journal article·2016-05

Wear Behavior and Mechanism of Fe-Al Intermetallic Coating Prepared by Hot-Dip Aluminizing and Diffusion

Q. Y. Zhang, Y. Zhou, J. Q. Liu, K. M. Chen, J. G. Mo, X. H. Cui, S. Q. Wang

Publisher page

Abstract

A Fe-Al intermetallic compound coating was prepared on AISI H13 steel by hot-dip aluminizing and subsequent high-temperature diffusion. Dry sliding wear tests of the Fe-Al intermetallic coating were performed at 298 K to 873 K (25 °C to 600 °C). The wear behavior of the Fe-Al intermetallic coating was noticed to vary markedly with the temperature and load. At 298 K (25 °C), the wear rate rapidly increased with an increase of the load. As the temperature was elevated, the wear rate dramatically decreased except for the cases under 300 N at 473 K and 673 K (200 °C and 400 °C). The Fe-Al intermetallic coating possessed an excellent elevated-temperature wear performance, especially at 673 K to 873 K (400 °C to 600 °C), but worse room-temperature one, which were noticed to be attributed to the existence and inexistence of thin tribo-oxide layers, respectively. Such a thin tribo-oxide layer was considered to provide a protection for the intermetallic compound. When the tribo-oxide layer did not form at room temperature or the formed one was massively delaminated above the critical load at elevated temperatures, Fe-Al intermetallic coating possessed poor wear resistance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · High-Temperature Coating Behaviors · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. N.S. Stoloff: Mater. Sci. Eng. A, 1998, vol. 258, pp.1-14.10.1016/S0921-5093(98)00909-5 ↗
2. C.G. McKamey, J.H. DeVan, P.F. Tortorell, V.K. Sikka: J. Mater. Res. 1991, vol. 6, pp. 1779-1805.10.1557/JMR.1991.1779 ↗
3. H.E. Maupin, R.D. Wilson, J.A. Hawk: Wear, 1993, vol.162-164, pp.432-440.10.1016/0043-1648(93)90527-S ↗
4. J.L. Jordan, S.C. Deevi: Intermetallics, 2003, vol.11, pp. 507-528.10.1016/S0966-9795(03)00027-X ↗
5. C.J. Li, H.T. Wang, G.J. Yang, and C.G. Bao: J. Therm. Spray Technol, vol. 20, pp. 227–33.
6. S.M. Zhu, X.S. Guan, K. Shibata, K. Iwasaki: Mater. Trans., 2002, vol.43, pp. 36-41.10.2320/matertrans.43.36 ↗
7. C.T. Liu, E.H. Lee, C.G. McKamey: Script Metall., 1989, vol. 23, pp. 875-880.10.1016/0036-9748(89)90263-9 ↗
8. C.T. Liu, E.P. George, P.J. Maziasz, J.H. Schneibel: Mater. Sci. Eng. A, 1998, vol. 258, pp. 84-98.10.1016/S0921-5093(98)00921-6 ↗
9. J. Qiu, I. Baker, F.E. Kennedy, Y. Liu, P.R. Munroe: Intermetallics, 2013, vol.40, pp. 19-27.10.1016/j.intermet.2013.03.020 ↗
10. Y.S. Kim, Y.H. Kim: Mater. Sci. Eng. A, 1998, vol. 258, pp. 319-324.10.1016/S0921-5093(98)00951-4 ↗
