journal article·2006-10

Strength distribution of fatigue crack initiation sites in an Al-Li alloy

T. Zhai

Publisher page

Abstract

The stress-number of cycles to failure (S-N) curves were measured along the short-transverse (S) and rolling (L) directions of a hot-cross-rolled AA 8090 Al-Li alloy plate (45-mm thick). The alloy was solution heat treated, quenched in water, strained by 6 pct, and peak aged. Fatigue tests were carried out in four-point bend at room temperature, 20 Hz, R=0.1, in air. It was found that the fatigue limits in the S and L directions were 147 and 197 MPa, respectively. The crack population on the surface of a sample at failure increased with the applied stress level and was found to be a Weibull function of the applied maximum stress in this alloy. The strength distribution of fatigue weakest links, where cracks were initiated, was derived from the Weibull function determined by the experimental data. The fatigue weakest-link density was defined as the crack population per unit area at a stress level close to the ultimate tensile stress and can be regarded as a materials property. The density and strength distribution of fatigue weakest links were found to be markedly different between the L and S directions, accounting for the difference in fatigue limit between the directions in this alloy. They were also found to be different between S-L and S-T samples, and between L-T and L-S samples of this alloy, which could not be revealed by the corresponding S-N curves measured. These differences were due to the anisotropy of the microstructures in different directions in this alloy.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Fatigue and fracture mechanics · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Proc. Short Course, D.E. Hardenbergh, ed., Pennsylvania State University, University Park, PA, 1956.
2. A.B.O. Soboyejo, I.R. Orisamolu, and W.O. Soboyejo: Probalistic Methods in Fatigue and Fracture, Trans Tech Publications Ltd., Aedermannsdorf, Switzerland, 2001.10.4028/b-gW2FJe ↗
3. P.C. Gope: J. Eng. Mater. Technol., 1999, vol. 124, pp. 421–27.10.1115/1.1417486 ↗
4. S.J. Hudak, Jr., D. Slavik, A. Nagy, J.H. Feiger, and G.G. Chell: Proc. 6th Nat. Turbine Engine High Cycle Fatigue (HCF) Conf., Jacksonville, FL, 2001, pp. 112–21.
5. D.B. Lanning, T. Nicholas, and A. Palazotto: Int. J. Fatigue, 2003, vol. 25, pp. 835–41.10.1016/S0142-1123(03)00156-7 ↗
6. D. Shan and H. Nayeb-Hashemi: NDT E Int., 1999, vol. 32, pp. 265–74.10.1016/S0963-8695(98)00053-X ↗
7. Y.X. Zhao: Mater. Sci. Eng, 2003, vol. A344, pp. 229–39.10.1016/S0921-5093(02)00392-1 ↗
8. S.J. Kim, Y.S. Kim, and S.W. Kwon: Key Eng. Mater., 2004, vols. 261–263, pp. 1275–80.10.4028/www.scientific.net/KEM.261-263.1275 ↗
9. H.D. Dudgeon: Ph.D. Thesis, University of Oxford, Oxford, United Kingdom, 1990.
10. T. Zhai, A.J. Wilkinson, J.W. Martin, and I.G. Palmer: Mater. Sci. Forum, 2000, vols. 331–337, pp. 1549–54.10.4028/www.scientific.net/MSF.331-337.1549 ↗
11. T. Zhai, Y.G. Xu, J.W. Martin, A.J. Wilkinson, and G.A.D. Briggs: Int. J. Fatigue, 1999, vol. 21, pp. 881–89.10.1016/S0142-1123(99)00084-5 ↗
12. T. Zhai, A. Wilkinson, and J.W. Martin: Mater. Sci. Forum, 2002, vols. 396–402, pp. 1279–84.10.4028/www.scientific.net/MSF.396-402.1279 ↗
13. D.N. Fager, M.V. Hyatt, and H.T. Diep: Scripta Metall., 1986, vol. 20, pp. 1159–64.10.1016/0036-9748(86)90195-X ↗
14. W.S. Miller, M.P. Thomas, and J. White: Scripta Metall., 1987, vol. 21, pp. 663–68.10.1016/0036-9748(87)90381-4 ↗
15. W.S. Miller, M.P. Thomas, D.J. Lloyd, and D. Creber: Proc. Aluminium-Lithium Alloys III, J. Baker, P.J. Gregson, S.J. Harris, and C.J. Peel, eds., Institute of Metals, London, 1986.
16. S.P. Lynch, B.C. Muddle, and T. Pasang: Acta Mater., 2001, vol. 49, pp. 2863–74.10.1016/S1359-6454(01)00217-8 ↗
17. M.D. Garratt, G.H. Bray, and D.A. Koss: Proc. Materials Solutions Conf., Indianapolis, IN, 2001, ASM INTERNATIONAL, Materials Park, OH, 2001, pp. 151–59.
18. J.X. Li, T. Zhai, M.D. Garratt, and G.H. Bray: Metall. Mater. Trans. A, 2005, vol. 36A, pp. 2529–39.10.1007/s11661-005-0126-z ↗
19. J.X. Li, X.P. Jiang, T. Zhai, (Department of Chemical and Materials Engineering, University of Kentucky) M.D. Garratt, and G.H. Bray (Alcoa Tech Center): unpublished results, 2006.
20. J. Wang, C. Wolverton, S. Muller, Z.-K. Liu, and L.-Q. Chen: Acta Mater., 2005, vol. 53, pp. 2759–64.10.1016/j.actamat.2005.02.035 ↗
21. N. Hansen, T. Teffers, and J.K. Kjems: Acta Metall., 1981, vol. 29, pp. 523–33.
22. M.A. Wells, D.J. Lloyd, I.V. Samarasekera, J.K. Brimacombe, and E.B. Hawbolt: Metall. Mater. Trans. B, 1998, vol. 29B, pp. 621–33.10.1007/s11663-998-0097-8 ↗
23. W.C. Liu, T. Zhai, and J.G. Morris: Scripta Mater., 2004, vol. 51, pp. 83–88.10.1016/j.scriptamat.2004.04.006 ↗
24. W.C. Liu, T. Zhai, C.-S. Man, and J.G. Morris: Scripta Mater., 2003, vol. 49, pp. 539–45.10.1016/S1359-6462(03)00350-6 ↗
25. W. Weibull: Proc. R. Swedish Inst. Eng. Res., 1939, vol. 151, pp. 1–45.
26. A. de S. Jayatilaka: Fracture of Engineering Brittle Materials, Applied Science Publishers, London, 1979.