journal article·2021-05Open access

Microstructure, Hardness, and Residual Stress of the Dissimilar Metal Weldments of SA508-309L/308L-304L

Weicheng Zhong, Jun-Li Lin, Yan Chen, Zhen Li, Ke An, Benjamin J. Sutton, Brent J. Heuser

Abstract

A dissimilar metal weldment consisting of SA508-309L-308L-304L is widely used in light-water nuclear reactors. These weldments demonstrate dissimilar susceptibility to stress corrosion cracking that are related to the microstructure, properties, and residual stress. In this work, microstructures, hardness, and the residual stress distribution of the dissimilar metal weldments were investigated, with the correlation of increased hardness in the heat-affected zone (HAZ) to the microstructure. 304L HAZ demonstrated similar grain morphology as the base material, and the increase in hardness was primarily attributed to the increased dislocation density. SA508 HAZ demonstrated a change of grain morphology resulting from the different peak temperatures and cooling rates. The increased hardness in the SA508 HAZ was attributed to the refined grain morphology, higher dislocation density, and higher number density of precipitates. A ~ 20–30-μm-wide martensitic zone formed at the fusion boundary of SA508-309L, where Cr-rich carbide precipitates were observed, with the average size and the number density of 44.1 ± 16.9 nm and 1.5 × 1021 m−3, respectively. Residual stress results demonstrated the largest tensile stress at 309L butter, indicating its high cracking susceptibility.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Non-Destructive Testing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. J. C. Lippold and D. J. Kotecki, Welding metallurgy and weldability of stainless steels, Wiley, New York 2005.
2. G. Mirshekari, E. Tavakoli, M. Atapour and B. Sadeghian, Materials & Design, vol. 55, pp. 905-911, 2014.10.1016/j.matdes.2013.10.064 ↗
3. L. Dong, C. Ma, Q. Peng, E.-H. Han and W. Ke, “Microstructure and stress corrosion cracking of a SA508-309L/308L-316L dissimilar metal weld joint in primary pressurized water reactor environment,” Journal of Materials Science and Technology, vol. 40, pp. 1–14, 2020.10.1016/j.jmst.2019.08.035 ↗
4. G. Li and J. Congleton, “Stress corrosion cracking of a low alloy steel to stainless steel transition weld in PWR primary waters at 292 C,” Corrosion Science, vol. 42, pp. 1005-1021, 2000.10.1016/S0010-938X(99)00131-6 ↗
5. J. Hou, Q. Peng, Y. Takeda, J. Kuniya and T. Shoji, “Microstructure and stress corrosion cracking of the fusion boundary region in an alloy 182-A533B low alloy steel dissimilar weld joint,” Corrosion Science, vol. 52, pp. 3949-3954, 2010.10.1016/j.corsci.2010.08.002 ↗
6. Z. Chen, Y. Lu, X. Ding and T. Shoji, “Microstructural and hardness investigations on a dissimilar metal weld between low alloy steel and Alloy 82 weld metal,” Materials Characterization, vol. 121, pp. 166-174, 2016.10.1016/j.matchar.2016.09.033 ↗
7. H. Ming, Z. Zhang, J. Wang, E.-H. Han and W. Ke, “Microstructural characterization of an SA508–309L/308L–316L domestic dissimilar metal welded safe-end joint,” Materials Characterization, vol. 97, pp. 101-115, 2014.10.1016/j.matchar.2014.08.023 ↗
8. T. Sarikka, M. Ahonen, R. Mouginot, P. Nevasmaa, P. Karjalainen-Roikonen, U. Ehrnsten and H. Hanninen, “Effect of mechanical mismatch on fracture mechanical behavior of SA 508–Alloy 52 narrow gap dissimilar metal weld,” International Journal of Pressure Vessels and Piping, vol. 157, pp. 30-42, 2017.10.1016/j.ijpvp.2017.08.003 ↗
9. W. Wang, Y. Lu, X. Ding and T. Shoji, “Microstructures and microhardness at fusion boundary of 316 stainless steel/Inconel 182 dissimilar,” Materials Characterization, vol. 107, pp. 255-261, 2015.10.1016/j.matchar.2015.07.018 ↗
10. J. Francis, W. Mazur and H. Bhadeshia, “Review type IV cracking in ferritic power plant steels,” Materials Science and Technology, vol. 22, pp. 1387-1395, 2006.10.1179/174328406X148778 ↗
11. [11] W.-C. Chung, J.-Y. Huang, L.-W. Tsay and C. Chen, “Microstructure and stress corrosion cracking behavior of the weld metal in alloy 52-A508 dissimilar welds,” Materials transactions, vol. 52, pp. 12-19, 2011.10.2320/matertrans.M2010294 ↗
12. J. Hou, Q. Peng, Y. Takeda, J. Kuniya, T. Shoji, J. Wang, E.-H. Han and W. Ke, “Microstructure and mechanical property of the fusion boundary region in an Alloy 182-low alloy steel dissimilar weld joint,” Journal of Materials Science, vol. 45, pp. 5332-5338, 2010.10.1007/s10853-010-4581-6 ↗
