Abstract

The influence of chloride ion activity on the susceptibility of aluminum alloys 5083-H131 and 7075-T6 to stress corrosion cracking (SCC) was investigated by conducting slow strain-rate tensile tests at a strain-rate of 10−7 s−1 in naturally aerated aqueous solutions with varying NaCl mass fraction (0.001 to 20 pct) and in a 3.5 pct mass fraction NaCl solution with varying strain-rates (10−8 to 10−4 s−1). This study found that both alloys exhibited reduced strengths and failure strains (times) in the solutions compared with laboratory air. The extent of these reductions was greater in alloy 5083 for the conditions examined. The strength and ductility of both alloys decreased with chloride ion activity in a manner that indicates a chemical reaction is responsible. The strength and ductility of both alloys decreased with strain-rate in a sigmoidal manner, but the transition in alloy 7075 occurred at slower strain-rates of approximately two orders of magnitude. It was deduced that the chloride ion interacts chemically with the passivated surface in the potential gradient at the crack tip to cause SCC. While no mechanism of cracking can be eliminated on the basis of these results alone, the results are consistent with the hypothesis that the absorbed hydrogen causes cracking in alloy 7075 while cracking in 5083 is the result of a dissolution mechanism.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. E. Deltombe, C. Vanleugenhaghe, and M. Pourbaix: in Atlas of Electrochemical Equilibria in Aqueous Solutions, M. Pourbaix, ed., NACE Intl., Houston, TX, 1974, pp. 168–76.
2. R.E. Ricker and D.J. Duquette: Metall. Trans. A, 1988, vol. 19A, pp. 1775–83.10.1007/BF02645146 ↗
3. M.R. Stoudt, A.K. Vasudevan, and R.E. Ricker: in Corrosion Testing of Aluminum Alloys. V.S. Agarwala and G. Ugiansky, eds., Vol. STP-1134, ASTM, Phila. PA., San Francisco, CA, 1992, pp. 196–213.10.1520/STP19590S ↗
4. E. Ghali: Corrosion Resistance of Aluminum and Magnesium Alloys: Understanding, Performance, and Testing, John Wiley & Sons, Inc., New York, 2010.10.1002/9780470531778 ↗
5. H.P. Goddard, W.B. Jepson, M.R. Bothwell, and R.L. Kane: The Corrosion of Light Metals, John Wiley & Sons, Inc., New York, 1967.
6. J. Kruger: Int. Mater. Rev., 1988, vol. 33, pp. 113–30.10.1179/095066088790324166 ↗
7. R.T. Foley: Corrosion, 1986, vol. 42, pp. 277–88.10.5006/1.3584905 ↗
8. D.D. Wagman, W.H. Evans, V.B. Parker, R.H. Schumm, I.Halow, S.M. Bailey, K.L. Churney, and R. L. Nuttall: J. Phys. Chem. Ref. Data, 1982, vol. 11, pp. 1–392.10.1063/1.555661 ↗
9. Z.A. Foroulis and M.J. Thubrikar: J. Electrochem. Soc., 1975, vol. 122, pp. 1296–1301.10.1149/1.2134003 ↗
10. G.S. Frankel, J. Electrochem. Soc., 1998, vol. 145, pp. 2186–98.10.1149/1.1838615 ↗
11. N.J.H. Holroyd and D. Hardie: Corros. Sci., 1981, vol. 21, p. 129.10.1016/0010-938X(81)90097-4 ↗
12. D. Hardie, N.J.H. Holroyd, and R.N. Parkins: Met. Sci., 1979, vol. 13, pp. 603–10.10.1179/msc.1979.13.11.603 ↗
13. J.L. Searles, P.I. Gouma, and R.G. Buchheit: Metall. Mater. Trans. A, 2001, vol. 32A, pp. 2859–67.10.1007/s11661-001-1036-3 ↗
14. T.D. Burleigh: Corrosion, 1991, vol. 47, pp. 89–98.10.5006/1.3585235 ↗
15. F.J. Bradshaw and C. Wheeler: Int. J. Fract. Mech., 1969, vol. 5, p. 255.10.1007/BF00190956 ↗
16. G.M. Scamans, R. Alani, and P.R. Swann: Corros. Sci., 1976, vol. 16, pp. 443–59.10.1016/0010-938X(76)90065-2 ↗
