journal article·2012-09

Full Densification of Molybdenum Powders Using Spark Plasma Sintering

B. Mouawad, M. Soueidan, D. Fabrègue, C. Buttay, V. Bley, B. Allard, H. Morel

Publisher page

Abstract

Pure molybdenum powder was sintered using Spark Plasma Sintering under various temperatures, and holding times, under a pressure of 77 MPa and a heating rate at 700°C/min. After sintering, a carbide layer was observed at the surface. The carbide layer thickness, the relative density of the sample as well as the microhardness and the grain size of Mo were measured. The carbide thickness depends on time and temperature and it was found that the carbide layer grows in a parabolic manner, with the activation energy of carbon diffusion in Mo being equal to 34 Kcal/mol. The densification of Mo is controlled mainly by the sintering temperature and the holding time. The molybdenum powder was successfully consolidated by SPS in short times. A relative density of 100% is achieved at a sintering temperature of 1850°C and a holding time of 30 minutes. It was shown that the hardness decreases slightly with temperature and time. It should be related to the increase in grain size with the sintering temperature and time.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. E.R. Braithwaite and J. Haber: Stud. Org. Chem., 1994, vol. 19, p. 662.
2. J.A. Shields and E.L. Baker: Adv. Mater. Process., 1999, vol. 155, pp. 61–64.
3. E.F. Baroch, M. Ostermann, and G. Patrick: Adv. Powder Metall., 1991, vol. 5, pp. 321–31.
4. T.S. Srivatsan, B.G. Ravi, M. Petraroli, and T.S. Sudarshan: Int. J. Refract. Met. Hard Mater., 2002, vol. 20, pp. 181–86.10.1016/S0263-4368(01)00076-2 ↗
5. P. Garg, S.J. Park, and R.M. German: Int. J. Refract. Met. Hard Mater., 2007, vol. 25, pp. 16–24.10.1016/j.ijrmhm.2005.10.014 ↗
6. H. Schwarzbauer and R. Kuhnert: IEEE Trans. Ind. Appl., 1991, vol. 27, pp. 93–95.10.1109/28.67536 ↗
7. R.M. German and C.A. Labombard: Int. J. Powder Metall. Powder Technol., 1982, vol. 18, pp. 147–50.
8. P.E. Zovas and R.M. German: Metall. Trans. A, 1983, vol. 15A, pp. 1103–10.
9. H. Hofmann, M. Grosskopf, M. Hofmann-Amten-Brink, and G. Petzow: Powder Metall., 1986, vol. 29, pp. 201–06.10.1179/pom.1986.29.3.201 ↗
10. Y. Hiraoka, T. Ogusu, and N. Yoshizawa: J. Alloys Compd., 2004, vol. 381, pp. 192–96.10.1016/j.jallcom.2004.03.112 ↗
11. K.S. Hwang and H.S. Huang: Acta Mater., 2003, vol. 51, pp. 3915–26.10.1016/S1359-6454(03)00216-7 ↗
12. K.S. Hwang and H.S. Huang: Int. J. Refract. Hard Mater., 2004, vol. 22, pp. 185–91.10.1016/j.ijrmhm.2004.06.003 ↗
13. R.M. German and Z.A. Munir: J. Less-Common Met., 1978, vol. 58, pp. 61–74.10.1016/0022-5088(78)90071-1 ↗
14. L.E. Murr, M.A. Meyers, and L.E. Murr: Shock Waves and High Strain-Rate Phenomena: Concepts and Applications, Plenum, New York, NY, 1981.
15. M. Meyers, B.B. Gupta, and L.E. Murr: J. Met., 1981, vol. 33, pp. 21–26.