11. Y.P. Bai, J.D. Xing, S.. Ma, Q. Huang, Y.Y. He, Z. Liu, Y.M. Gao: Mater. Character,. 2013, vol. 78, pp. 69-78.10.1016/j.matchar.2013.01.014 ↗
12. D.E. Alman, J.A. Hawk, J.H. Tylczak, C.P. Dogan, R.D. Wilson: Wear, 2001, vol. 251, pp. 875–884.10.1016/S0043-1648(01)00745-1 ↗
13. G. Sharma, P.K. Limaye, R.V. Ramanujan, M. Sundararaman, N. Prabhu: Mater. Sci. Eng. A, 2004, vol. 386, pp. 408-414.10.1016/S0921-5093(04)00999-2 ↗
14. Sharma G, Sundararaman M, Prabhu N, Goswami GL. Sliding wear resistance of iron aluminides. Bull Mater Sci 2003;26: 311-314.10.1007/BF02707452 ↗
15. J. Li, Y.S. Yin, H.T. Ma: Tribol. Int., 2005, vol. 38, pp. 159-163.10.1016/j.triboint.2004.07.024 ↗
16. J. Yang, P.Q. La, W.M. Liu, J.Q. Ma, Q.J. Xue: Intermetallics, 2005, vol. 13, pp. 1184-1189.10.1016/j.intermet.2005.03.005 ↗
17. J. Yang, P.Q. La, W.M. Liu, Q.J. Xue: Wear, 2004, vol. 257, pp. 104-109.10.1016/j.wear.2003.10.012 ↗
18. J. Wang, J.D. Xing, L. Cao, W. Su, Y.M. Gao: Wear, 2010, vol. 268, pp. 473–480.10.1016/j.wear.2009.09.006 ↗
19. X.H. Zhang, J.Q. Ma, L.C. Fu, S.Y. Zhu, F. Li, Jun Yang, W.M. Liu: Tribol. Int., 2013, vol. 61, pp. 48-55.10.1016/j.triboint.2012.12.005 ↗
20. P. Nagpal, I. Baker: Mater. Character., 1991, vol. 27, pp. 167-173.10.1016/1044-5803(91)90060-H ↗
21. P.J. Blau, C.E. DeVore: Trans. ASME, 1988, vol. 110, pp. 646-652.10.1115/1.3261707 ↗
22. N.R. Bonda, D.A. Rigney: Mat. Res. Soc. Symp. Proc., 1989, vol. 133, pp. 585-590.10.1557/PROC-133-585 ↗
23. Y.L. Liao: Master Dissertation of Jiangsu University, Zhenjiang, 2014.
24. S. Kobayashi, T. Yakou: Mater. Sci. Eng. A, 2002, vol. 338, pp. 44–53.10.1016/S0921-5093(02)00053-9 ↗
25. K.M. Chen, Q.Y. Zhang, X.X. Li, L. Wang, X.H. Cui, S.Q. Wang: Tribol. Trans., 2014, vol. 57, pp. 838-845.10.1080/10402004.2014.916372 ↗
26. S.Q. Wang, M.X Wei, F. Wang, X.H. Cui, C. Dong: Tribol. Lett., 2008, vol. 32, pp. 67-72.10.1007/s11249-008-9361-y ↗
27. Q.Y. Zhang, K.M. Chen, L. Wang, X.H. Cui, S.Q. Wang: Tribol. Int., 2013, vol. 61, pp. 214–223.10.1016/j.triboint.2013.01.003 ↗
28. M. Kerridge: Proc. Phys. Soc. B, 1955, vol. 68, pp. 400-408.10.1088/0370-1301/68/7/302 ↗
29. D.A. Rigney: Wear, 1992, vol. 152, pp. 187-192.10.1016/0043-1648(92)90214-S ↗
30. F.H. Stott, M. P. Jordan: Wear, 2001, vol. 250, pp. 391-400.10.1016/S0043-1648(01)00601-9 ↗
31. A. Pauschitza, M. Roy, F. Franek: Tribol. Int., 2008, vol. 41, pp. 584–602.10.1016/j.triboint.2007.10.003 ↗
32. H. Kato: Wear, 2003, vol. 255, pp. 426-429.10.1016/S0043-1648(03)00077-2 ↗
33. Z.C. Lu, M.Q. Zeng, Y. Gao, M. Zhu: Wear, 2013, vol. 304, pp. 162–172.10.1016/j.wear.2013.05.001 ↗
34. M. Koeppe, Ch. Hartig, H. Mecking: Intermetallics, 1999, vol. 7, pp. 415-422.10.1016/S0966-9795(98)00111-3 ↗
35. M. Kupka: Intermetallics, 2006, vol.14, pp. 149-155.10.1016/j.intermet.2005.04.013 ↗