17. G.A. Young and J.R. Scully: Metall. Mater. Trans. A, 2002, vol. 33, p. 101–15.10.1007/s11661-002-0009-5 ↗
18. N.J.H. Holroyd and G.M. Scamans: Metall. Mater. Trans. A, 2011, vol. 42A, pp. 3979–98.10.1007/s11661-011-0793-x ↗
19. R.N. Parkins: in Stress Corrosion Cracking: The Slow Strain-Rate Technique, G.M. Ugiansky and J.H. Payer, eds., Vol. STP 665, ASTM, Phila. PA, 1979, pp. 5–25.10.1520/STP38106S ↗
20. J.H. Payer, W.E. Berry, and W.K. Boyd: in Stress Corrosion Cracking: The Slow Strain-Rate Technique, G.M. Ugiansky and J.H. Payer, eds., Vol. STP 665, ASTM, Phila. PA, 1979, pp. 61–77.10.1520/STP38109S ↗
21. R.N. Parkins: in Slow Strain-rate Testing for the Evaluation of Environmentally Induced Cracking: Research and Engineering Applications, R.D. Kane, ed., Vol. ASTM STP 1210, American Society for Testing and Materials, Phil., PA, 1993, pp. 7–21.10.1520/STP12751S ↗
22. J.A. Beavers and G.H. Koch: in Slow Strain-rate Testing for the Evaluation of Environmentally Induced Cracking, R.D. Kane, ed., ASTM STP, Vol. 1210, American Society for Testing and Materials, Phil., PA, 1993, pp. 22–39.
23. ASTM: in Annual Book of ASTM Standards, Vol. 03.02, ASTM Intl., West Conshohocken, PA, 2006.
24. T.B. Cassagne, J. Kruger, and E.N. Pugh: in Environmentally Assisted Cracking: Science and Engineering, W.B. Lisagor, T.W. Crooker, and B.N. Leis, eds., Vol. STP 1049, ASTM, Phila., PA, 1989, p. 59–75.
25. T.B. Cassagne: PhD Dissertation, The Johns Hopkins University, 1988.
26. U. Bertocci, E.N. Pugh, and R.E. Ricker: in Environment-Induced Cracking of Metals, R.P. Gangloff and M. B. Ives, eds., NACE Intl., Houston, TX, 1990, pp. 273–86.
27. G.L. Bianchi and J. R. Galvele: Corro. Sci., 1993, vol. 34, pp. 1411–22.10.1016/0010-938X(93)90237-B ↗
28. S.B. Farina, G.S. Duffo, and J.R. Galvele: Corro. Sci., 2005, vol. 47, pp. 239–45.10.1016/j.corsci.2004.05.019 ↗
29. R.E. Ricker: J. Met., 1995, vol. 47, pp. 32–35.
30. R.E. Ricker: in Hydrogen Effects on Materials Behavior and Corrosion Deformation Interactions, N.R. Moody, A.W. Thompson, R.E. Ricker, G.S. Was, and R.H. Jones, eds., TMS, Warrendale, PA, 2003, pp. 629–38.
31. R.E. Ricker: J. ASTM Int., 2008, vol. 5, p. 10.10.1520/JAI101350 ↗
32. P.W. Slattery, J. Smit, and E.N. Pugh; in Environmental Sensitive Fracture: Evaluation and Comparison of Test Methods, S.W. Dean, E.N. Pugh, and G.M. Ugiansky, eds., Vol. STP-821, ASTM, Phila., PA, 1984, p. 399–411.10.1520/STP34445S ↗
33. C.D. Kim and B.E. Wilde: in Stress Corrosion Cracking: The Slow Strain-Rate Technique, G.M. Ugiansky and J.H. Payer, eds., Vol. STP 665, ASTM, Phila. PA, 1979, pp. 97–112.10.1520/STP38111S ↗
34. R.E. Ricker: Properties of NaCl Solutions at 25 °C that Influence Corrosion Reactions and SCC, National Institute of Standards and Technology, 2012, p. 10.
35. W.J. Hamer and Y.-C. Wu: J. Chem. Ref. Data, 1972, vol. 1, p. 1047–99.10.1063/1.3253108 ↗
36. C.-F. Pan: J. Chem. Eng. Data, 1981, vol. 26, pp. 183–84.10.1021/je00024a028 ↗
37. J.I. Partanen and P.O. Minkkinen: Acta Chem. Scand., 1993, vol. 47, p. 768–76.10.3891/acta.chem.scand.47-0768 ↗
38. J.I. Partanen and A.K. Covington: J. Chem. Eng. Data, 2009, vol. 54, p. 208–19.10.1021/je800188a ↗
39. V.M.M. Lobo and J.L Quaresma: Electrolyte Solutions: Literature Data on Thermodynamic and Transport Properties, Vol. 2 Published by the author, Coimbra, Portugal, 1981.
