Role of Nonmetallic Inclusions in Hydrogen Embrittlement of High-Strength Carbon Steels with Different Microalloying
Source abstract
Abstract
High-strength carbon steels of 1200 MPa strength level with different microalloying were tensile tested at constant extension rate and constant load under continuous electrochemical hydrogen charging. The results show that hydrogen markedly reduces elongation and time to fracture of all the studied steels. Fractography of the steels shows that nonmetallic inclusions (NMIs) play the major role in crack initiation in hydrogen-charged specimens. The role of NMIs in the hydrogen-induced fracture of steels is discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. R.P. Gangloff: Compr. Struct. Integr., 2003, vol. 6, p. 31.10.1016/B0-08-043749-4/06134-6 ↗
2. J.P. Hirth: Metall. Trans. A, 1980, vol. 11A, pp. 861–90.10.1007/BF02654700 ↗
3. G.R. Caskey, Jr.: Hydrogen Degradation of Ferrous Alloys, Noyes Publications, Park Ridge, 1985, p. 822.
4. T. Doshida, H. Suzuki, K. Takai, N. Oshima, and T. Hirade: ISIJ Int., 2012, vol. 52, pp. 198–207.10.2355/isijinternational.52.198 ↗
5. M. Nagumo, K. Takai, and N. Okuda: J. Alloys Compd., 1999, vols. 293–295, pp. 310–16.10.1016/S0925-8388(99)00322-9 ↗
6. M. Nagumo, T. Tamaoki, and T. Sugawara: Hydrogen Effects on Material Behaviour and Corrosion Deformation Interactions, TMS, Warrendale, PA, 2003, p. 999.
7. M. Nagumo: Mater. Sci. Technol., 2004, vol. 20, pp. 940–50.10.1179/026708304225019687 ↗
8. S. Fujita and Y. Murakami: Metall. Mater. Trans. A, 2012, vol. 44A, pp. 303–21.
9. Y. Yagodzinskyy, O. Todoshchenko, S. Papula, and H. Hänninen: Steel Res. Int., 2010, vol. 82, pp. 20–25.10.1002/srin.201000227 ↗