journal article·2018-11

Effect of Process Atmosphere Dew Point and Tin Addition on Oxide Morphology and Growth for a Medium-Mn Third Generation Advanced Steel During Intercritical Annealing

Maedeh Pourmajidian, Brian Langelier, Joseph R. McDermid

Publisher page

Abstract

The combined effects of process atmosphere oxygen partial pressure, annealing time, and a 0.05 wt pct Sn addition on the selective oxidation of a model 0.1C-6Mn-2Si third generation advanced high-strength steel (3G-AHSS) composition were investigated. External and internal oxidation of both steels were observed after intercritical annealing at 963 K (690 °C) for holding times of 60 to 600 seconds under all process atmosphere dew points explored—i.e., 223 K, 243 K, and 278 K (− 50 °C, − 30 °C, and + 5 °C). The external MnO morphology was changed from compact and continuous film-like nodules to a fine and discrete globular morphology, with thinner external oxides, for the Sn-added steel. Cross-sectional TEM analysis revealed that the Sn addition also resulted in significant refinement of the internal oxide network. Kinetic studies showed that both the external and internal oxidation followed a parabolic rate law, where the Sn addition to the steel chemistry resulted in lower external and internal oxidation rates. 3D atom probe tomography of the external oxide/steel interface showed that Sn was segregated to the interface with enrichment levels ten times the bulk value, which was concluded to be responsible for the observed morphological changes. The resultant refined external oxide structure is expected to have significant benefits with respect to reactive wetting by the continuous galvanizing bath.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · Advanced Materials Characterization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. [1] D.W. Suh and S.J. Kim: Scripta Mater. 2017, vol. 126, pp. 63–7.10.1016/j.scriptamat.2016.07.013 ↗
2. [2] M. J. Merwin: Mater. Sci. Forum, 2007, vol. 539, pp. 4327–32.10.4028/www.scientific.net/MSF.539-543.4327 ↗
3. [3] M.J. Merwin: Iron & Steel Technol., 2008, vol. 5, pp. 66–84.
4. [4] R. L. Miller: Metall. Mater. Trans. B, 1972, vol. 3, pp. 905–12.10.1007/BF02647665 ↗
5. K.M.H. Bhadhon, J.R. McDermid, and F.E. Goodwin: The 10th International Conference on Zinc and Zinc Alloy Coated Steel Sheet (Galvatech 2015), 2015, pp. 936–43.
6. [6] J. Mahieu, S. Claessens, and B.C. De Cooman: Metall. Mater. Trans. A, 2001, vol. 32A, pp. 2905–8.10.1007/s11661-001-1042-5 ↗
7. [7] J. Maki, J. Mahieu, B.C. De Cooman, and S. Claessens: Mater. Sci. Technol., 2003, vol. 19, pp. 125–31.10.1179/026708303225009300 ↗
8. [8] J. Mahieu, B.C. De Cooman, J. Maki, and S. Claessens: Iron Steelmaker, 2002, vol. 29, pp. 29–34.10.1179/030192302225005556 ↗
9. [9] E.M. Bellhouse, and J.R. McDermid: Metall. Mater. Trans. A, 2011, vol. 42, pp. 2753–68.10.1007/s11661-011-0685-0 ↗
10. [10] E.M. Bellhouse, and J.R. McDermid: Metall. Mater. Trans. A, 2012, vol. 43A, pp. 2426–41.10.1007/s11661-011-0983-6 ↗
