journal article·2020-02Open access

The Effect of Interface Morphology on the Electro-Mechanical Properties of Ti/Cu Clad Composites Produced by Explosive Welding

Henryk Paul, Wojciech Skuza, Robert Chulist, Magdalena Miszczyk, Aleksander Gałka, Mariusz Prażmowski, Janusz Pstruś

Abstract

Abstract The effect of interfacial microstructure on the electro-mechanical properties of explosively welded titanium and copper plates is discussed. Mechanical testing proved that using detonation velocities ranging from 2000 to 3000 m s−1and stand-off distances from 1.5 to 9.0 mm, joints that satisfy the strength criteria for a good quality clad were produced. Scanning electron microscopy images show that all interfaces exhibit a wave character. It was noticed that as the stand-off distances and detonation velocities increase, the amplitude and period of the waves, as well as the quantity of the melt zones, increase as well. Also, as the interface waviness and volume fraction of the melt zones increase, the resistivity increases substantially. The experimental data demonstrate that the bonding between both metals is always achieved by surface melting of several tenths of a nanometer, which can be detected only by transmission electron microscopy. Most of the phases that form within the melt zones do not appear in the equilibrium phase diagram and show an amorphous/nano-grained structure. Only a very small amount of equilibrium phases such as CuTi3, Cu3Ti, Cu4Ti3was revealed employing synchrotron X-ray diffraction.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Microstructure and mechanical properties · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. M. Yang, H. Ma, Z. Shen, Y. Sun, Fusion Eng. Des., 2019, vol. 143, pp. 106-114.10.1016/j.fusengdes.2019.03.137 ↗
2. M-X. Xie, X-T. Shang, L-J. Zhang, Q-L. Bai, T-T. Xu, Metals, 2018, vol. 8(3), pp. 159-173.10.3390/met8030159 ↗
3. K. Topolski, Z. Szulc, H. Garbacz, J. Mater. Eng. Perform., 2016, vol. 25, pp. 3231-3237.10.1007/s11665-016-2080-x ↗
4. F. Findik, Mater. Des., 2011, vol. 32, pp. 1081–1093.10.1016/j.matdes.2010.10.017 ↗
5. P. Corigliano, V. Crupi, E. Guglielmino, A. M. Sili, Mar. Struct., 2018, vol. 57, pp. 207-218.10.1016/j.marstruc.2017.10.004 ↗
6. P. Corigliano, V. Crupi, E. Guglielmino, Ocean Eng., 2018, vol. 160(15), pp. 346-353.10.1016/j.oceaneng.2018.04.070 ↗
7. Y. Kaya, Metals, 2018, vol. 8(7), pp. 544-559.10.3390/met8070544 ↗
8. S.M. Aceves, F. Espinosa-Loza, J.W. Elmer, R. Huber, Int. J. Hydrogen Energy, 2015, vol. 40(3), pp. 1490-1503.10.1016/j.ijhydene.2014.11.038 ↗
9. A. Sanjurjo, B.J. Wood, K.H. Lau, G.T. Tong, D.K. Choi, M.C.H. McKubre, H.K. Song, N. Church, Surf. Cat. Technol., 1991, vol. 49, pp. 110-115.10.1016/0257-8972(91)90040-4 ↗
10. L.Y. Demidenko, N.A. Onatskaya, Surf. Eng. Appl. Electrochem., 2008, vol. 44(3), pp. 245-247.10.3103/S1068375508030149 ↗
11. K. Aydin, Y. Kaya, N. Kahraman, Mater. Des., 2012, vol. 37, pp. 356-368.10.1016/j.matdes.2012.01.026 ↗
12. J. Hemanth, Open Journal of Composite Materials, 2017, vol. 7, pp. 105-116.10.4236/ojcm.2017.72007 ↗
13. Y. Zhao, W. Wang, K. Yan, C. Liu, J. Zou, J. Mater. Proc. Techn., 2018, vol. 257, pp. 244-249.10.1016/j.jmatprotec.2018.03.001 ↗
14. Guo S, Peng Y, Xu X, Diao C, Kong J, Luo T-Y, Wang K-H, Zhu Y (2017) Mater. Des. 124:51-50.10.1016/j.matdes.2017.02.054 ↗
15. S.D. Meshram, T. Mohandas, G.M. Reddy, J. Mater. Proc. Technol., 2007, vol. 184(1), pp. 330-337.10.1016/j.jmatprotec.2006.11.123 ↗
16. R. Kumar, M. Balasubramanian, Def. Technol., 2015, vol. 11(1), pp. 65-75.10.1016/j.dt.2014.10.001 ↗
17. J.S. Lee, H. Son, I.H. Oh, C.S. Khan, C.H. Yun, S.C. Lim, H.C. Kwon, J. Mater. Proc. Technol., 2007, vol. 187-188, pp. 653-656.10.1016/j.jmatprotec.2006.11.144 ↗
