Water Penetration—Its Effect on the Strength and Toughness of Silica Glass
Source abstract
Abstract
When a crack forms in silica glass, the surrounding environment flows into the crack opening, and water from the environment reacts with the glass to promote crack growth. A chemical reaction between water and the strained crack-tip bonds is commonly regarded as the cause of subcritical crack growth in glass. In silica glass, water can also have a secondary effect on crack growth. By penetrating into the glass, water generates a zone of swelling and, hence, creates a compression zone around the crack tip and on the newly formed fracture surfaces. This zone of compression acts as a fracture mechanics shield to the stresses at the crack tip, modifying both the strength and subcritical crack growth resistance of the glass. Water penetration is especially apparent in silica glass because of its low density and the fact that it contains no modifier ions. Using diffusion data from the literature, we show that the diffusion of water into silica glass can explain several significant experimental observations that have been reported on silica glass, including (1) the strengthening of silica glass by soaking the glass in water at elevated temperatures, (2) the observation of permanent crack face displacements near the crack tip of a silica specimen that had been soaked in water under load, and (3) the observation of high concentrations of water close to the fracture surfaces that had been formed in water. These effects are consistent with a model suggesting that crack growth in silica glass is modified by a physical swelling of the glass around the crack tip. An implication of water-induced swelling during fracture is that silica glass is more resistant to crack growth than it would be if swelling did not occur.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Glass properties and applications · Structural Analysis of Composite Materials · Building materials and conservation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. D.W. Richerson: The Magic of Ceramics, The American Ceramic Society, Westerville, OH, 2000.
2. A.K. Varshneya: Fundamentals of Inorganic Glasses, Academic Press, Inc., Harcourt Brace & Company, Publishers, San Diego, CA, 1994.10.1016/B978-0-08-057150-8.50025-2 ↗
3. S.W. Freiman, S.M. Wiederhorn, and J.J. Mecholsky: J. Am. Ceram. Soc., 2009, vol. 92, no. 7, pp. 1371–82.10.1111/j.1551-2916.2009.03097.x ↗
4. M. Ciccotti: J. Phys. D: Appl. Phys., 2009, vol. 42, p. 214006.10.1088/0022-3727/42/21/214006 ↗
5. B.R. Lawn: Fracture of Brittle Solids, 2nd ed., Cambridge University Press, Cambridge, U.K., 1993.10.1017/CBO9780511623127 ↗
6. C.R. Kurkjian, P.K. Gupta, R.K. Brow, and N. Lower: J. Noncryst. Solids, 2003, vol. 316, pp. 114–24.10.1016/S0022-3093(02)01943-9 ↗
7. L. Pauling: The Nature of the Chemical Bond, 3rd ed., Cornell University Press, Ithaca, NY, 1960.
8. R.M. McMeeking and A.G. Evans: J. Am. Ceram. Soc., 1982, vol. 65, pp. 242–46.10.1111/j.1151-2916.1982.tb10426.x ↗
9. J.E. Shelby: J. Non-Cryst., 2004, no. 349, pp. 331–36.10.1016/j.jnoncrysol.2004.08.206 ↗
10. R. Bruckner: Glastech. Ber., 1970, vol. 43, pp. 8–12.
11. R. Bruckner: J. Non-Cryst. Solids, 1971, vol. 5, pp. 281–85.10.1016/0022-3093(71)90068-8 ↗
12. J.F. Shackelford, J.S. Masaryk, and R.M. Fulrath: J. Am. Ceram. Soc., 1970, vol. 53, p. 417.10.1111/j.1151-2916.1970.tb12145.x ↗
13. M. Tomozawa, W.-T. Han, and W.A. Lanford: J. Am. Ceram. Soc., 1991, vol. 74, no. 10, pp. 2573–76.10.1111/j.1151-2916.1991.tb06801.x ↗
14. F. Lechenault, D.L. Rountree, F. Cousin, J.-P Bouchaud, L. Ponson, and E. Bouchaud: Phys. Rev. Lett., 2011, vol. 106, p. 165504.10.1103/PhysRevLett.106.165504 ↗
15. C. Janssen: Proceedings of Tenth International Congress on Glass, Kyoto, Japan 1974, Ceramic Society of Japan, Tokyo, Japan, 1974, pp. 10–23.
16. T.A. Michalske, W.L. Smith, and E.P. Chen: Eng. Fract. Mech., 1993, vol. 45, pp. 637–42.10.1016/0013-7944(93)90269-X ↗
17. M.Y. He, M.R. Turner, and A.G. Evans: Acta Metall. Mater., 1995, vol. 43, pp. 3453–58.10.1016/0956-7151(95)00036-U ↗
18. A. Zouine, O. Dersch, G. Walter, and F. Rauch: Phys. Chem. Glasses, 2007, vol. 48, pp. 85–91.
19. S. Ito and M. Tomozawa: J. Am. Ceram. Soc., 1982, vol. 65, no. 8, pp. 368–71.10.1111/j.1151-2916.1982.tb10486.x ↗
20. K. Hirao and M. Tomozawa: J. Am. Ceram. Soc., 1987, vol. 70, no. 6, pp. 377–82.10.1111/j.1151-2916.1987.tb05654.x ↗
21. S.M. Wiederhorn, T. Fett, G. Rizzi, M.J. Hoffmann, and J.-P. Guin: Eng. Fract. Mech., 2012, in press.
22. S.M. Wiederhorn: J. Am. Ceram. Soc., 1969, vol. 52, no. 2, pp. 99–105.10.1111/j.1151-2916.1969.tb13350.x ↗
23. S.M. Wiederhorn, T. Fett, G. Rizzi, S. Fünfschilling, M.J. Hoffmann, and J.-P. Guin: J. Am. Ceram. Soc., 2011, vol. 94, no. S1, pp. S196–S203.10.1111/j.1551-2916.2011.04530.x ↗
24. Mathematica: Wolfram Research, Champaign, IL.
25. K. Han, M. Ciccotti, and S. Roux: EPL, 2010, vol. 89, p. 66003.10.1209/0295-5075/89/66003 ↗
26. S.M. Wiederhorn, S.W. Freiman, E.R. Fuller, Jr., and C.J. Simmons: J. Mater. Sci., 1982, vol. 17, pp. 3460–78.10.1007/BF00752191 ↗
27. S.M. Wiederhorn, E.R. Fuller, Jr., and R. Thomson: Met. Sci., 1980, vol. 14, pp. 450–8.10.1179/msc.1980.14.8-9.450 ↗
28. R.H. Doremus: J. Mater. Res., 1995, vol. 10, pp. 2379–89.10.1557/JMR.1995.2379 ↗
29. S.M. Wiederhorn and L.H.Bolz: J. Am. Ceram. Soc., 1970, vol. 53, no. 10, pp. 543–48.10.1111/j.1151-2916.1970.tb15962.x ↗
30. G.W. Weidmann and D.G. Holloway: Phys. Chem. Glasses, 1974, vol. 15, pp. 68–75.
31. D.H. Roach, S. Lathabai, and B.R. Lawn: J. Am. Ceram. Soc., 1988, vol. 71, no. 2, pp. 97–105.10.1111/j.1151-2916.1988.tb05824.x ↗
32. T. Fett and D. Munz: Stress Intensity Factors and Weight Functions, Computational Mechanics Publications, Southampton, U.K., 1997.