journal article·2018-04

Effect of Low-Temperature Environment on Stress Corrosion Cracking Behavior of X80 Pipeline Steel in Simulated Alkaline Soil Solution

Fei Xie, Dan Wang, Ming Wu, Chengxiang Yu, Dongxu Sun, Xu Yang, Changhao Xu

Publisher page

Abstract

The stress corrosion cracking (SCC) of X80 pipeline steel in simulated alkaline soil solution under different temperatures was investigated by slow-strain-rate testing, scanning electron microscopy and energy-dispersive spectroscopy. Results showed that the fracture was transgranular and brittle at 273 K to 278 K (0 °C to 5 °C), and the metal surface was dissolved by a large number of chloride ions. Furthermore, hydrogen embrittlement was caused by the hydrogen atom extended to the high-stress region. The fracture process was controlled by hydrogen-induced cracking, and SCC was highly sensitive at this stage. At 288 K to 298 K (15 °C to 25 °C), the fracture morphology was attributed to the mixed mode of ductile and brittle fractures, the fracture process was controlled by the mechanism of hydrogen-induced cracking and anodic dissolution, and the susceptibility to SCC decreased. When the temperature reached 308 K to 318 K (35 °C to 45 °C), the fracture was mainly intergranular and ductile, the fracture process was controlled by anodic dissolution, and SCC sensitivity was the smallest in this temperature range.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. [1] Zhou M, Du L X, Zhao Y F: Journal of Wuhan University of Technology-Mater Sci Ed, 2012, vol. 27, pp. 252–55.10.1007/s11595-012-0447-x ↗
2. [2] Zhao Wei, Zou Yong, Matsuda Kenji: Mater. Des., 2016, vol. 99, pp. 44–56.10.1016/j.matdes.2016.03.036 ↗
3. [3] Wang Shuai-Xing, Liu Dao-Xin, Du Nan: Int. J. Electrochem. Sci., 2016, vol. 11, pp. 8797–8809.10.20964/2016.10.08 ↗
4. [4] Yan Mao-Cheng; Yang Shuang; Xu Jin:Acta Metall. Sin.,2016, vol. 52, pp. 1133–141.
5. [5] Xia Da-Hai, Wu Su-Bo, Zhu Yu: Electrochem., 2016, vol. 84, pp. 238–24210.5796/electrochemistry.84.238 ↗
6. Wang L.W., Liu Z.Y., Cui Z.Y., Du C.W.,Wang X.H., Li X.G.:Corros. Sci., 2014, pp. 401–410.10.1016/j.corsci.2014.04.053 ↗
7. Liu Z.Y., Li X.G., Du C.W., Lu L., Zhang Y.R., Cheng Y.F.: Corros. Sci., 2009, pp. 895-900.10.1016/j.corsci.2009.01.007 ↗
8. [9] Li Yong, Liu Zhi-Yong, Ke Le: Int. J. Electrochem. Sci., 2016, vol. 11, pp. 5021–5034.10.20964/2016.06.46 ↗
9. [10] Chen Wei-Xing: Corros., 2016, vol.72, pp. 962–977.10.5006/1967 ↗
10. [11] Liu, Z. Y., Wang, X. Z., Du, C. W.:Mater. Sci. Eng., 2016, vol. 658, pp. 348–354.10.1016/j.msea.2016.02.019 ↗
11. [12] Liu Zhi-Yong, Li Zong-Shu; Zhan XiaoLin: Acta Metall. Sin.,2016, vol. 52, pp. 965–972.
