Hot Salt Stress Corrosion Cracking Behavior of Ti-6242S Alloy
Source abstract
Abstract
The hot salt stress corrosion cracking behavior of Ti-6A1-2Sn-4Zr-2Mo-0.1Si (Ti-6242S) alloy was studied in the temperature range from 523.15 K to 673.15 K (250 °C to 400 °C). The alloy showed marginal susceptibility at 573.15 K (300 °C), and the extent susceptibility found to increase significantly at higher test temperatures. The specimens did not fail in long-term (1000 hours) hot salt constant load exposure tests carried out at 623.15 K and 673.15 K (350 °C and 400 °C), even at the stress levels more than the 80 pct of their ultimate tensile strength. However, the salt exposure in both stressed and unstressed conditions found to significantly impair the room-temperature ductility. The study shows that pitting and formation of slip step were the precursor events for SCC initiation; and the cracks were found to grow in transgranular manner in the primary-α phase and discontinuous-faceted manner in the transformed β colony. Furthermore, the XRD analysis of hot salt-exposed specimens revealed the presence of titanium hydride phase, which could be responsible for the embrittlement.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. C. Leyens and M. Peters: Titanium and Titanium Alloys, Wiley, Weinheim, 2003, pp. 19–23, 239–249.10.1002/3527602119 ↗
2. G. Lütjering and J. C. Williams: Titanium, 2nd ed., Springer, New York, 2003, pp. 250–59.10.1007/978-3-540-71398-2 ↗
3. M. Peters, J. Kumpfert, C.H. Ward, and C. Leyens: Adv. Eng. Mater., 2003, vol. 5, pp. 419–27.10.1002/adem.200310095 ↗
4. R.R. Boyer: Mater. Sci. Eng. A, 1966, vol. 213, pp. 103–14.10.1016/0921-5093(96)10233-1 ↗
5. V.C. Petersen and H.B. Bomberger: ASTM STP, 1966, vol. 397, pp. 80–94.
6. M. Encrenaz, P. Faure, and J. A. Petit: Corros. Sci., 1998, vol. 40, pp. 939–50.10.1016/S0010-938X(98)00028-6 ↗
7. H.R. Gray: NASA Technical Note, D-6498, 1971.
8. R.G. Lingwall and E.J. Ripling: NASA Technical Report N67-38350, 1967.
9. M.D. Pustode, V.S. Raja, and N. Paulose: Corros. Sci., 2014, vol. 82, pp. 191–96.10.1016/j.corsci.2014.01.013 ↗
10. H.R. Gray and J.R. Johnston: Metall. Trans. A, 1970, vol. 1, pp. 3101–05.10.1007/BF03038425 ↗
11. R.K. Dinnappa: Key Eng. Mater., 1988, vol. 20–28, pp. 2255–71.
12. S.P. Rideout, M.R. Louthan, and J.C.L. Selby: ASTM STP, 1966, vol. 397, pp. 137–51.
13. R.L. Kirchner and E.J. Ripling: NASA Technical Note, N65-82069, 1964.
14. H.R. Gray: NASA Technical Note, D-6188, 1971.
15. J.D. Jackson and W.K. Boyd: DMIC Technical Note, 1966.
16. G. Heimerl, D. Braski, D. Royster and H. Dexter: ASTM STP, 1966, vol. 397, pp. 194–14.
17. H. Dexture: NASA Technical Note, D-3299, 1966.
18. Standard Test Methods for Tension Testing of Metallic Materials, ASTM E8.
19. K. Prasad and V.K. Varma: Mater. Sci. Eng. A, 2008, vol. 486, pp. 158–66.10.1016/j.msea.2007.09.020 ↗
20. B.S. Padekar, R.K. Singh Raman, V.S. Raja, and L. Paul: Corros. Sci., 2013, vol. 71, pp. 1–9.10.1016/j.corsci.2013.01.001 ↗
21. G.H. Koch, A.J. Bursle, and E.N. Pugh: Metall. Trans. A, 1978, vol. 9A, pp. 129–31.10.1007/BF02647182 ↗
22. V.C. Petersen: J. Met., 1971, vol. 23, pp. 40–47.
23. R.S. Ondrejcin: Metall. Trans., 1970, vol. 1, pp. 3031–36.10.1007/BF03038416 ↗
24. M. Garfinkle: Metall. Trans., 1973, vol. 4, pp. 1677–86.10.1007/BF02666196 ↗
25. M.W. Mahoney and A.S. Tetelman: Metall. Trans. A, 1976, vol. 7A, pp. 1579–58.
26. N.E. Paton and R.A. Spurling: Metall. Trans. A, 1976, vol. 7A, pp. 1769–74.10.1007/BF02817895 ↗
27. D.A. Meyn: Metall. Trans., 1974, vol. 5, pp. 2405–14.10.1007/BF02644024 ↗
28. E. Tal-Gutelmacher and D. Eliezer: Mater. Trans., 2004, vol. 45, pp. 1594–1600.10.2320/matertrans.45.1594 ↗
29. H.J. Christ, M. Decker, and S. Zeitler: Metall. Trans. A, 2000, vol. 31A, pp. 1507–17.10.1007/s11661-000-0161-8 ↗