Abstract

The susceptibility of Mg-Al-Sr alloys to hot tearing during permanent mold casting was investigated using constrained rod casting (CRC) in a steel mold. The alloys included Mg-xAl-1.5Sr and Mg-xAl-3Sr, where x = 4, 6, or 8 wt pct. The hot-tearing susceptibility (HTS) was determined based on the widths and locations of the cracks in the rods. With the Mg-xAl-1.5 Sr alloys, the HTS decreased significantly with increasing Al content. With the Mg-xAl-3Sr alloys, the trend was similar but not as significant. At the same Al content, the HTS was significantly lower at 3 wt pct Sr than at 1.5 wt pct Sr. To help understand the HTS of these alloys, the solidification path and phase fractions were calculated for each alloy. The HTS was found to increase with increasing fraction solid at the end of primary solidification.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. R.A. Dodd, W.A. Pollard, and J.W. Meier: Trans. AFS, 1957, vol. 65, pp. 100–16.
2. R.A. Rosenberg, M.C. Flemings, and H.F. Taylor: Trans. AFS, 1960, vol. 68, pp. 518–28.
3. G. Cao and S. Kou: Mater. Sci. Eng., A, 2006, vol. 417 (1–2), pp. 230–38.10.1016/j.msea.2005.10.050 ↗
4. D. Argo, M. Pekguleryuz, P. Vermette, and M. Lefebvre: Die Casting 2001, North American Die Casting Association, Cincinnati, OH, Oct. 29–Nov. 1, 2001, pp. 181–86.
5. Y. Wang, B. Sun, Q. Wang, Y. Zhu, and W. Ding: Mater. Lett., 2002, vol. 53 (1–2), pp. 35–39.10.1016/S0167-577X(01)00449-9 ↗
6. B. Powell, A.A. Luo, B.L. Tiwari, and V. Rezhets: in Magnesium Technology, H.I. Kaplan, ed., TMS, Warrendale, PA, 2002, pp. 123–29.
7. G. Cao and S. Kou: Metall. Mater. Trans. A, 2006, vol. 37A, pp. 3647–63.10.1007/s11661-006-1059-x ↗
8. S. Lin, C. Aliravci, and M.O. Pekguleryuz: Metall. Mater. Trans. A, 2007, vol. 38A, pp. 1056–68.10.1007/s11661-007-9132-7 ↗
9. C. Zhang, H.B. Cao, G.P. Cao, S. Kou, and Y.A. Chang: JOM, 2008, vol. 60 (12), pp. 48–51.10.1007/s11837-008-0166-0 ↗
10. Pandat—Phase Diagram Calculation Software Package for Multicomponent Systems, Computherm LLC, Madison, WI.
11. PanMg—Database for Mg Alloys, CompuTherm LLC, Madison, WI.
12. M.C. Flemings: Solidification Processing, McGraw-Hill, New York, NY, 1974.
13. T.W. Clyne and G.J. Davies: Br. Foundryman, 1981, vol. 74 (4), pp. 65–73.
14. J. Campell: Castings, 2nd ed., Butterworth Heinemann, Oxford, United Kingdom, 2003.
15. D.G. Eskin, Suyitno, and L. Katgerman: Prog. Mater. Sci., 2004, vol. 79, pp. 629–711.10.1016/S0079-6425(03)00037-9 ↗