12. [13] Jeong Dae-Ho, Jung Woo-Jin, Kim YoungJu: Met. Mater. Int., .,2015, vol. 21, pp.785–792.10.1007/s12540-015-5132-0 ↗
13. Fan Lin, Liu Zhi-Yong, Guo, Wei-Min:Acta Metall. Sin. (Engl. Lett.),2015, vol. 28,pp.866–875.10.1007/s40195-015-0270-4 ↗
14. [15] Zhu M., Du C. W., Li X. G.: Corros., 2014,vol. 70, pp.1181–1188.10.5006/1232 ↗
15. [16] Zhu Min, Du Cui-Wei, Li Xiao-Gang: Corros. Sci.,2014, vol. 87, pp.224–232.10.1016/j.corsci.2014.06.028 ↗
16. [17] Zhao Wei, Zou Yong, Matsuda Kenji: Corros. Sci.,2016, vol. 70, pp.455–468.10.1016/j.corsci.2015.10.038 ↗
17. [18] Nie X H, Li X G, Du C W.: Electrochem., 2009, vol.39, pp. 277.10.1007/s10800-008-9669-1 ↗
18. [19] Wang Y H, Wen J.: Corros. Sci. Prot. Technol., 2000, vol.12, pp. 359.
19. [20] Paul Okonkwo C., Ahmed Essam, Mohamed A. M. A.: Int. J. Electrochem. Sci.,2015, vol. 10, pp. 10246–10260.10.1016/S1452-3981(23)11257-0 ↗
20. [21] Qi Ya-Meng, Luo Hong-Yun, Zheng Shu-Qi: Int. J. Electrochem. Sci.,2014, vol. 9, pp. 2101–2112.10.1016/S1452-3981(23)07914-2 ↗
21. Ye Cun-Dong, kong De-Jun,Zhang Lei: Journal of Central South University (Sci.Technol.),2015,vol.46, pp. 2432–2438.
22. [23] Guo Hao, Li Guang-Fu, Cai Xun: Acta Metall. Sin.,2004, vol. 40, pp. 967–971.
23. [24]Zhang Juan, Wei Cheng-Fu, Wang Zai-Jun:Tansactions of Mater. Treat.,2008, vol.28, pp.29–32.
24. [25] Fei Xie, Chang-Hao Xu, Dan Wang, Ming Wu, Hai-Yan Wang, Hong-Yu Xie: Iron Steel,2015, vol.50, pp.89–94.
25. [26]Zhou Jian-Long, Li Xiao-Gang, Du Cui-Wei, Li Yun-Ling,: Acta Metall. Sin.,2010,vol.42,pp251-256.10.3724/SP.J.1037.2009.00470 ↗
26. [27]Yao Xiao-Fei, Xie Fa-Qin, Wu Xiang-Qing: Oil Field Equipment,2012, vol.41, pp.50–53.
27. X.-S. Jiang, and H. Zhao: Austempered Ductile Cast Iron, Machinery Industry Press, Beijing. 2010
28. S.-X. Wang, D.-X. Liu, N. Du: Adv. Mater. Sci. Eng., 2015.
29. [30]Wu Ming, Zong Yue, Xie Fei, Zhao Qi-Hui, Zhang Xin, Dong Shi-Tong, Ge Lan: Heat Treat. Met.,2017,vol.02,pp.62-66.
30. Fei Xie, Dan Wang, Ming Wu,Jia-Liang Song, Kang-Nan Zhang, Xu Yang: Journal of Central South University(Sci.Technol.),2015, vol.2, pp.690–696.
31. Wiley-VCH Verlag GmbH & Co. KGaA, Weinheim, Basics of Corrosion Chemistry, 2011.
32. S.P. Trasatti , N.R. Moody, A.W. Thompson, R.E. Ricker: Hydrog. Eff. Mater. Behav. Corros., 2012.
33. [34]Wang Shuai-Xing, Liu Dao-Xin, Du Nan: Int. J. Electrochem. Sci.,2015, vol.10, pp.4393–4404.10.1016/S1452-3981(23)06631-2 ↗
34. Wan Dan, Xie Fei, Wu Ming, Chen Xu, Fu Yang, Zhang Wen-Jian, Ge Lan: Journal of Central South University (Sci.Technol.), 2014,vol.45,pp.2985-2992.
35. H. Luo, C.F. Dong, Z.Y. Liu, M.T.J. Maha, X.G. Li: Mater. Corros., 2013, vol. 64, pp. 26–33.10.1002/maco.201106146 ↗