Mechanical Properties of Super Duplex Stainless Steel 2507 after Gas Phase Thermal Precharging with Hydrogen
Source abstract
Abstract
Thermal precharging of super duplex stainless steel 2507 with 125 wppm hydrogen significantly reduced tensile ductility and fracture toughness. Strain-hardened 2507 exhibited more severe ductility loss compared to the annealed microstructure. The reduction of area (RA) was between 80 and 85 pct for both microstructures in the noncharged condition, while reductions of area were 25 and 46 pct for the strain-hardened and annealed microstructures, respectively, after hydrogen precharging. Similar to the effect of internal hydrogen on tensile ductility, fracture toughness of strain-hardened 2507 was lowered from nearly 300 MPa m1/2 in the noncharged condition to less than 60 MPa m1/2 in the hydrogen-precharged condition. While precharging 2507 with hydrogen results in a considerable reduction in ductility and toughness, the absolute values are similar to high-strength austenitic steels that have been tested under the same conditions, and which are generally considered acceptable for high-pressure hydrogen gas systems. The fracture mode in hydrogen-precharged 2507 involved cleavage cracking of the ferrite phase and ductile fracture along oblique planes in the austenite phase, compared to 100 pct microvoid coalescence in the absence of hydrogen. Predictions from a strain-based micromechanical fracture toughness model were in good agreement with the measured fracture toughness of hydrogen-precharged 2507, implying a governing role of austenite for resistance to hydrogen-assisted fracture.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Fatigue and fracture mechanics · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (67)
Show source-provided references
1. H.R. Gray, H.G. Nelson, R.E. Johnson, W.B. McPherson, F.S. Howard, J.H. Swisher: Int. J. Hydrogen Energy, 1978, vol. 3, pp. 105–1810.1016/0360-3199(78)90059-9 ↗
2. H.G. Nelson: in Embrittlement of Engineering Alloys, C.L. Briant and S.K. Banerji, eds., Academic Press, New York, 1983, pp. 275–35910.1016/B978-0-12-341825-8.50014-3 ↗
3. W. Zheng, D. Hardie: Corr. Sci, 1991, vol. 32, pp. 23–3610.1016/0010-938X(91)90061-S ↗
4. W. Zheng, D. Hardie: Corrosion, 1991, vol. 47, pp. 792–9910.5006/1.3585190 ↗
5. A.A. El-Yazgi, D. Hardie: Corr. Sci, 1996, vol. 38, pp. 735–4410.1016/0010-938X(95)00162-D ↗
6. A.A. El-Yazgi, D. Hardie: Mater. Sci. Technol., 2000, vol. 16, pp. 506–1010.1179/026708300101508162 ↗
7. H.G. Nelson and J.E. Stein: Report No. NASA TN D-7265, Ames Research Center, National Aeronautics and Space Administration, Moffett Field, CA, Apr. 1973
8. M.R. Louthan, R.G. Derrick, J.A. Donovan, and G.R. Caskey: in Effect of Hydrogen on Behavior of Materials: Proceedings of an International Conference, 1975, Moran WY, A.W. Thompson and I.M. Bernstein, eds., Metallurgical Society of the AIME, New York, 1976, pp. 337–47
9. M.R. Louthan, R.G. Derrick: Corr. Sci., 1975, vol. 15, pp. 565–7710.1016/0010-938X(75)90022-0 ↗
10. M.R. Louthan, G. Caskey: Int. J. Hydrogen Energy, 1976, vol. 1, pp. 291–30510.1016/0360-3199(76)90024-0 ↗
11. T.-P. Perng, C.J. Altstetter: Acta Metall, 1986, vol. 34, pp. 1771–8110.1016/0001-6160(86)90123-9 ↗
12. T.-P. Perng, M. Johnson, C.J. Altstetter: Acta Metall., 1989, vol. 37, pp. 3393–9710.1016/0001-6160(89)90211-3 ↗
13. R.B. Hutchings, A. Turnbull, A.T. May: Scripta Metall. Mater., 1991, vol. 25, pp. 2657–6210.1016/0956-716X(91)90134-M ↗
14. A. Turnbull, R.B. Hutchings: Mater. Sci. Eng., 1994, vol. A177, pp. 161–7110.1016/0921-5093(94)90488-X ↗
15. F. Iacoviello, M. Habashi, M. Cavallini: Mater. Sci. Eng., 1997, vol. A224, pp. 116–2410.1016/S0921-5093(96)10545-1 ↗
