High-Temperature Creep Degradation of the AM1/NiAlPt/EBPVD YSZ System
Source abstract
Abstract
The failure mechanisms of a NiAlPt/electron beam physical vapor deposition yttria-stabilized-zirconia thermal barrier coating system deposited on the AM1 single crystalline substrate have been investigated under pure creep conditions in the temperature range from 1273 K to 1373 K (1000 °C to 1100 °C) and for durations up to 1000 hours. Doubly tapered specimens were used allowing for the analysis of different stress states and different accumulated viscoplastic strains for a given creep condition. Under such experiments, two kinds of damage mechanisms were observed. Under low applied stress conditions (i.e., long creep tests), microcracking is localized in the vicinity of the thermally grown oxide (TGO). Under high applied stress conditions, an unconventional failure mechanism at the substrate/bond coat interface is observed because of large creep strains and fast creep deformation, hence leading to a limited TGO growth. This unconventional failure mechanism is observed although the interfacial bond coat/top coat TGO thickening is accelerated by the mechanical applied stress beyond a given stress threshold.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. M. Martena, D. Botto, P. Fino, S. Sabbadini, M. Gola and C. Badini, Eng. Fail. Anal., 2006, vol. 13, pp. 409-26 .10.1016/j.engfailanal.2004.12.027 ↗
2. R.C. Reed, The Superalloys - Fundamentals and Applications (Cambridge University Press, Cambridge UK, 2006).10.1017/CBO9780511541285 ↗
3. H.E. Evans, Surf. Coat. Tech., 2011, vol. 206, pp. 1512-21.10.1016/j.surfcoat.2011.05.053 ↗
4. D.S. Balint, T. Xu, J.W. Hutchinson and A.G Evans: Acta Mater., 2006, vol. 54, pp. 1815-20.10.1016/j.actamat.2005.12.008 ↗
5. R. Panat, S. Zhang and K.J. Hsia, Acta Mater., 2003, vol. 51, pp. 239-49.10.1016/S1359-6454(02)00395-6 ↗
6. V. Lughi, V. K. Tolpygo and D. R. Clarke, Mater. Sci. Eng. A, 2004, vol. 368, pp. 212-21.10.1016/j.msea.2003.11.018 ↗
7. R. G. Wellman, M. J. Deakin, and J. R. Nicholls, Trib. Int., 2005, vol. 38, pp. 798-804.10.1016/j.triboint.2005.02.008 ↗
8. C. Mercer, S. Faulhaber, A. G. Evans and R. Darolia, Acta Mater., 2005, vol. 53, pp. 1029-39.10.1016/j.actamat.2004.11.028 ↗
9. A.M. Karlsson, T. Xu, and A.G. Evans, Acta Mater., 2002, vol. 50, pp. 1211-18.10.1016/S1359-6454(01)00422-0 ↗
10. M.Y. He, D.R.Mumm and A.G. Evans, Surf. Coat. Tech., 2004, vol. 185, pp. 184-93.10.1016/j.surfcoat.2004.01.025 ↗
11. C. Courcier, V. Maurel, L. Rémy, S. Quilici, I. Rouzou and A. Phelippeau, Surf. Coat. Tech., 2011, vol. 205, pp. 3763-73.10.1016/j.surfcoat.2011.01.008 ↗
12. M. W. Chen, R. T. Ott, T. C. Hufnagel, P. K. Wright, and K. J. Hemker, Surf. Coat. Tech., 2003, vol. 163-164, pp. 25-30.10.1016/S0257-8972(02)00591-1 ↗
13. D. Pan, M. W. Chen, P. K. Wright and K. J. Hemker, Acta Mater., 2003, vol. 51, pp. 2205-17.10.1016/S1359-6454(03)00014-4 ↗
