗
14. C. J. Park, V. S. Rao and H. S. Kwon, CORROSION 2005, vol. 61, pp. 76-83.10.5006/1.3278163 ↗
15. J.-Y. Maetz, S. Cazottes, C. Verdu and X. Kleber, Metall. Mater. Trans. A 2016, vol. 47, pp. 239-53.10.1007/s11661-015-3215-7 ↗
16. M. Naghizadeh and M. H. Moayed, Corrosion Science 2015, vol. 94, pp. 179-89.10.1016/j.corsci.2015.01.051 ↗
17. Z. Wei, J. Laizhu, H. Jincheng and S. Hongmei, Materials Characterization 2009, vol. 60, pp. 50-55.10.1016/j.matchar.2008.07.002 ↗
18. Z. Zhang, H. Zhao, H. Zhang, Z. Yu, J. Hu, L. He and J. Li, Corros. Sci. 2015, vol. 93, pp. 120-25.10.1016/j.corsci.2015.01.014 ↗
19. L. Zhang, Y. Jiang, B. Deng, W. Zhang, J. Xu and J. Li, Materials Characterization 2009, vol. 60, pp. 1522-28.10.1016/j.matchar.2009.08.009 ↗
20. K. Ravindranath and S. N. Malhotra, Corros. Sci. 1995, vol. 37, pp. 121-32.10.1016/0010-938X(94)00120-U ↗
21. B. Deng, Z. Wang, Y. Jiang, T. Sun, J. Xu and J. Li, Corrosion Science 2009, vol. 51, pp. 2969-75.10.1016/j.corsci.2009.08.015 ↗
22. B. Deng, Z. Wang, Y. Jiang, H. Wang, J. Gao and J. Li, Electrochim. Acta 2009, vol. 54, pp. 2790-94.10.1016/j.electacta.2008.11.038 ↗
23. A. Bhattacharya and P. M. Singh, CORROSION 2008, vol. 64, pp. 532-40.10.5006/1.3278489 ↗
24. L. Pezzato, M. Lago, K. Brunelli, M. Breda and I. Calliari, J. Mater. Eng. Perform. 2018, vol. 27, pp. 3859-68.10.1007/s11665-018-3408-5 ↗
25. I. Calliari, M. Dabalà, E. Ramous and G. Straffelini, Mater. Sci. Forum 2009, vol. 604-605, pp. 419-26.
26. T. H. Chen, K. L. Weng and J. R. Yang, Mater. Sci. Eng. A 2002, 338, 259-70.10.1016/S0921-5093(02)00093-X ↗
27. E. A. Melo and R. Magnabosco, Metall. Mater. Trans. A 2017, vol. 48, pp. 5273-84.10.1007/s11661-017-4299-z ↗