16. S.S. Chen, T.I. Wu, J.K. Wu: J. Mater. Sci., 2004, vol. 39, pp. 67–7110.1023/B:JMSC.0000007729.14528.a8 ↗
17. M. Baskes: Report No. SAND83-8231, Sandia National Laboratories, Livermore, CA, June 1983
18. M.F. Hardwick and S.L. Robinson: Report No. SAND99–8202, Sandia National Laboratories, Livermore, CA, Nov. 1998
19. L. Ma, G. Liang, J. Tan, L. Rong, Y. Li: J. Mater. Sci. Technol., 1999, vol. 15, pp. 67–7010.1179/026708399773002836 ↗
20. R.J. Walter and W.T. Chandler: Report No. NASA CR-102425, Rocketdyne for NASA, Canoga Park, CA, Feb. 1969
21. R.P. Jewitt, R.J. Walter, W.T. Chandler, and R.P. Frohmberg: Report No. NASA CR-2163, Rocketdyne for NASA, Canoga Park, CA, Mar. 1973
22. B.C. Odegard, A.J. West: Mater. Sci. Eng., 1975, vol. 19, pp. 261–7010.1016/0025-5416(75)90113-5 ↗
23. T.L. Anderson: Fracture Mechanics: Fundamentals and Applications, CRC Press, Boca Raton, FL, 1995
24. C. San Marchi, D.K. Balch, and B.P. Somerday: Proc. PVP-2005: ASME Pressure Vessels and Piping Division Conf., Denver, CO, ASME, New York, July 17–21, 2005
25. C. San Marchi, B.P. Somerday, S.L. Robinson: Int. J. Hydrogen Energy, 2007, vol. 32, pp. 100–1610.1016/j.ijhydene.2006.05.008 ↗
26. X.K. Sun, J. Xu, Y.Y. Li: Mater. Sci. Eng., 1989, vol. A114, pp. 179–87
27. J.H. Holbrook and A.J. West: in Hydrogen Effects in Metals: Proceedings of the Third International Conference on Effect of Hydrogen on Behavior of Materials, 1980, Moran WY, I.M. Bernstein and A.W. Thompson, eds., The Metallurgical Society of AIME, New York, 1981, pp. 655–63
28. G.R. Caskey: Report No. DP-1643, EI du Pont Nemours, Savannah River Laboratory, Aiken, SC, June 1983
29. J.P. Hirth: Metall. Trans. A, 1980, vol. 11A, pp. 861–9010.1007/BF02654700 ↗
30. G.J. Thomas: in Hydrogen Effects in Metals: Proceedings of the Third International Conference on Effect of Hydrogen on Behavior of Materials, 1980, Moran WY, I.M. Bernstein and A.W. Thompson, eds., The Metallurgical Society of AIME, New York, 1981, pp. 77–85
31. E.J. Vesely, R.K. Jacobs, M.C. Watwood, and W.B. McPherson: in Hydrogen Effects in Materials: Proceedings of the Fifth International Conference on the Effect of Hydrogen on the Behavior of Materials, 1994, Moran WY, A.W. Thompson and N.R. Moody, eds., TMS, Warrendale, PA, 1996, pp. 363–7410.1002/9781118803363.ch34 ↗
32. M.C. Young, S.L.I. Chan, L.W. Tsay, C.S. Shin: Mater. Chem. Phys., 2005, vol. 91, pp. 21–2710.1016/j.matchemphys.2004.10.042 ↗
33. H. Sieurin, R. Sandstrom: Eng. Fract. Mech., 2006, vol. 73, pp. 377–9010.1016/j.engfracmech.2005.03.009 ↗
34. N.R. Moody, M.W. Perra, and S.L. Robinson: in Hydrogen Effects on Material Behavior: Proceedings of the Fourth International Conference on the Effect of Hydrogen on the Behavior of Materials, 1989, Moran WY, N.R. Moody and A.W. Thompson, eds., TMS, Warrendale, PA, 1990, pp. 625–35
35. M.W. Perra: in Environmental Degradation of Engineering Materials in Hydrogen, M.R. Louthan, R.P. McNitt and R.D. Sisson, eds., Laboratory for the Study of Environmental Degradation of Engineering Materials, Virginia Polytechnic Institute, Blacksburg, VA, 1981, pp. 321–33
36. N.R. Moody, S.L. Robinson, W.M. Garrison: Res. Mechanica, 1990, vol. 30, pp. 143–206
37. T.J. Marrow, C.A. Hippsley, J.E. King: Acta Metall. Mater., 1991, vol. 39, pp. 1367–7610.1016/0956-7151(91)90224-O ↗
38. R. Oltra, C. Bouillot, R. Magnin: Scripta Mater., 1996, vol. 35, pp. 1101–0510.1016/1359-6462(96)00293-X ↗
39. S.P. Lynch: Acta Metall., 1988, vol. 38, pp. 2639–6110.1016/0001-6160(88)90113-7 ↗
40. S.P. Lynch: Metallography, 1989, vol. 23, pp. 147–7110.1016/0026-0800(89)90016-5 ↗
41. P. Rozenak, I.M. Robertson, H.K. Birnbaum: Acta Metall. Mater., 1990, vol. 38, pp. 2031–4010.1016/0956-7151(90)90070-W ↗