18. Hosseini M, DaneshManesh H (2015) Mater. Des. 81:122-132.10.1016/j.matdes.2015.05.010 ↗
19. N. Kahraman, B. Gülenç, J. Mater. Proc. Techn., 2005, vol. 169, pp. 67-71.10.1016/j.jmatprotec.2005.02.264 ↗
20. T.Z. Blazynski (ed.): Explosive Welding, Forming and Compaction, Applied Science Publishers LTD, New York 1983.
21. V.I. Lysak, S.V. Kuzmin, Explosive welding of metal layered composite materials. In: Paton BE, editor. Ukraine. Kiev: E.O. Paton Electric Welding Institute, 2003.
22. I.A. Bataev, D.V. Lazurenko, S. Tanaka, K. Hokamoto, A.A. Bataev, Y. Guo, A.M. Jorge Jr., Acta Mater., 2017, vol. 135, pp. 277-289.10.1016/j.actamat.2017.06.038 ↗
23. H. Paul, L. Lityńska-Dobrzyńska, M. Prażmowski, Metall. Mater. Trans. A, 2013, vol. 44A, pp. 3836-3851.10.1007/s11661-013-1703-1 ↗
24. H. Paul, J. Morgiel, M. Faryna, M. Prażmowski, M. Miszczyk, Int. J. Mater. Res., 2015, vol. 106(7), pp. 782-792.10.3139/146.111230 ↗
25. H. Paul, M.M. Miszczyk, R. Chulist, M. Prażmowski, J. Morgiel, A. Gałka, M. Faryna, F. Brisset, Mater. Des., 2018, vol. 153, pp. 177-189.10.1016/j.matdes.2018.05.014 ↗
26. J. Song, A. Kostka, M. Veehmayer, D. Raabe, Mater. Sci. Eng. A, 2011, vol. 528, pp. 2641–2647.10.1016/j.msea.2010.11.092 ↗
27. Lazurenko DV, Bataev IA, Mali VI, Bataev AA, Milutina IN, Lozhlin VS, Esikov MA, Jorge AMJ (2016) Mater. Des. 102:122-130.10.1016/j.matdes.2016.04.037 ↗
28. S.R. Carpenter: in Shock Waves and High-strain-rate Phenomena in Metals, M.A. Meyers and L.E. Murr, eds., Plenum Press, New York, 1981, pp. 941–45.10.1007/978-1-4613-3219-0_53 ↗
29. H. Paul, M. Faryna, M. Prażmowski, R. Banski, Arch. Metall. Mater., 2011, vol. 56, pp. 463-474.
30. R. Mendes, B. Ribeiro, A. Loureiro, Mater. Des., 2013, vol. 51, pp. 182-192.10.1016/j.matdes.2013.03.069 ↗
31. S.K. Godunov, A.A. Deribas, N.S. Kozin, J. Appl. Mech. Tech. Phys., 1971, vol. 2(3), pp. 398-406.10.1007/BF00851622 ↗
32. S.R. Reid, N.H.S. Sherif, J. Mech. Eng. Sci., 1976, vol. 18(2), pp. 87-94.10.1243/JMES_JOUR_1976_018_016_02 ↗
33. D. Jaramillov, O.T. Inal, A. Szecket, J. Mater. Sci., 1987, vol. 22(9), pp. 3143-3147.10.1007/BF01161175 ↗
34. S.A.L. Salem, S.T.S. Al-Hassani: in Shock waves and high strain rate phenomena in metals: concepts and applications. Meyers MA, Murr LE, eds., Proceedings of the International conference on metallurgical effects of high-strain-rate deformation and fabrication, Plenum Press, New York 1981, pp. 1003–18
35. P. Manikandan, K. Hokamoto, M. Fujita, K. Raghukandan, R. Tomoshige, J. Mater. Proc. Technol., 2008, vol. 195(1–3), pp. 232-240.10.1016/j.jmatprotec.2007.05.002 ↗
36. Bataev IA, Tanaka S, Zhou Q, Lazurenko DV, JorgeJunior AM, Bataev AA, Hokamoto K, Mori A, Chen P (2018) Mater. Des. 169:107649.10.1016/j.matdes.2019.107649 ↗
37. D. Fronczek, J. Wojewoda-Budka, R. Chulist, A. Sypień, A. Kornewa, Z. Szulc, N. Schell, P. Zieba, Mater. Des., 2016, vol. 91, pp. 80-89.10.1016/j.matdes.2015.11.087 ↗