11. [11] E.M. Bellhouse and J.R. McDermid: Metall. Mater. Trans. A, 2010, vol. 41A, pp. 1539–53.10.1007/s11661-010-0192-8 ↗
12. [12] L. Cho, S.J. Lee, M.S. Kim, Y.H. Kim and B.C. De Cooman: Metall. Mater. Trans. A., 2013, 44A, pp. 362–71.10.1007/s11661-012-1392-1 ↗
13. [13] Y.F. Gong, H.S. Kim and B.C. De Cooman: ISIJ Int., 2009, vol. 49, pp. 557–63.10.2355/isijinternational.49.557 ↗
14. [14] Y.F. Gong, H.S. Kim and B.C. De Cooman: ISIJ Int., 2008, vol. 48, pp. 1745–51.10.2355/isijinternational.48.1745 ↗
15. [15] K.R. Jo, L. Cho, J.H. Oh, M.S. Kim, K.C. Kang and B.C. De Cooman: Metall. Mater. Trans. A, 2017, vol. 48, pp. 3635–41.10.1007/s11661-017-4154-2 ↗
16. [16] M. Blumenau, M. Norden, F. Friedel and K. Peters: Surf. Coat. Technol., 2011, vol. 206, pp. 559–67.10.1016/j.surfcoat.2011.07.088 ↗
17. [17] Y.F. Gong and B.C. De Cooman: ISIJ Int., 2011, vol. 51, pp. 630–7.10.2355/isijinternational.51.630 ↗
18. [18] A. Ruck, D. Monceau, and H.J. Grabke: Steel Res., 1996, vol. 67, pp. 240–6.10.1002/srin.199605484 ↗
19. [19] G. Lyudkovsky: IEEE Trans. Magn., 1986, vol. 22, pp.508–46.10.1109/TMAG.1986.1064606 ↗
20. [20] L.Cho, M.S. Kim, Y.H. Kim and B.C. De Cooman: Metall. Mater. Trans. A, 2014, vol. 45A, pp. 4484–98.10.1007/s11661-014-2394-y ↗
21. [21] L. Cho, E.J. Seo, G.S. Jung, D.W. Suh and B.C. De Cooman: Metall. Mater. Trans. A, 2016, vol. 47A, pp. 1705–19.10.1007/s11661-016-3331-z ↗
22. [22] J. Oh, L. Cho, M. Kim, K. Kang and B.C. De Cooman: Metall. Mater. Trans. A, 2016, vol. 47A, pp. 5474–86.10.1007/s11661-016-3735-9 ↗
23. [23] Z.T. Zhang, I.R. Sohn, F.S. Pettit, G.H. Meier and S. Sridhar: Metall. Mater. Trans. B, 2009, vol. 40B, pp. 567–84.10.1007/s11663-009-9255-x ↗
24. [24] Y.Y. Zhang, Y.Y. Zhang, F.H. Yang and Z.T. Zhang: J. Iron. Steel Res. Int., 2013, vol. 20, pp. 39–56.10.1016/S1006-706X(13)60067-9 ↗
25. [25] E.D. Hondores and M.P. Seah: Int. Met. Rev., 1977, vol. 22, pp. 262–301.
26. [26] M. Seah: J. Catal, 1979, vol. 57, pp. 450–7.10.1016/0021-9517(79)90011-3 ↗
27. [27] D. Melford: Philos. Trans. R. Soc. A, 1980, vol. 295, pp. 89–103.10.1098/rsta.1980.0078 ↗
28. [28] D.K. Matlock, J.G. Speer, E. De Moor and P.J. Gibbs: JESTECH, 2012, vol. 15, pp. 1–12.
29. [29] B.C. De Cooman, P. Gibbs, S. Lee and D.K. Matlock: Metall. Mater. Trans. A, 2015, vol. 44A, pp. 2563–72.
30. [30] S. Lee, K. Lee and B.C. De Cooman: Metall. Mater. Trans. A, 2013, vol. 46A, pp. 2356–63.
31. [31] S. Lee and B.C. De Cooman: Metall. Mater. Trans. A, 2013, vol. 45A, pp. 709–16.
32. [32] R. Khondker, A. Mertens and J.R. McDermid: Mater. Sci. Eng. A, 2007, vol. 463, pp. 157–65.10.1016/j.msea.2006.09.116 ↗
33. [33] E.M. Bellhouse and J.R. McDermid: Mater. Sci. Eng. A, 2008, vol. 491, pp. 39–46.10.1016/j.msea.2007.12.033 ↗
34. [34] R. Kavitha and J.R. McDermid: Surf. Coat. Technol., 2012, vol. 212, pp. 152–8.10.1016/j.surfcoat.2012.09.038 ↗
35. [35] R. Sagl, A. Jarosik, D. Stifter and G. Angeli: Corros. Sci., 2013, vol. 70, pp. 268–75.10.1016/j.corsci.2013.01.039 ↗
36. Morris: FREED Thermodynamic Database, v7.8.1, 2013.