13. K. Mao, H. Wang, Y. Wu, V. Tomar and J. P. Wharry, “Microstructure-property relationship for AISI 304/308L stainless steel laser weldment,” Materials Science and Engineering: A, vol. 721, pp. 234-243, 2018.10.1016/j.msea.2018.02.092 ↗
14. Y. Feng, Z. Luo, Z. Liu, Y. Li, Y. Luo and Y. Huang, “Keyhole gas tungsten arc welding of AISI 316L stainless steel,” Materials & Design, vol. 85, pp. 24–31, 2015.10.1016/j.matdes.2015.07.011 ↗
15. S. Sabooni, F. Karimzadeh, M. Enayati, A. Ngan and H. Jabbari, “Gas tungsten arc welding and friction stir welding of ultrafine grained AISI 304L stainless steel: microstructural and mechanical behavior characterization,” Materials Characterization, vol. 109, pp. 138-151, 2015.10.1016/j.matchar.2015.08.009 ↗
16. S. Kumar and A. Shahi, “Effect of heat input on the microstructure and mechanical properties of gas tungsten arc welded AISI 304 stainless steel joints,” Materials & Design, vol. 32, pp. 3617–3623, 2011.10.1016/j.matdes.2011.02.017 ↗
17. P. Sedek, J. Brozda, L. Wang and P. Withers, “Residual stress relief in MAG welded joints of dissimilar steels,” International journal of pressure vessels and piping, vol. 80, pp. 705-713, 2003.10.1016/j.ijpvp.2003.08.004 ↗
18. V. Satyanarayana, G. M. Reddy and T. Mohandas, “Dissimilar metal friction welding of austenitic–ferritic stainless steels,” Journal of Materials Processing Technology, vol. 160, pp. 128-137, 2005.10.1016/j.jmatprotec.2004.05.017 ↗
19. A. Joseph, S. K. Rai, T. Jayakumar and N. Murugan, “Evaluation of residual stresses in dissimilar weld joints,” International Journal of Pressure Vessels and Piping, vol. 82, pp. 700-705, 2005.10.1016/j.ijpvp.2005.03.006 ↗
20. C. Shiga, H. Y. Yasuda, K. Hiraoka and H. Suzuki, “Effect of Ms temperature on residual stress in welded joints of high-strength steels,” Welding in the World, vol. 54, pp. R71-R79, 2010.10.1007/BF03263490 ↗
21. W. Woo, V. Em, C. R. Hubbard, H.-J. Lee and K. S. Park, “Residual stress determination in a dissimilar weld overlay pipe by neutron diffraction,” Materials Science and Engineering: A, vol. 528, pp. 8021-8027, 2011.10.1016/j.msea.2011.07.059 ↗
22. D. Kotecki and T. Siewert, “WRC-1992 constitution diagram for stainless steel weld metals: a modification of the WRC-1988 diagram,” Welding Journal, vol. 71, pp. 171-178, 1992.
23. K. An, H. D. Skorpenske, A. D. Stoica, D. Ma, X.-L. Wang and E. Cakmak, “First in situ lattice strains measurements under load at VULCAN,” Metallurgical and Materials Transactions A, vol. 42, pp. 95-99, 2011.10.1007/s11661-010-0495-9 ↗
24. J.-A.J. Wang, E.A. Payzant, J.R. Bunn, and K. An: Neutron Residual Stress Mapping for Spent Nuclear Fuel Storage Canister Weldment, Oak Ridge National Lab.(ORNL) No. ORNL/TM-2018/827, Oak Ridge, TN, 2018.10.2172/1435212 ↗
25. M.T. Hutchings, P.J. Withers, T.M. Holden, and T. Lorentzen: Introduction to the characterization of residual stress by neutron diffraction, CRC Press, 2005.10.1201/9780203402818 ↗
26. A. Mark, J. Francis, H. Dai, M. Turski, P. Hurrell, S. Bate, J. Kornmeier and P. Withers, “On the evolution of local material properties and residual stress in a three-pass SA508 steel weld,” Acta materialia, vol. 60, pp. 3268-3279, 2012.10.1016/j.actamat.2012.03.022 ↗
27. R. Moat, H. Stone, A. Shirzadi, J. Francis, S. Kundu, A. Mark, H. Bhadeshia, L. Karlsson and P. Withers, “Design of weld fillers for mitigation of residual stresses in ferritic and austenitic steel welds,” Science and Technology of Welding and Joining, vol. 16, pp. 279-284, 2011.10.1179/1362171811Y.0000000003 ↗
28. G. Palumbo, K. Aust, E. Lehockey, U. Erb and P. Lin, “On a more restrictive geometric criterion for special CSL grain boundaries,” Scripta materialia, vol. 38, pp. 1685–1690, 1998.10.1016/S1359-6462(98)00077-3 ↗
29. K. Fujiyama, K. Mori, D. Kaneko, H. Kimachi, T. Saito, R. Ishii and T. Hino, “Creep damage assessment of 10Cr-1Mo-1W-VNbN steel forging through EBSD observation,” International Journal of Pressure Vessels and Piping, vol. 86, pp. 570-577, 2009.10.1016/j.ijpvp.2009.04.011 ↗
30. A. Putz, M. Althuber, A. Zelic, E. Westin, T. Willidal and N. Enzinger, “Methods for the measurement of ferrite content in multipass duplex stainless steel welds,” Welding in the World, vol. 63, pp. 1075-1086, 2019.10.1007/s40194-019-00721-4 ↗