38. A. Durgutlu, H. Okuyucu, B. Gulenc, Mater. Des., 2008, vol. 29, pp. 1480-1484.10.1016/j.matdes.2007.07.012 ↗
39. N. Kahraman, N. Gulenc, F. Findik, J. Mater. Proc. Technol., 2005, vol. 171, pp. 241-249.
40. AkhbariMousavi SAA, FarhadiSartanagi P (2009) Mater. Des. 30:459-468.10.1016/j.matdes.2008.06.016 ↗
41. K. Hokamoto, A. Chiba, M. Fujita, T. Izuma, Compos. Eng., 1995, vol. 5(8), pp. 1069-1079.10.1016/0961-9526(95)00059-V ↗
42. H. Paul, M. M. Miszczyk, A. Gałka, R. Chulist, Z. Szulc, Arch. Metall. Mater., 2019, vol. 64, pp. 683-694.10.24425/amm.2019.127599 ↗
43. G.G. Zu, X. Li, J. Zhang, H. Zhang, Journal of Wuhan University of Technology – Mater. Sci. Ed., 2015, vol. 30(6), pp. 1199-1203.
44. A. D. Tete, A.Y. Deshmukh, R.R. Yerpude, International Journal of Engineering and Technology, 2013, vol. 2(3), pp. 259-265.10.14419/ijet.v2i3.1023 ↗
45. M. Prażmowski, D. Rozumek, H. Paul, Eng. Fail. Anal., 2017, vol. 75, pp. 71-81.10.1016/j.engfailanal.2016.12.022 ↗
46. R. Chulist, L. Straka, A. Sozinov, T. Lippmann, W. Skrotzki, Scripta Mater., 2013, vol. 68, pp. 671-674.10.1016/j.scriptamat.2013.01.024 ↗
47. F. Moisy, A. Gueydan, X. Sauvage, A. Guillet, C. Keller, E. Guilmeau, E. Hug, Mater. Des., 2018, vol. 155, pp. 366-374.10.1016/j.matdes.2018.06.021 ↗
48. Z. Livne, A. Munitz, J. Mat. Sci., 1987, vol. 22, pp. 1495-1500.10.1007/BF01233153 ↗
49. Q. Chu, M. Zhang, J. Li, Ch. Yan, Mater. Sci. Eng. A, 2017, vol. 689, pp. 323-331.10.1016/j.msea.2017.02.075 ↗
50. B. Crossland, Explosive welding of metals and its application, Clarendon Press Oxford, 1982.
51. A. Durgutlu, B. Gulenc, F. Findik, Mater. Des., 2005, vol. 26(6), pp. 497-507.10.1016/j.matdes.2004.07.021 ↗
52. B. Wronka, J. Mater. Sci., 2010, vol. 45, pp. 4078-4083.10.1007/s10853-010-4494-4 ↗
53. Miszczyk MM, Paul H, Driver JH, Drzymała P (2017) Acta Mater. 125:109–12410.1016/j.actamat.2016.11.054 ↗
54. Hammerschmidt M, Kreye H (1981) Microstructure and bonding mechanism in explosive welding. In Murr MA, Murr LE (eds) Shock Waves and High-Strain-Rate Phenomena in Metals. Plenum Press, New York
55. K. Nakamura, S. Kikuchi, Journal of the Japan Institute of Metals and Materials, 2008, vol. 72(10), pp. 800-803.10.2320/jinstmet.72.800 ↗
56. H. Paul, Ł. Maj, M. Prażmowski, A. Gałka, M. Miszczyk, P. Petrzak, Procedia Manufacturing, 2018, vol. 15, pp. 1391-1398.
57. A.A. Eze, T. Jamiru, R. Sadiku, M.O. Durowoju, W.K. Kupaloti, I.D. Ibrachim, B.A. Abadele, P.A. Olubambi, S. Diouf, J. Alloys and Compounds, 2018, vol. 736, pp. 163-171.10.1016/j.jallcom.2017.11.129 ↗
58. J. Zhang, Y.C. Zhou, J. Mater. Res., 2008, vol. 23(4), pp. 924-932.10.1557/jmr.2008.0126 ↗
59. J. B. Liu, L. Meng and Y. W. Zeng, Mater. Sci. Engn. A, 2006, vol. 435-436, pp. 237–244.10.1016/j.msea.2006.07.125 ↗
60. M. Ueda, K. Ota, M. Ikeda, Mater. Trans., 2013, vol. 54, pp. 1650-1654.10.2320/matertrans.MH201306 ↗
61. R. Chulist, D.M. Fronczek, Z. Szulc, J. Wojewoda-Budka, Mater. Charact., 2017, vol. 129, pp. 242-246.10.1016/j.matchar.2017.05.007 ↗
62. C.L.P. Pavithra, B.V. Sarada, K.V. Rajulapati, M. Ramakrishna, R.C. Gundakaram, T.N. Rao, G. Sundararajan, Cryst. Growth Des., 2015, vol. 15, pp. 4448-4458.10.1021/acs.cgd.5b00748 ↗