37. [37] K. Thompson, D. Lawrence, D.J. Larson, J.D. Olson, T.F. Kelly and B. Gorman: Ultramicroscopy, 2007, vol. 107, pp. 131–9.10.1016/j.ultramic.2006.06.008 ↗
38. [38] B.R. Strohmeier and D.M. Hercules: J. Phys. Chem., 1984, vol. 88, pp. 4922–9.10.1021/j150665a026 ↗
39. [39] M.C. Biesinger, B.P. Payne, A.P. Grosvenor, L.W.M. Lau, A.R. Gerson and R.St.C. Smart: Appl. Surf. Sci., 2011, vol. 257, pp. 2717–30.10.1016/j.apsusc.2010.10.051 ↗
40. [40] A. Aoki: Jpn. J. Appl. Phys., 1976, vol. 15, pp. 305–11.10.1143/JJAP.15.305 ↗
41. N. Birks, G.H. Meier and F.S. Pettit: Introduction to the High-temperature Oxidation of Metals. 2nd ed., Cambridge University Press: Cambridge, 2006, p. 338.10.1017/CBO9781139163903 ↗
42. [42] J.H. Rask, B.A. Miner and P.R. Buseck: Ultramicroscopy, 1987, vol. 21, pp. 321–6.10.1016/0304-3991(87)90030-1 ↗
43. P.L. Potapov, K. Jorissen and D. Schryvers: Phys. Rev. B, 2004, vol. 70, pp. 1–10.10.1103/PhysRevB.70.045106 ↗
44. [44] H.K. Schmid and W. Mader: Micron, 2006, vol. 37, pp. 426–32.10.1016/j.micron.2005.12.004 ↗
45. [45] H. Tan, J. Verbeeck, A. Abakumov and G. Van Tendeloo: Ultramicroscopy, 2012, vol. 116, pp. 24–33.10.1016/j.ultramic.2012.03.002 ↗
46. [46] A.P. Grosvenor, E.M. Bellhouse, A. Korinek, M. Bugnet and J.R. McDermid: Appl. Surf. Sci., 2016, vol. 379, pp. 242–8.10.1016/j.apsusc.2016.03.235 ↗
47. [47] K. Kimoto, T. Sekiguchi and T. Aoyama: J. Electron. Microsc., 1997, vol. 46, pp. 369–74.10.1093/oxfordjournals.jmicro.a023532 ↗
48. Gatan, http://www.eels.info/atlas/silicon. Accessed 12 June 2017.
49. [49] E.A. Marquis, B.P. Geiser, T.J. Prosa and D.J. Larson: J. Microsc., 2011, vol. 24, pp. 225–33.10.1111/j.1365-2818.2010.03421.x ↗
50. [50] X.S. Li, S.I. Baek, C.S. Oh, S.J. Kim and Y.W. Kim: Scripta Mater., 2007, vol. 57, pp. 113–16.10.1016/j.scriptamat.2007.03.040 ↗
51. [51] Y. Suzuki, T. Yamashita, Y. Sugimoto, S. Fujita and S. Yamaguchi: ISIJ Int., 2009, vol. 49, pp. 564–73.10.2355/isijinternational.49.564 ↗
52. [52] D. Huin, P. Flauder and J.B. Leblond: Oxid. Met., 2005, vol. 64, pp. 131–67.10.1007/s11085-005-5718-x ↗
53. [53] J. Takada, K. Kashiwagi and M. Adachi: J. Mater. Sci., 1984, vol. 19, pp. 3451–3458.10.1007/BF00549838 ↗
54. [54] H. Liu, W. Shi, Y. He and L. Li: Surf. Interface Anal., 2010, vol. 42, pp. 1685–9.10.1002/sia.3368 ↗
55. [55] M. Auinger, V.G. Praig, B. Linder and H. Danninger: Corros. Sci., 2015, vol. 96, pp. 133–43.10.1016/j.corsci.2015.04.009 ↗
56. [56] M. Pourmajidian and J.R. McDermid: Mat. Met. Trans. A, 2018, vol. 49A, pp. 1795–1808.10.1007/s11661-018-4513-7 ↗
57. [57] M. Pourmajidian and J.R. McDermid: ISIJ Int., 2018, https://doi.org/10.2355/isijinternational.isijint-2017-688.10.2355/isijinternational.ISIJINT-2017-688 ↗
58. [58] C. Wagner: Zh. Elektrochem, 1959, vol. 63, pp. 772–82.
59. [59] S. Alibeigi, R. Kavitha, R.J. Meguerian and J.R. McDermid: Acta. Mater., 2011, vol. 59, pp. 3537–49.10.1016/j.actamat.2011.02.027 ↗
60. [60] R. Sagl, A. Jarosik, G. Angeli, T. Haunschmid, G. Hesser and D. Stifter: Acta Mater., 2014, vol. 72, pp. 192–9.10.1016/j.actamat.2014.03.037 ↗