journal article·2012-09

Microstructure and Hydrogen-Induced Failure Mechanisms in Fe and Ni Alloy Weldments

J. A. Fenske, I. M. Robertson, Raghavan Ayer, Martin Hukle, Dan Lillig, Brian Newbury

Publisher page

Abstract

The microstructure and fracture morphology of AISI 8630-IN625 and ASTM A182-F22-IN625 dissimilar metal weld interfaces were compared and contrasted as a function of postweld heat treatment (PWHT) duration. For both systems, the microstructure along the weld interface consisted of a coarse grain heat-affected zone in the Fe-base metal followed by discontinuous martensitic partially mixed zones and a continuous partially mixed zone on the Ni side of the fusion line. Within the partially mixed zone on the Ni side, there exists a 200-nm-wide transition zone within a 20-μm-wide planar solidification region followed by a cellular dendritic region with Nb-Mo–rich carbides decorating the dendrite boundaries. Although there were differences in the volume of the partially mixed zones, the major difference in the metal weld interfaces was the presence of M7C3 precipitates in the planar solidification region, which had formed in AISI 8630-IN625 but not in ASTM A182-F22-IN625. These precipitates make the weldment more susceptible to hydrogen embrittlement and provide a low energy fracture path between the discontinuous partially mixed zones.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. I.M. Robertson, D. Lillig, and P.J. Ferreira: in Proc. 2008 Int. Hydrogen Conf.—Effects of Hydrogen on Materials, W.Y. Jackson Hole, B. Somerday, P. Sofronis, and R. Jones, eds., ASM INTERNATIONAL, Materials Park, OH, 2009, pp. 22–37.
2. I.M. Robertson, H.K. Birnbaum, and P. Sofronis: in Dislocations in Solids, J.P. Hirth and L. Kubin, eds., Elsevier, New York, NY, 2009, vol. 19, pp. 249–93.10.1016/S1572-4859(09)01504-6 ↗
3. R.P. Gangloff: in Proc. 2008 Int. Hydrogen Conf. —Effects of Hydrogen on Materials, W.Y. Jackson Hole, B. Somerday, P. Sofronis, and R. Jones, eds., ASM INTERNATIONAL, Metals Park, OH, 2009, pp. 1–21.
4. R.P. Gangloff: Critical Issues in Hydrogen Assisted Cracking of Structural Alloys, Elsevier, New York, NY, 2008, pp. 141–65.
5. H.K. Birnbaum: J. Less-Common Met., 1984, vol. 104, pp. 31–41.10.1016/0022-5088(84)90433-8 ↗
6. B.G. Pound: Acta Mater., 1998, vol. 46, pp. 5733–43.10.1016/S1359-6454(98)00247-X ↗
7. G.M. Pressouyre: Acta Metall., 1980, vol. 28, pp. 895–911.10.1016/0001-6160(80)90106-6 ↗
8. G.M. Pressouyre and I.M. Bernstein: Metall. Trans. A, 1978, vol. 9A, pp. 1571–80.10.1007/BF02661939 ↗
9. G.M. Pressouyre and I.M. Bernstein: Metall. Trans. A, 1981, vol. 12A, pp. 835–44.10.1007/BF02648348 ↗
10. F. Wei and K. Tsuzaki: Metall. Mater. Trans. A, 2006, vol. 37A, pp. 331–53.10.1007/s11661-006-0004-3 ↗
11. J. Takahashi, K. Kawakami, Y. Kobayashi, and T. Tarui: Scripta Mater., 2010, vol. 63, pp. 261–64.10.1016/j.scriptamat.2010.03.012 ↗
12. D.F. Johnson and E.A. Carter: Acta Mater., 2009, vol. 58, pp. 638–48.10.1016/j.actamat.2009.09.042 ↗
13. A. Van der Ven and G. Ceder: Acta Mater., 2004, vol. 52, pp. 1223–35.10.1016/j.actamat.2003.11.007 ↗
14. S. Kou: Welding Metallurgy, 2nd ed., Wiley-Interscience, Hoboken, NJ, 2003.
15. H.I. Lange, S. Aldstedt, and E. Ostby: Investigation of Fractured Weld Connection on Hub No. AB-103 Asgard B, SINTEF, Trondheim, Norway, 2001.
16. V.C.M. Beaugrand, L.S. Smith, and M.F. Gittos: Corrosion 2009, Atlanta, GA, NACE International, Houston, TX, 2009, 12 p.
17. V. Olden, P.E. Kvaale, P.A. Simensen, S. Aaldstedt, and J.K. Solberg: ASME 2003 22nd Int. Conf. on Offshore Mechanics and Arctic Engineering (OMAE2003), Cancun, Mexico, ASME, New York, NY, 2003, pp. 109–15.10.1115/OMAE2003-37196 ↗
18. V.C.M. Beaugrand, L.S. Smith, and M.F. Gittos: 28th Int. Conf. on Ocean, Offshore and Arctic Engineering, OMAE2009, Honolulu, HI, 2009, vol. 6, pp. 227–36.10.1115/OMAE2009-80030 ↗
19. M.F. Gittos and H.G. Pisarski: “Materials Selection for Dissimilar Joints in Subsea Hubs,” Final Report, The Welding Institute, Cambridge, United Kingdom, 2006.
20. G.E. Dieter: Mechanical Metallurgy Third Edition, McGraw-Hill, Inc., New York, NY, 1986.
21. J.A. Fenske: Ph.D. Thesis, University of Illinois at Urbana Champaign, 2010.
22. S. Kou and Y.K. Yang: Weld. J., 2007, vol. 86, pp. 303–12.
23. M.L. Santella: J. Press. Vess. Technol., 2012, vol. 134, pp. 021404–5.10.1115/1.4005399 ↗
24. J.P. Hirth: Metall. Trans. A, 1980, vol. 11A, pp. 861–90.10.1007/BF02654700 ↗
25. E. Bain and H.W. Paxton: Alloying Elements in Steel, ASM, Metals Park, OH, 1961.
26. R.A. Oriani and P.H. Josephic: Scripta Metall., 1979, vol. 13, pp. 469–71.10.1016/0036-9748(79)90071-1 ↗
27. P. Novak, R. Yuan, B.P. Somerday, P. Sofronis, and R.O. Ritchie: J. Mech. Phys. Solids, 2010, vol. 58, pp. 206–26.10.1016/j.jmps.2009.10.005 ↗
28. G.M. Pressouyre and I.M. Bernstein: Acta Metall., 1979, vol. 27, pp. 89–100.10.1016/0001-6160(79)90059-2 ↗