Abstract
The fatigue strength and crack initiation mechanisms of very-high-cycle fatigue (VHCF) for two low alloy steels were investigated. Rotary bending tests at 52.5 Hz with hour-glass type specimens were carried out to obtain the fatigue propensity of the test steels, for which the failure occurred up to the VHCF regime of 108 cycles with the S-N curves of stepwise tendency. Fractography observations show that the crack initiation of VHCF is at subsurface inclusion with “fish-eye” pattern. The fish-eye is of equiaxed shape and tends to tangent the specimen surface. The size of the fish-eye becomes large with the increasing depth of related inclusion from the surface. The fish-eye crack grows faster outward to the specimen surface than inward. The values of the stress intensity factor (K I ) at different regions of fracture surface were calculated, indicating that the K I value of fish-eye crack is close to the value of relevant fatigue threshold (ΔK th ). A new parameter was proposed to interpret the competition mechanism of fatigue crack initiation at the specimen surface or at the subsurface. The simulation results indicate that large inclusion size, small grain size, and high strength of material will promote fatigue crack initiation at the specimen subsurface, which are in agreement with experimental observations.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fatigue and fracture mechanics · Fire effects on concrete materials · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. A. Wöhler: Engineering, 1867, vol. 2, pp. 160–61.
2. Annual Book of ASTM Standards, E468-90 (2004), ASTM, Philadelphia, PA, 2006, Sect. 3, vol. 03.01, pp. 556–61.
3. M. Kikukawa, K. Ohji, and K. Ogura: J. Basic Eng., Trans. ASME D, 1965, vol. 87D, pp. 857–64.10.1115/1.3650830 ↗
4. T. Naito, H. Ueda, and M. Kikuchi: J. Soc. Mater. Sci. Jpn., 1983, vol. 32, pp. 1162–66.10.2472/jsms.32.1162 ↗
5. T. Naito, H. Ueda, and M. Kikuchi: Metall. Trans. A, 1984, vol. 15A, pp. 1431–36.10.1007/BF02648572 ↗
6. S.E. Stanzl, E.K. Tschegg, and H. Mayer: Int. J. Fatigue, 1986, vol. 8, pp. 195–200.10.1016/0142-1123(86)90021-6 ↗
7. P. Lukáš and L. Kunz: Fatigue Fract. Eng. Mater. Struct., 2002, vol. 25, pp. 747–53.10.1046/j.1460-2695.2002.00562.x ↗
8. Y. Murakami, N.N. Yokoyama, and J. Nagata: Fatigue Fract. Eng. Mater. Struct., 2002, vol. 25, pp. 735–46.10.1046/j.1460-2695.2002.00576.x ↗
9. C. Bathias and P.C. Paris: Gigacycle Fatigue in Mechanical Practice, Marcel Dekker, New York, NY, 2005.
10. H. Emura and K. Asami: Trans. JSME, Part A, 1989, vol. 55, pp. 45–50.10.1299/kikaia.55.45 ↗
11. T. Sakai, Y. Sato, and N. Oguma: Fatigue Fract. Eng. Mater. Struct., 2002, vol. 25, pp. 765–73.10.1046/j.1460-2695.2002.00574.x ↗
12. K. Shiozawa, L. Lu, and S. Ishihara: Fatigue Fract. Eng. Mater. Struct., 2001, vol. 24, pp. 781–90.10.1046/j.1460-2695.2001.00459.x ↗
13. Y. Ochi, T. Matsumura, K. Masaki, and S. Yoshida: Fatigue Fract. Eng. Mater. Struct., 2002, vol. 25, pp. 823–30.10.1046/j.1460-2695.2002.00575.x ↗
14. S. Nishijima and K. Kanazawa: Fatigue Fract. Eng. Mater. Struct., 1999, vol. 22, pp. 601–07.10.1046/j.1460-2695.1999.00206.x ↗
15. C. Bathias: Fatigue Fract. Eng. Mater. Struct., 1999, vol. 22, pp. 559–65.10.1046/j.1460-2695.1999.00183.x ↗
16. Q.Y. Wang, J.Y. Berard, S. Rathery, and C. Bathias: Fatigue Fract. Eng. Mater. Struct., 1999, vol. 22, pp. 673–77.10.1046/j.1460-2695.1999.t01-1-00184.x ↗
17. M.D. Chapetti, T. Tagawa, and T. Miyata: Mater. Sci. Eng. A, 2003, vol. 356, pp. 236–44.10.1016/S0921-5093(03)00136-9 ↗
18. Y. Hong, A. Zhao, and G. Qian: Acta Metall. Sinica, 2009, vol. 45, pp. 769–80.
19. G. Qian, C. Zhou, and Y. Hong: Acta Mater., 2011, vol. 59, pp. 1321–27.10.1016/j.actamat.2010.10.064 ↗
20. E. Takeuchi, Y. Furuya, N. Nagashima, and S. Matsuoka: Fatigue Fract. Eng. Mater. Struct., 2008, vol. 31, pp. 599–605.10.1111/j.1460-2695.2008.01257.x ↗
21. C. Sun, A. Zhao, and Y. Hong: Struct. Longevity, 2011, vol. 045, pp. 1–12.
22. T. Sakai: J. Solid Mech. Mater. Eng., 2009, vol. 3, pp. 425–39.10.1299/jmmp.3.425 ↗
23. T. Sakai, Y. Sato, Y. Nagano, M. Takeda, and N. Oguma: Int. J. Fatigue, 2006, vol. 28, pp. 1547–54.10.1016/j.ijfatigue.2005.04.018 ↗
24. K. Shiozawa, Y. Morii, S. Nishino, and L. Lu: Int. J. Fatigue, 2006, vol. 28, pp. 1521–32.10.1016/j.ijfatigue.2005.08.015 ↗
25. G. Qian and Y. Hong: Acta Metall. Sinica, 2009, vol. 45, pp. 1356–63.
26. G. Qian, Y. Hong, and C. Zhou: Eng. Failure Analysis, 2010, vol. 17, pp. 1517–25.10.1016/j.engfailanal.2010.06.002 ↗
27. Y.L. Bai, M.F. Xia, H.Y. Wang, and F.J. Ke: China Particuology, 2003, vol. 1, pp. 7–12.10.1016/S1672-2515(07)60093-1 ↗
28. T. Tanaka and T. Mura: J. Appl. Mech., Trans. ASME, 1981, vol. 48, pp. 97–103.10.1115/1.3157599 ↗
29. T. Tanaka and T. Mura: Metall. Trans. A, 1982, vol. 13A, pp. 117–23.10.1007/BF02642422 ↗