journal article·2013-09

Effect of Segregation of Secondary Phase Particles and “S” Line on Tensile Fracture Behavior of Friction Stir-Welded 2024Al-T351 Joints

Z. Zhang, B. L. Xiao, Z. Y. Ma

Publisher page

Abstract

A 5-mm-thick 2024Al-T351 plate was friction stir welded (FSWed) at welding speeds of 100, 200, and 400 mm min−1 with a constant rotation rate of 800 rpm, and the microstructure and tensile fracture behavior of the joints were investigated in detail. FSW resulted in the redistribution of secondary phase particles along the recrystallized grain boundaries at the nugget zone (NZ), forming linear segregation bands consisting of secondary phase particles. The segregation bands, mainly present in the shoulder-driven zone, were believed to result from periodic material flow, with the average band spacing on the longitudinal and horizontal cross sections equal to the tool advancement per revolution. At a low welding speed of 100 mm min−1, in spite of the highest density of segregation bands, the FSWed 2024Al-T351 joint fractured along the low hardness zone (LHZ) of the heat-affected zone because of large hardness gap between NZ and LHZ. Increasing the welding speed to 200 and 400 mm min−1 reduced both the hardness gap between NZ and LHZ and the density of segregation bands. In this case, the segregation bands played a role, resulting in unusual fracture of the joints along the segregation bands. The “S” line originated from the oxide film on the initial butting surfaces and did not affect the fracture behavior of the FSWed 2024Al-T351 joints.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. F. Lefebvre, S. Ganguly and I. Sinclair: Mater. Sci. Eng. A, 2005, vol. 397, pp. 338–45.10.1016/j.msea.2005.02.051 ↗
2. D. Fersini and A. Pirondi: Eng. Fract. Mech., 2007, vol. 74, pp. 468–80.10.1016/j.engfracmech.2006.07.010 ↗
3. W.M. Thomas, E.D. Nicholas, J.C. Needham, M.G. Murch, P. Templesmith, and C.J. Dawes: G.B. Patent Application No. 9125978.8, 1991.
4. M.A. Sutton, B.Yang, A.P. Reynolds and R. Taylor: Mater. Sci. Eng. A, 2002, vol. 323, pp. 160–66.10.1016/S0921-5093(01)01358-2 ↗
5. Y.S. Sato and H. Kokawa: Metall. Mater. Trans. A, 2001, vol. 32A, pp. 3023–31.10.1007/s11661-001-0177-8 ↗
6. S.R. Ren, Z.Y. Ma, L.Q. Chen : Scripta Mater., 2007, vol. 56, pp. 69–72.10.1016/j.scriptamat.2006.08.054 ↗
7. F.C. Liu, Z.Y. Ma: Metall. Mater. Trans. A, 2008, vol. 39A, pp.2378–88.10.1007/s11661-008-9586-2 ↗
8. C.B. Fuller, M.W. Mahoney, M. Calabrese and L. Micona: Mater. Sci. Eng. A, 2010, vol. 527, pp. 2233–40.10.1016/j.msea.2009.11.057 ↗
9. R. Brown, W. Tang and A.P. Reynolds: Mater. Sci. Eng. A, 2009, vol. 115, pp. 513-14.
10. M.W. Mahoney, C.G. Rhodes, J.G. Flintoff, R.A. Spurling and W.H. Bingel: Metall. Mater. Trans. A, 1998, vol. 29A, pp. 1955–64.10.1007/s11661-998-0021-5 ↗
11. Y.H. Zhao, S.B. Lin, L. Wu and F.X. Qu: Trans. Nonferrous. Met. Soc. China, 2005, vol. 15, pp. 1248–52.
12. H.J. Liu, H. Fujii, M. Maedaa and K. Nogi: J. Mater. Process. Technol., 2003, vol. 142, pp. 692–96.10.1016/S0924-0136(03)00806-9 ↗
13. C. Genevois, A. Deschamps, A. Denquin, B. Doisneau-cottignies: Acta Mater., 2005, vol. 53. pp. 2447–58.10.1016/j.actamat.2005.02.007 ↗
14. H. Aydin, A. Bayram, A. Uguz, K.S. Akay: Mater. Des., 2009, vol. 30, pp. 2211–2221.10.1016/j.matdes.2008.08.034 ↗
