In the present study, effects of notch shape and specimen thickness on drop-weight tear test (DWTT) properties of API X70 and X80 line-pipe steels fabricated by varying hot-rolling conditions were investigated. The DWTT was conducted on the rolled steels, and the results were discussed in comparison with the Charpy V-notch (CVN) impact test and crack-tip opening angle (CTOA) test data. The DWTT results indicated that the steels rolled in the single-phase region had the higher upper shelf energy (USE) than the steel rolled in the two-phase region, because their microstructures were composed of acicular ferrite (AF). The DWTT energy transition temperature (ETT) of the steel rolled in the two-phase region was the lowest, because it had a finer effective grain size and the lowest volume fraction of hard secondary phases. Chevron notch (CN) DWTT energy density did not increase much with increasing specimen thickness, whereas pressed notch (PN) DWTT energy density increased by 1 to 3 J/mm2, because the total energy of the CN DWTT increased less than that of the PN DWTT due to the larger stress concentration at the CN. The ETT increased with increasing specimen thickness due to the increase in constraint state, and the ETT of the CN DWTT was slightly lower than that of PN DWTT. The measured CTOA showed better correlation with the DWTT propagation energy than with the CVN or DWTT total energy because it was related to the crack propagation speed. The value of sin (2CTOA) reliably showed a linearly proportional relation with the DWTT propagation energy density.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Forming Simulation Techniques · Fatigue and fracture mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. G.M. McClure, A.R. Duffy, and R.J. Eiber: J. Eng. Industry, 1965, Aug., pp. 265–7810.1115/1.3670809 ↗
2. R.J. Eiber, A.R. Duffy, G.M. McClure: Impact Testing of Metals, ASTM, West Conshohocken, PA, 1970, pp. 181–9110.1520/STP32062S ↗
3. API Recommended Practice 5L3, American Petroleum Institute, Washington DC, 1996
4. R. Denys: Pipeline Technology, vol. I, Elsevier, Amsterdam, 2000, pp. 1–116
5. D.P. Fairchild, M.L. Macia, S.D. Papka, C.W. Petersen, J.H. Stevens, S.T. Barbas, N.V. Bangaru, J.Y. Koo, M.J. Luton: Proc. Int. Pipe Dreamer’s Conf., Scientific Surveys Ltd., Yokohama, Japan, 2002, pp. 307–21
6. K.T. Corbett, R.R. Bowen, C.W. Petersen: Int. J. Offshore Polar Eng., 2004, 14:75–80
7. G. Mannucci and D. Harris: Fracture Properties of API X100 Gas Pipeline Steels, Final Report, European Commission, 2002, pp. 1–128
8. D.J. Horsley: Eng. Fract. Mech., 2003, 70:547–5210.1016/S0013-7944(02)00136-4 ↗
9. G.M. Wilkowski, W.A. Maxey, R.J. Eiber: Can. Metall. Q. 1980, 19:59–7710.1179/cmq.1980.19.1.59 ↗
10. N. Nozaki, K. Bessyo, Y. Sumitomo, I. Takeuchi, A. Yamashita: Sumitomo Search, 1981, 26:76–90
11. S.-T. Oh, H.-J. Chang, K.H. Oh, H.N. Han: Met. Mater. Int., 2006, 12:121–2910.1007/BF03027467 ↗
12. B. Hwang, S. Lee, Y.M. Kim, N.J. Kim, J.Y. Yoo, C.S. Woo: Mater. Sci. Eng. A, 2004, A368:18–2710.1016/j.msea.2003.09.075 ↗
13. B. Hwang, Y.G. Kim, S. Lee, N.J. Kim, J.Y. Yoo: Metall. Mater. Trans. A, 2005, 36A:371–8710.1007/s11661-005-0309-7 ↗
14. I. Tamura, H. Sekine, T. Tanaka, and C. Ouchi: Thermomechanical Processing of High-Strength Low-Alloy Steels, Butterworth & Co., Ltd., 1988, pp. 1–15310.1016/B978-0-408-11034-1.50004-0 ↗