31. F.W. Brust and P.M. Scott: ASME Pressure Vessels and Piping Conference, 2007.
32. C. Jang, P.-Y. Cho, M. Kim, S.-J. Oh and J.-S. Yang, “Effects of microstructure and residual stress on fatigue crack growth of stainless steel narrow gap welds,” Materials & Design, vol. 31, pp. 1862–1870, 2010.10.1016/j.matdes.2009.10.062 ↗
33. Q. Wang, M. Zhang, W. Liu, X. Wei, J. Xu, J. Chen, H. Lu and C. Yu, “Study of type-II boundary behavior during SA508-3/EQ309L overlay weld interfacial failure process,” Journal of Materials Processing Technology, vol. 247, pp. 64-72, 2017.10.1016/j.jmatprotec.2017.04.009 ↗
34. L. Tan, L. Rakotojaona, T. R. Allen, R. K. Nanstad and J. T. Busby, “Microstructure optimization of austenitic Alloy 800H (Fe–21Cr–32Ni),” Materials science and engineering: A, vol. 528, no. 6, pp. 2755-2761, 2011.10.1016/j.msea.2010.12.052 ↗
35. L. Tan, K. Sridharan, T. R. Allen, R. K. Nanstad and D. A. McClintock, “Microstructure tailoring for property improvements by grain boundary engineering,” Journal of Nuclear Materials, vol. 374, no. 1-2, pp. 270-280, 2008.10.1016/j.jnucmat.2007.08.015 ↗
36. T. Liu, Q. Bai, X. Ru, S. Xia, X. Zhong, Y. Lu and T. Shoji, “Grain boundary engineering for improving stress corrosion cracking of 304 stainless steel,” Materials Science and Technology, vol. 35, pp. 477-487, 2019.10.1080/02670836.2019.1570661 ↗
37. J. W. Kim, K. Lee, J. S. Kim and T. S. Byun, “Local mechanical properties of Alloy 82/182 dissimilar weld joint between SA508 Gr. 1a and F316 SS at RT and 320 C,” Journal of Nuclear Materials, vol. 384, pp. 212-221, 2009.10.1016/j.jnucmat.2008.11.019 ↗
38. Y. Wang, R. Kannan and L. Li, “Characterization of as-welded microstructure of heat-affected zone in modified 9Cr–1Mo–V–Nb steel weldment,” Materials Characterization, vol. 118, pp. 225-234, 2016.10.1016/j.matchar.2016.05.024 ↗
39. W. Guo, S. Dong, J. A. Francis and L. Li, “Microstructure and mechanical characteristics of a laser welded joint in SA508 nuclear pressure vessel steel,” Materials Science and Engineering: A, vol. 625, pp. 65-80, 2015.10.1016/j.msea.2014.11.056 ↗
40. B. Lee, M. Kim, J. Yoon and J. Hong, “Characterization of high strength and high toughness Ni–Mo–Cr low alloy steels for nuclear application,” International journal of Pressure Vessels and piping, vol. 87, pp. 74-80, 2010.10.1016/j.ijpvp.2009.11.001 ↗
41. S. Lee, S. Kim, B. Hwang, B. Lee and C. Lee, “Effect of carbide distribution on the fracture toughness in the transition temperature region of an SA 508 steel,” Acta materialia, vol. 50, pp. 4755–4762, 2002.10.1016/S1359-6454(02)00313-0 ↗
42. S. Kim, S. Y. Kang, S. Lee, S. J. Oh, S.-J. Kwon, O. H. Kim and J. H. Hong, “Correlation of the microstructure and fracture toughness of the heat-affected zones of an SA 508 steel,” Metallurgical and Materials Transactions A, vol. 31, pp. 1107-1119, 2000.10.1007/s11661-000-0106-2 ↗
43. M. Calcagnotto, D. Ponge, E. Demir and D. Raabe, “Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD,” Materials Science and Engineering: A, vol. 527, pp. 2738-2746, 2010.10.1016/j.msea.2010.01.004 ↗