15. H. Aydin, A. Bayram, A. Uguz, I. Durgun: Mater. Des., 2010, vol. 31. pp. 2568–77.10.1016/j.matdes.2009.11.030 ↗
16. Srivatsan T.S, Vasudevan S, Park L: Mater. Sci. Eng. A, 2007, vol. 466, pp. 235–45.10.1016/j.msea.2007.02.100 ↗
17. Z. Hu, S. Yuan, X. Wang, G. Liu, Y. Huang: Mater. Des., 2011, vol. 32, pp. 5055–60.10.1016/j.matdes.2011.05.035 ↗
18. K.N. Krishnan: Mater. Sci. Eng. A, 2002, vol. 327, pp. 246–51.10.1016/S0921-5093(01)01474-5 ↗
19. Reynolds, A.P.: Sci. Technol. Weld. Join., 2000, vol. 5, pp. 120–24.10.1179/136217100101538119 ↗
20. Y.S. Sato, H. Takauchi, S.H.C. Park and H. Kokawa: Mater. Sci. Eng. A, 2005, vol. 405, pp. 333–38.10.1016/j.msea.2005.06.008 ↗
21. N. Afrin, D.L. Chen, X. Cao, M. Jahazi : Mater. Sci. Eng. A, 2005, vol. 472, pp. 179–86.10.1016/j.msea.2007.03.018 ↗
22. S. Lim, S. Kim, C.G. Lee, C.D. Yim, S.J. Kim: Metall. Mater. Trans. A. 2005, vol. 36A, pp. 1609-12.10.1007/s11661-005-0252-7 ↗
23. M. Abbasi Gharacheh, A.H. Kokabi, G.H. Daneshi, B. Shalchi and R. Sarrafi: Int. J. Mach. Tool. Manuf., 2006, vol. 46, pp. 1983–87.10.1016/j.ijmachtools.2006.01.007 ↗
24. C.Z. Zhou, X.X. Yang, G.H. Luan: Scripta Mater., 2006, vol. 54, pp. 1515–20.10.1016/j.scriptamat.2005.12.036 ↗
25. S.S. Di, X.Q. Yang, D.P. Fang, and G.H. Luan: Mater. Chem. Phys., 2007, vol. 104, pp. 244–48.10.1016/j.matchemphys.2007.01.023 ↗
26. L. Fratini, G. Buffa and R. Shivpuri: Acta Mater., 2008, vol. 58, pp. 2056–67.10.1016/j.actamat.2009.11.048 ↗
27. K. Kumar and S.V. Kailas: Mater. Sci. Eng. A. 2008, vol. 485, pp. 367–74.10.1016/j.msea.2007.08.013 ↗
28. Z. Zhang, B.L. Xiao, D. Wang, Z.Y. Ma: Metall. Mater. Trans. A, 2011, vol. 42A, pp. 1717–26.10.1007/s11661-010-0545-3 ↗
29. W.J. Arbegast: Scripta Mater., 2008, vol. 58, pp. 372–76.10.1016/j.scriptamat.2007.10.031 ↗
30. Z. Liu, P.H. Chong, A.N. Butt, P. Skeldon, G.E. Thompson: Appl. Surf. Sci., 2005, vol. 247, pp. 294–99.10.1016/j.apsusc.2005.01.067 ↗
31. D.Q. Zhu and W.J. van Ooij: Corros. Sci., 2003, vol.45, pp. 2177–97.10.1016/S0010-938X(03)00061-1 ↗
32. S.W. Xu and X.M. Deng: Acta Mater., 2008, vol. 56, pp. 1326–41.10.1016/j.actamat.2007.11.016 ↗
33. KA.A. Hassan, P.B. Prangnell, A.F. Norman, D.A. Price, S.W. Williams: Sci. Tech. Weld. Joi., 2003, vol. 8, pp. 257–68.10.1179/136217103225005480 ↗
34. A.P. Reynolds, W. Tang, Z. Khandkar, J.A. Khan, K. Lindner: Sci. Technol. Weld. Join., 2005, vol. 10, pp. 190–99.10.1179/174329305X37024 ↗
35. M.W. Mahoney, C.G. Rhodes, J.G. Flintoff, R.A. Spurling, W.H. Bingel: Metall. Mater. Trans. A, 1998, vol. 29A, pp. 1955–64.10.1007/s11661-998-0021-5 ↗
36. P.A. Colegrove and H.R. Shercliff: Sci. Technol. Weld. Join., 2003, vol. 8, pp. 360–68.10.1179/136217103225005534 ↗
37. Y.S. Sato, M. Urata, H. Kokawa: Metall. Mater. Trans. A, 2002, vol. 33A, pp. 625–35.10.1007/s11661-002-0124-3 ↗
38. Z.W. Chen and S. Cui: Scripta Mater., 2008, vol. 58, pp. 417–20.10.1016/j.scriptamat.2007.10.026 ↗
39. G.R. Cui, Z.Y. Ma, S.X. Li: Scripta Mater., 2008, vol. 58, pp.1082–85.10.1016/j.scriptamat.2008.02.003 ↗
40. A.P. Reynolds: Scripta Mater., 2008, vol.58, pp. 338–42.10.1016/j.scriptamat.2007.10.048 ↗
41. A. Arora, Z. Zhang, A. De, and T. DebRoy: Scripta Mater., 2009, vol. 61, pp. 863–66.10.1016/j.scriptamat.2009.07.015 ↗
42. X. Deng and S. Xu: Trans. NAMRI/SME, 2001, vol. 28, pp. 631–38.
43. P.B. Prangnell and C.P. Heason: Acta Mater., 2005, vol. 53, pp. 3179–92.10.1016/j.actamat.2005.03.044 ↗