40. J.I. Partanen: J. Chem. Eng. Data, 2009, vol. 54, pp. 882–889.10.1021/je800680u ↗
41. W. Mendenhall and T. Sincich, Statistics for Engineering and the Sciences, Dellen Publ. Co., San Francisco, 1992.
42. S.W. Ciraldi, Ph.D. Dissertation, Univ. of Illinois, 1980.
43. S.W. Ciraldi, J.L. Nelson, R.A. Yeske, and E.N. Pugh, in Hydrogen Effects in Metals, I.M.B.A.W. Thompson ed., TMS/AIME, New York, 1981, p. 437.
44. N.J.H. Holroyd and G.M. Scamans: in Environment-Sensitive Fracture: Evaluation and Comparison of Test Methods, S.W. Dean, E.N. Pugh, and G.M. Ugiansky, eds., Vol. STP-821, ASTM, Phil. PA, 1984, pp. 202–41.
45. M. Khobaib and C.T. Lynch: in Environment-Sensitive Fracture: Evaluation and Comparison of Test Methods, S.W. Dean, E.N. Pugh, and G.M. Ugiansky, eds., Vol. STP 821, ASTM, Phil. PA, 1984, pp. 242–55.
46. H. H. Uhlig and R. W. Revie, Corrosion and Corrosion Control, 4th ed. John Wiley & Sons, New York, 2008.
47. H. Bohni and H. H. Uhlig: J. Electrochem. Soc., 1969, vol. 116, p. 906.10.1149/1.2412167 ↗
48. R.E. Ricker and D.J. Duquette: in Aluminum Lithium Alloys II, T.H. Sanders and E.A. Starke, eds., The Metallurgy Society of AIME, Warrendale, PA, 1984, pp. 581–96.
49. R.H. Jones and R.E. Ricker: in Metals Handbook Ninth Edition Vol. 13: Corrosion, J.R. Davis, ed., ASM Intl., Materials Park, OH, 1987, pp. 145–63.
50. R.H. Jones and R.E. Ricker: in Stress-Corrosion Cracking: Materials Performance and Evaluation, R.H. Jones, ed., ASM Intl., Materials Park, OH, 1992, p. 1-40.10.31399/asm.tb.sccmpe2.t55090001 ↗
51. R.T. Foley: J. Electrochem. Soc., 1975, vol. 122, pp. 1493–94.10.1149/1.2134051 ↗
52. R.T. Foley, I&EC product R&D, 1978, vol. 17, p. 14.10.1021/i360065a005 ↗
53. S.A. Matwiyoff and W.E. Wageman: Inorg. Chem., 1970, vol. 9, pp. 1031–36.10.1021/ic50087a006 ↗
54. X. Jin, W. Yang, Z. Qian, Y. Wang, and S. Bi: Dalton Trans., 2011, vol. 40, pp. 5052–58.10.1039/c0dt01822h ↗
55. M. Dietzel and G. Bohme, Geochim. Cosmochim. Acta, 2005, vol. 69, pp. 1199–11.10.1016/j.gca.2004.08.027 ↗
56. D.J. Wesolowski, D.A. Palmer, and P. Benezeth: Geochim. Cosmochim. Acta, 2006, vol. 70, pp. 2140–42.10.1016/j.gca.2005.10.038 ↗
57. H. Buhl, in Stress Corrosion Cracking-The Slow Strain-Rate Technique, G.M. Ugiansky and J.H. Payer, eds., Vol. STP-665, ASTM, Phil. PA, 1979, pp. 333–46.10.1520/STP38125S ↗
58. G.M. Ugiansky, C.E. Johnson, D.S. Thompson, and E.H. Gillespie: in Stress Corrosion Cracking: The Slow Strain-Rate Technique, G.M. Ugiansky and J.H. Payer, eds., Vol. STP 665, ASTM, Phila. PA, 1979, pp. 254–65.10.1520/STP665-EB ↗
59. F.P. Ford and P.L. Andresen, in Corrosion Mechanisms in Theory and Practice, P. Marcus and J. Oudar, eds., Marcel Dekker, Inc., New York, 1995, pp. 501–46.