14. A. Bickard: Ph.D. Dissertation, Ecole des Mines de Paris, France, 1998.
15. J. L. Smialek, D. Zhu and M. D. Cuy, Scripta Mater., 2008, vol. 59, pp. 67-70.10.1016/j.scriptamat.2008.02.055 ↗
16. F. Riallant: Ph.D. Dissertation, ISAE-Ensma, France, 2013.
17. D. Seo, K. Ogawa, Y. Nakao, H. Miura, and T.Shoji, Surf. Coat. Tech., 2009, vol. 203, pp. 1979-83.10.1016/j.surfcoat.2009.01.029 ↗
18. A. G. Evans, D. R. Mumm, J. W. Hutchinson, G. H. Meier and F. S. Pettit, Prog. Mater. Sci., 2001, vol. 46, pp. 505-53.10.1016/S0079-6425(00)00020-7 ↗
19. G.C. Rybicki and J.L. Smialek, Oxid. Met., 1989, vol. 31, pp. 275-309.10.1007/BF00846690 ↗
20. J.B. Le Graverend, J. Cormier, P. Caron, S. Kruch, F. Gallereneau and J. Mendez Mater. Sci. Eng. A, 2011, vol. 528, pp. 2620-34.10.1016/j.msea.2010.11.081 ↗
21. T. Liang, H. Guo, H. Peng and S. Gong, J. Alloys Comp., 2011, vol. 509, pp. 8542-48.10.1016/j.jallcom.2011.05.102 ↗
22. V.G. Karaivanov, W.S. Slaugther, S. Siw, and M.K. Chyu: ASME Turbo Expo 2010: Power for Land, Sea and Air, ASME, Glasgow, UK, 2010, GT2010-23421.
23. G. Calvarin-Amiri, R. Molins and A. M. Huntz, Oxid. Met., 2000, vol. 53, pp. 399-426.10.1023/A:1004553623556 ↗
24. N. Roy, R.N. Ghosh, and M.C. Pandey, ISIJ International, 2001, vol. 41, pp. 915-21.10.2355/isijinternational.41.915 ↗
25. R. Viswanathan, Damage Mechanisms and Life Assessment of High Temperature Components (ASM International, Materials Park, OH, 1989).10.31399/asm.tb.dmlahtc.9781627083409 ↗
26. V.K. Tolpygo and D.R. Clarke, Acta Mater., 2000, vol. 48, pp. 3283-93.10.1016/S1359-6454(00)00156-7 ↗
27. V.K. Tolpygo and D.R. Clarke, Acta Mater., 2004, vol. 52, pp. 5115-27.
28. V.K. Tolpygo and D.R. Clarke, Acta Mater., 2004, vol. 52, pp. 5129-41.
29. S. V. Prikhidko and A. J. Ardell, Acta Mater., 2003, vol. 51, pp. 5001-12.10.1016/S1359-6454(03)00329-X ↗
30. S. V. Prikhidko and A. J. Ardell, Acta Mater., 2003, vol. 51, pp. 5013-19.10.1016/S1359-6454(03)00327-6 ↗
31. S. V. Prikhidko and A. J. Ardell, Acta Mater., 2003, vol. 51, pp. 5021-36.10.1016/S1359-6454(03)00328-8 ↗
32. W. Johnson and P. Voorhees, Metall. Trans. A, 1987, vol. 18A, pp. 1213-28.10.1007/BF02647191 ↗
33. X. Peng, D.R. Clarke and F. Wang,, Oxid. Met., 2003, vol. 60, pp. 225-40.10.1023/A:1026015101783 ↗
34. D.K. Das, Prog. Mat. Sci., 2013, vol. 58, pp. 151-82.10.1016/j.pmatsci.2012.08.002 ↗
35. P. Sallot: Ph.D. Dissertation, Ecole des Mines de Paris, Paris, France, 2012.
36. D. Texier: Ph.D. Dissertation, Université de Toulouse, ENSIACET, Toulouse, France, 2013.
37. E. P. Busso, H. E. Evans, Z. Q. Qian, and M. P. Taylor, Acta Mater., 2010, vol. 58, pp. 1242-51.10.1016/j.actamat.2009.10.028 ↗
38. M. D. Thouless, Thin Sol. Films, 1989, vol. 181, pp. 397-406.10.1016/0040-6090(89)90508-7 ↗
39. R. T. Wu, K. Kawagishi, H. Harada and R. C. Reed, Acta Mater., 2008, vol. 56, pp. 3622-29.10.1016/j.actamat.2008.03.046 ↗
40. J. A. Haynes, B. A. Pint, Y. Zhang and I. G. Wright, Surf. Coat. Tech., 2008, vol. 203, pp. 413-6.10.1016/j.surfcoat.2008.08.063 ↗
41. M. Gell, J. Eric, V. Krishnakumar, K. Mccaron, B. Barber, Y.-H. Sohn and V. K. Tolpygo, Surf. Coat. Tech., 1999, vol. 120-121, pp. 53-60.10.1016/S0257-8972(99)00338-2 ↗
42. J.R. Vaunois: in Thermal Barrier Coating III Conference, M.J. Maloney, U. Schulz, D. Rickerby, R. Darolia, O. Lavigne, H. Murakami, and H. Guo, eds., ECI, Irsee, Germany, 2011.