16. D. Raybould, D. Morris, and G. Cooper: J. Mater. Sci., 1979, vol. 14, pp. 2523–26.10.1007/BF00737047 ↗
17. A.M. Staver: in Proc. Int. Conf., Shock Waves High Strain Rate Phenomena in Metals, M.A. Meyers and L.E. Murr, eds., Plenum, New York, NY, 1981, pp. 865–69.10.1007/978-1-4613-3219-0_49 ↗
18. P. Kasiraj, P.J. Kasiraj, R.B. Schwarz, and T.J. Ahrens: J. Mater. Sci., 1984, vol. 32, pp. 1235–41.
19. R.V. Raman: Adv. Mater. Process., 1990, vol. 137, p. 109.
20. C.A. Kelto, E.E. Timm, and A.J. Pyzik: Annu. Rev. Mater. Sci., 1989, vol. 19, pp. 527–50.10.1146/annurev.ms.19.080189.002523 ↗
21. G. Jones, J.R. Groza, K. Yamazaki, and K. Shoda: Mater. Manuf. Process., 1994, vol. 9, pp. 1105–14.10.1080/10426919408934978 ↗
22. J. Groza, S.H. Risbud, and K. Yamazaki: J. Mater. Res., 1992, vol. 7, pp. 2643–45.10.1557/JMR.1992.2643 ↗
23. B.G. Ravi, P.D. Ramesh, N. Gupta, and K.J. Rao: J. Mater. Chem., 1997, vol. 7, pp. 2043–48.10.1039/a701976i ↗
24. B.G. Ravi, V. Praveen, M.P. Selvam, and K.J. Rao: Mater. Res. Bull., 1998, vol. 33, pp. 1527–36.10.1016/S0025-5408(98)00135-4 ↗
25. S.H. Yoo, T.S. Sudarshan, K. Sethuram, G. Subhash, and R.J. Dowding: Powder Metall., 1999, vol. 42, pp. 181–82.10.1179/003258999665549 ↗
26. T.S. Srivatsan, B.G. Ravi, A.S. Naruka, L. Riester, M. Petraroli, and T.S. Sudarshan: J. Powder Technol., 2001, vol. 114, pp. 136–44.10.1016/S0032-5910(00)00285-0 ↗
27. Z. Shen and M. Nygren: J. Mater. Chem., 2001, vol. 11, pp. 204–07.10.1039/b003200j ↗
28. L. Gao, J.S. Hong, H. Miyamoto, and S.D.D.L. Torre: J. Eur. Ceram. Soc., 2000, vol. 20, pp. 2149–52.10.1016/S0955-2219(00)00086-8 ↗
29. Z. Munir, U. Anselmi-Tamburini, and M. Ohyanagi: J. Mater. Sci., 2006, vol. 41, pp. 763–77.10.1007/s10853-006-6555-2 ↗
30. D.M. Hulbert, A. Anders, J. Andersson, E.J. Lavernia, and A.K. Mukherjee: Scripta Mater., 2009, vol. 60, pp. 835–38.10.1016/j.scriptamat.2008.12.059 ↗
31. R. Ohser-Wiedemann, U. Martin, H.J. Seifert, and A. Müller: Int. J. Refract. Met. Hard Mater., 2010, vol. 28, pp. 550–57.10.1016/j.ijrmhm.2010.03.003 ↗
32. E. Parthé and V. Sadogopan: Acta Crystallogr., 1963, vol. 16, pp. 202–05.10.1107/S0365110X63000487 ↗
33. P. Liu and J.A. Rodriguez: J. Chem. Phys., 2004, vol. 120, p. 5414.10.1063/1.1647050 ↗
34. K. Oshikawa, M. Nagai, and S. Omi: J. Phys. Chem. B, 2001, vol. 105, pp. 9124–31.10.1021/jp0111867 ↗
35. L. Börnestein: Condens. Matter, 2006, vol. 26.
36. Y. Isobe, P. Son, and M. Miyake: J. Less-Common Met., 1989, vol. 147, pp. 261–68.10.1016/0022-5088(89)90199-9 ↗
37. S.M. Tuominen and J.M. Dahl: 108th AIME Annual Meeting, New Orleans, LA, Feb. 1979.
38. G.-S. Kim, H.G. Kim, D.-G. Kim, S.-T. Oh, M.-J. Suk, and Y.D. Kim: J. Alloys Compd., 2009, vol. 469, pp. 401–05.10.1016/j.jallcom.2008.01.149 ↗
39. T.S. Srivatsan, B.G. Ravi, M. Petraroli, and T.S. Sudarshan: Int. J. Refract. Met. Hard Mater., 2002, vol. 20, pp. 181–86.10.1016/S0263-4368(01)00076-2 ↗