journal article·2011-07

High-Temperature Erosion-Corrosion Performance of High-Velocity Oxy-Fuel Sprayed Ni-20 Cr Coating in Actual Boiler Environment

G. Kaushal, H. Singh, S. Prakash

Publisher page

Abstract

The high-velocity oxy-fuel (HVOF) spray technique was used to deposit Ni-20Cr coating on a commonly used boiler steel ASTM A213 347H. The specimens with and without coating were exposed to the super heater zone of a thermal power plant boiler at a temperature of 973 K (700 °C) under cyclic conditions to ascertain their erosion-corrosion (E-C) behavior. High-temperature oxidation behavior of the specimens was also evaluated under cyclic thermal loading conditions at an elevated temperature of 1173 K (900 °C). Mass change data and thickness loss were measured to formulate the kinetics of E-C/oxidation for the specimens. The exposed specimens were characterized by X-ray diffraction (XRD) and field emission–scanning electron microscopy/energy dispersive spectroscopy (FE-SEM/EDS). The uncoated steel suffered higher E-C in comparison with its coated counterpart in terms of mass loss as well as thickness loss. It was observed that overall mass loss was reduced by 31 pct and thickness loss by 44 pct after the application of the coating. The possible formation of Cr2O3 phase in the coated substrate may be suggested to contribute to better E-C behavior. During air oxidation exposures, the coating was found to be intact with only marginal spallation of its oxide scales, which is an indicator of good adhesion between the coating and substrate steel. The air oxidation mass change data indicated that the coating enhanced the oxidation resistance of the steel by 85 pct.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Erosion and Abrasive Machining · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. M.H. Li, X.F. Sun, J.G. Li, Z.Y. Zhang, T. Jin, H.R. Guan, and Z.Q. Hu: Oxid. Met., 2003, vol. 59, p. 591–605.10.1023/A:1023604214245 ↗
2. S. Watanabe and S. Yamamoto: Jpn. Inst. Mater., 1977, vol. 47, p. 26–29.
3. A. Motoki and M. Yoaiba: Jpn. Soc. Corr. Eng., 1990, vol. 39, p. 192.
4. Y. Matsubara and A. Tomiguchi: Proc. 13th Int. Thermal Spray Conf., Orlando, FL, ASM International, Materials Park, OH, 1992, p. 637.
5. L. Byrnes and M. Kramer: Proc. 7th National Thermal Spray Conf., Boston, MA, ASM International, Materials Park, OH, 1994, p. 39.
6. Metals Handbook, ASM, Metals Park, OH, 1975, vol. 10.
7. T. Sundararajan, S. Kuroda, and F. Abe: Metall. Mater. Trans. A, 2004, vol. 35A, p. 3187–99.10.1007/s11661-004-0063-2 ↗
8. K. Yamada, Y. Tomono, J. Morimoto, Y. Sasaki, and A. Ohmori: Vacuum, 2002, vol. 65, p. 533–40.10.1016/S0042-207X(01)00468-7 ↗
9. A.J. Minchener and J.E. Oakey: J. Phys., 1993, vol. IV, C9 (3), p. 679–86.
10. A.V. Levy and Y.F. Man: Wear, 1986, vol. 111, p. 135–59.10.1016/0043-1648(86)90216-4 ↗
11. J. Zhou and S. Bahadur: Proc. Conf. on Corrosion and Particle Erosion at High Temperature, TMS, Warrendale, PA, 1989, p. 313.
12. T. Singh and G. Sundrajan: Metall. Trans. A, 1990, vol. 21A, p. 3187–99.10.1007/BF02647314 ↗