15. J.W. Kim, J.W. Choi, D.B. Bae: Metall. Mater. Int., 2005, 11:131–3410.1007/BF03027456 ↗
16. I.D. Choi, D.M. Kim, S.J. Kim, D.M. Bruce, D.K. Matlock, J.G. Speer: Metall. Mater. Int., 2006, 12:13–1910.1007/BF03027517 ↗
17. ASTM Standard E23-02, Standard Test Methods for Notched Bar Impact Testing of Metallic Materials, ASTM, West Conshohocken, PA, 2002, pp. 1–26
18. W. Oldfield: Curve fitting impact test data-a statistical procedure, ASTM Standardizations News, 1975, pp. 24–29
19. ASTM Standard E346-03, Standard Test Methods for Drop-Weight Tear Tests of Ferritic Steels, ASTM, West Conshohocken, PA, 2003, pp. 1–6
20. P.E. O’Donoghue, M.F. Kanninen, C.P. Leung, G. Demofonti, S. Venzi: Int. J. Pres. Ves. Piping, 1997, 70:11–2510.1016/S0308-0161(96)00012-9 ↗
21. J.C. Newman Jr., M.A. James, U. Zerbst: Eng. Fract. Mech., 2003, 70:371–8510.1016/S0013-7944(02)00125-X ↗
22. G. Demofonti, G. Buzzichelli, S. Venzi, M. Kanninen: 1995 R. Deney, (ed.), Pipeline Technology, vol. II. Elsevier, New York, NY
23. L.N. Pussegoda, S. Verbit, A. Dinovitzer, W. Tyson, A. Glover, L. Collins, and L. Carlson: Proc. 2000 Int. Pipeline Conf., ASME, New York, NY, 2000, vol. 1, pp. 247–54
24. L.N. Pussegoda: Comparison of Propagation Energy from Back-slotted Specimens with CTOA, Final Report (4916-4C), Fleet Technology Ltd., Kanata, ON, 2001
25. D.L. Rudland, Y.-Y. Wang, G. Wilkowski, D.J. Horsley: Eng. Fract. Mech. 2004, 71:2533–4910.1016/j.engfracmech.2003.12.007 ↗
26. N. Pussegoda, L. Malik, A. Dinovitzer, B.A. Graville, and A.B. Rothwell: Proc. 2000 Int. Pipeline Conf., J.R. Ellwood, ed., ASME, New York, NY, 2000, vol. 1, pp. 239–46
27. D.L. Rudland, G. Wilkowski, Y.-Y. Wang, D. Horsley, B. Rothwell, and A. Glover: Proc. 2002 Int. Pipeline Conf., Calgary, AB, Canada, Sept. 2002
28. L.N. Pussegoda, A. Fredj, A. Fonzo, G. Demofonti, G. Mannucci, and B. Rothwell: Proc. 2006 Int. Pipeline Conf., Calgary, AB, Canada, Sept. 2006
29. N.J. Kim: J. Met., 1983, 35:21–27
30. J.Y. Koo, M.J. Luton, N.V. Bangaru, R.A. Petkovic, D.P. Fairchild, C.W. Petersen, H. Asahi, T. Hara, Y. Terada, M. Sugiyama, H. Tamehiro, Y. Komizo, S. Okaguchi, M. Hamada, A. Yamamoto, and I. Takeuchi: Proc. 13th Int. Offshore and Polar Engineering Conf., Honolulu, HI, 2003, pp. 10–18
31. Y. Shiota, Y. Tomota, A. Moriai, T. Kamiyama: Met. Mater. Int., 2005, 11:371–7610.1007/BF03027507 ↗
32. B. Hwang, S.Y. Shin, S. Lee, N.J. Kim, S. Kim, K.B. Kang: Metall. Mater. Trans. A, 2006, 37A:371–8010.1007/s11661-006-0007-0 ↗
33. A.H. Priest, B. Holmes: Int. J. Fract., 1981, 17:277–9910.1007/BF00034502 ↗
34. B.N. Leis: 2000, in R. Denys, (ed.), Pipeline Technology, vol. I. Elsevier, Amsterdam, pp. 343–58
35. P. Salvini, A. Fonzo, G. Mannucci: Eng. Fract. Mech. 2003, 70:553–6610.1016/S0013-7944(02)00137-6 ↗
36. G. Demofonti, G. Mannucci, M. Di Biagio, H.G. Hillenbrand, D. Harris: 2004 . R. Denys, (ed.), Pipeline Technology Conf., I. Scientific Surveys, Ltd., Ostend, Belgium, 467–81
37. A.B. Rothwell: 2000, . R. Denys, (ed.), Pipeline Technology, vol. I. Elsevier, Amsterdam, pp. 387–405
38. G. Wilkowski, Y.-Y. Wang, D. Rudland: 2000, . R. Denys, (ed.), Pipeline Technology I. Elsevier, Amsterdam, 359–86
39. M. Ogasawara: Nippon Steel Techn. Rep., 1983, Jun., No. 21, pp. 339–45
40. S.Y. Shin, B. Hwang, S. Lee, N.J. Kim, S.S. Ahn: J. Kor. Inst. Met. Mater., 2006, 44:1–9
41. B. Hwang, Y.G. Kim, S. Lee, N.J. Kim, J.Y. Yoo: Metall. Mater. Trans. A, 2005, 36A:2107–1410.1007/s11661-005-0331-9 ↗