Time-Resolved X-Ray Microtomography Observation of Intermetallic Formation Between Solid Fe and Liquid Al

Guillaume Pasche, Mario Scheel, Robin Schäublin, Cécile Hébert, Michel Rappaz, Aïcha Hessler-Wyser

Abstract

Time-resolved in situ X-ray tomography combined with scanning electron microscopy was performed on an Al-Fe diffusion system at 973 K (700 °C) to study the formation of the main intermetallic compounds occurring at the interface. After nucleation on the liquid side of the interface, growth occurs in both liquid and solid directions. In the direction of the solid, growth starts with a particular tongue-like feature which then progressively thickens. The thickening is linked to the deformation of the iron matrix during the formation of the intermetallic compound. Growth in the direction of the liquid is slowed down by erosion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Solidification and crystal growth phenomena · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. K. Bouché, F. Barbier, A. Coulet (1998). Mater. Sci. Eng. A 249:167–75.10.1016/S0921-5093(98)00573-5 ↗
2. Bouayad A., Gerometta Ch., Belkebir A., Ambari A. (2003). Mater. Sci. Eng. A 363:53–61.10.1016/S0921-5093(03)00469-6 ↗
3. Eggeler G., Auer W., Kaesche H. (1986). J. Mater. Sci. 21:3348–50.10.1007/BF00553379 ↗
4. Eggeler G., Theuerkauf Th., Auer W. (1985) Z. Werkstofftech. 16:359–65.10.1002/mawe.19850161008 ↗
5. Cheng W.-J., Wang C.-J. (2009). Surf. Coat. Technol. 204:824–28.10.1016/j.surfcoat.2009.09.061 ↗
6. Kwon S.C., Lee J.Y. (1981). Can. Metall. Q. 20:351–57.10.1179/000844381795270156 ↗
7. Yeremenko V.N., Natanzon Ya.V., Dybkov V.I. (1981). J. Mater. Sci. 16:1748–56.10.1007/BF00540620 ↗
8. Tanaka Y., Kajihara M. (2009). Mater. Trans. 50:2212–20.10.2320/matertrans.M2009128 ↗
9. W. Kajoch and A. Fajkiel: International Die Casting Congress and Exposition, Detroit, 16th trans. T91-034, 1991, pp. 67–74.
10. Phillion A.B. (2012). JOM. 64:66–67.10.1007/s11837-011-0215-y ↗
11. Grujic K., Hegna T., Laundal K.M. (2012) JOM 64:96–101.10.1007/s11837-011-0233-9 ↗
12. Pereiro-Lopez E., Ludwig W., Bellet D., Baruchel J. (2003). Def. Diff. Forum 216-217:241–48.10.4028/www.scientific.net/DDF.216-217.241 ↗
13. Ludwig W., Pereiro-Lopez E., Bellet D. (2005). Acta Mater. 53(1):151–62.10.1016/j.actamat.2004.09.012 ↗
14. Ludwig O., Dimichiel M., Salvo L., Suéry M., Falus P. (2005). Metall. Mater. Trans. A 36A:1515–23.10.1007/s11661-005-0243-8 ↗
15. M. Di Michiel, J.M. Merino, D. Fernandez-Carreiras, T. Buslaps, V. Honkimäki, P. Falus, T. Martins, and O. Svensson: Sci. Instrum., 2005, vol. 76, p. 043702.10.1063/1.1884194 ↗
16. Abramoff M.D., Magalhaes P.J., Ram S.J. (2004). Biophoton. Int. 11:36–41.
17. D.A. Porter and K.E. Easterling: Phase Transformations in Metals and Alloys, 2nd ed., CRC Press, Boca Raton, FL, 1992.10.1007/978-1-4899-3051-4 ↗