13. A.V. Levy and P. Crook: Wear, 1991, vol. 151, p. 337–50.10.1016/0043-1648(91)90260-2 ↗
14. R. Norling and I. Olefjord: Wear, 2003, vol. 254, p. 173–84.10.1016/S0043-1648(02)00299-5 ↗
15. B.S. Sidhu and S. Prakash: Metall. Mater. Trans. A, 2006, vol. 37A, p. 1927–36.10.1007/s11661-006-0135-6 ↗
16. G. Kaushal, H. Singh, and S. Prakash: Proc. Int. Thermal Spray Conf. Expo, Maastricht, The Netherlands, ASM International, Materials Park, OH, 2008, p. 1351.
17. G. Kaushal, H. Singh, and S. Prakash: Proc. Int. Thermal Spray Conf. Expo, Las Vegas, NV, 2009, ASM International, Materials Park, OH, p. 685.10.31399/asm.cp.itsc2009p0685 ↗
18. L. Gil and M.H. Staia: Thin Solid Films., 2002, vols. 420–421, p. 446–54.10.1016/S0040-6090(02)00815-5 ↗
19. J.M. Miguel, J.M. Guilemany, and S. Vizcaino: Tribol. Int., 2003, vol. 36, p. 181–87.10.1016/S0301-679X(02)00144-5 ↗
20. M.M. Helali and M.S.J. Hashmi: Proc. 10th Conf. of the Irish Manufacturing Committee (IMC 10), Irish Manufacturing Committee, Ireland, 1992, p. 377.
21. M.E. Aalamialeagha, S.J. Harris, and M.J. Emamighomi: Mater. Sci., 2003, vol. 38, p. 4587–96.10.1023/A:1027302122749 ↗
22. N.F. Ak, C. Tekmen, I. Ozdemir, H.S. Soykan, and E. Celik: Surf. Coat. Technol., 2003, vols. 173–174, p. 1070–73.10.1016/S0257-8972(03)00367-0 ↗
23. B.S. Sidhu: Ph.D. Thesis, Metals and Materials Engineering Department, IITR, Roorkee, India, 2003.
24. B.S. Sidhu and S. Prakash: Wear, 2006, vol. 260, pp. 1035–44.10.1016/j.wear.2005.07.003 ↗
25. T. Sidhu: Ph.D. Thesis, IITR, Roorkee, India, 2006.
26. T.S. Sidhu, R.D. Agrawal, and S. Prakash: Surf. Coat. Technol., 2006, vol. 201 (3–4), p. 1602–12.10.1016/j.surfcoat.2006.02.047 ↗
27. D. Das, R. Balasubramaniam, and M.N. Mungole: J. Mater. Sci., 2002, vol. 37 (6), p. 1135–48.10.1023/A:1014307219963 ↗
28. R. Kumar, V.K. Tewari, and S. Prakash: Metall. Mater. Trans. A, 2007, vol. 38A, p. 54–57.10.1007/s11661-006-9053-x ↗
29. T.S. Sidhu, R.D. Agrawal, and S. Prakash: J. Mater. Eng. Performance, 2006, vol. 15 (1), p. 130–38.10.1361/105994906X83411 ↗
30. T.S. Sidhu, R.D. Agrawal, and S. Prakash: Metall. Mater. Trans. A, 2007, vol. 38A, p. 77–85.10.1007/s11661-006-9002-8 ↗
31. S. Singh, D. Puri, and S. Prakash: Metall. Mater. Trans. A, 2005, vol. 36A, p. 1007–15.10.1007/s11661-005-0294-x ↗
32. Ul-Hamid: Mater. Chem. Phys., 2003, vol. 80, p. 135–42.10.1016/S0254-0584(02)00448-0 ↗
33. T. Sundararajan, S. Kuroda, T. Itagaki, and F. Abe: Iron Steel Inst. Jpn. Int., 2003, vol. 43 (1), p. 104–11.10.2355/isijinternational.43.104 ↗
34. M.F. Stroosnijder, R. Mevrel, and M.J. Bennet: Mater. High Temp., 1994, vol. 12 (1), pp. 53–66.10.1080/09603409.1994.11689470 ↗
35. S. Kamal, R. Jayaganthan, S. Prakash, and S. Kumar: J. Alloys Compd., 2008, vol. 463, (1–2), p. 358–72.10.1016/j.jallcom.2007.09.019 ↗
36. F.H. Stott: The Role of Active Elements in the Oxidation Behavior of High Temperature Metals and Alloys, E. Lang, ed., Elsevier Applied Science, London, 1998.
37. U.K. Chatterjee, S.K. Bose, and S.K. Roy: Environmental Degradation of Metals, Marcel Dekker, New York, NY, 2001.10.1201/9781482292244 ↗