42. H.K. Birnbaum, P. Sofronis: Mater. Sci. Eng., 1994, vol. A176, pp. 191–20210.1016/0921-5093(94)90975-X ↗
43. K.A. Nibur, D.F. Bahr, B.P. Somerday: Acta Mater., 2006, vol. 54, pp. 2677–8410.1016/j.actamat.2006.02.007 ↗
44. P. Sofronis: J. Mech. Phys. Solids, 1995, vol. 43, pp. 1385–40710.1016/0022-5096(95)00037-J ↗
45. G.R. Caskey: in Hydrogen Degradation of Ferrous Alloys, R.A. Oriani, J.P. Hirth, and M. Smialowski, eds., Noyes Publications, Park Ridge, NJ, 1985, pp. 822–62
46. B.C. Odegard, J.A. Brooks, and A.J. West: in Effect of Hydrogen on Behavior of Materials: Proceedings of an International Conference, 1975, Moran WY, A.W. Thompson and I.M. Bernstein, eds., The Metallurgical Society of AIME, New York, 1976, pp. 116–25
47. Y. Liang, P. Sofronis, N. Aravas: Acta Mater., 2003, vol. 51, pp. 2717–3010.1016/S1359-6454(03)00081-8 ↗
48. A.W. Thompson: in Hydrogen in Metals: Proceedings of the International Conference on the Effects of Hydrogen on Materials Properties and Selection and Structural Design, 1973, Champion PA, I.M. Bernstein and A.W. Thompson, eds., American Society of Metals, Metals Park, OH, 1974, pp. 91–105
49. R.O. Ritchie, A.W. Thompson: Metall. Trans. A, 1985, vol. 16A, pp. 233–4810.1007/BF02815305 ↗
50. R.O. Ritchie, J.F. Knott, J.R. Rice: J. Mech. Phys. Solids, 1973, vol. 21, pp. 395–41010.1016/0022-5096(73)90008-2 ↗
51. R.M. McMeeking: J. Mech. Phys. Solids, 1977, vol. 25, pp. 357–8110.1016/0022-5096(77)90003-5 ↗
52. B.P. Somerday, Y. Leng, R.P. Gangloff: Fatigue Fract. Eng. Mater. Struct., 1995, vol. 18, pp. 1031–5010.1111/j.1460-2695.1995.tb01418.x ↗
53. K.S. Chan: Acta Metall., 1989, vol. 37, pp. 1217–2610.1016/0001-6160(89)90116-8 ↗
54. ASTM G 142–98, Standard Test Method for Determination of Susceptibility of Metals to Embrittlement in Hydrogen Containing Environments at High Pressure, High Temperature, or Both, ASTM, Philadelphia, PA, 1998
55. A.W. Thompson, J.A. Brooks: Metall. Trans. A, 1975, vol. 6A, pp. 1431–4210.1007/BF02641935 ↗
56. J.A. Brooks, M.R. Louthan: Metall Trans. A, 1980, vol. 11A, pp. 1981–8610.1007/BF02655117 ↗
57. B.C. Odegard and A.J. West: in Hydrogen Effects in Metals: Proceedings of the Third International Conference on Effect of Hydrogen on Behavior of Materials, 1980, Moran WY, I.M. Bernstein and A.W. Thompson, eds., The Metallurgical Society of AIME, New York, 1981, pp. 597–606
58. S.L. Robinson, N.R. Moody: J. Nucl. Mater., 1986, vol. 140, pp. 245–5110.1016/0022-3115(86)90206-0 ↗
59. N.R. Moody, S.L. Robinson, and W.M. Garrison: in Metallography of Advanced Materials: Proceedings of the Twentieth Annual Technical Meeting of the International Metallographic Society, 1987, Monterey CA, H.J. Cialone, M.E. Blum, G.W.E. Johnson, and G.F. VanderVoort, eds., ASM, Metals Park, OH, 1988, pp. 177–92
60. B.C. Odegard, S.L. Robinson, and N.R. Moody: in Hydrogen Effects in Materials: Proceedings of the Fifth International Conference on the Effect of Hydrogen on the Behavior of Materials, 1994, Moran WY, A.W. Thompson and N.R. Moody, eds., TMS, Warrendale, PA, 1996, pp. 591–9810.1002/9781118803363.ch51 ↗
61. R.E. Stoltz, J.B. VanderSande: Metall. Trans. A, 1980, vol. 11A, pp. 1033–3710.1007/BF02654717 ↗
62. A.W. Thompson, I.M. Bernstein: Advances in Corrosion Science and Technology, Volume 7, Plenum Publishing Corporation, New York, NY, 1980, pp. 53–17510.1007/978-1-4615-9065-1_2 ↗
63. R.E. Schramm, R.P. Reed: Metall. Trans. A, 1975, vol. 6A, pp. 1345–5110.1007/BF02641927 ↗
64. C.G. Rhodes, A.W. Thompson: Metall. Trans. A, 1977, vol. 8A, pp. 1901–0510.1007/BF02646563 ↗
65. W. Reick, M. Pohl, A.F. Padilha: Steel Res., 1996, vol. 67, pp. 253–5610.1002/srin.199605486 ↗
66. G. Han, J. He, S. Fukuyama, K. Yokogawa: Acta Mater., 1998, vol. 46, pp. 4559–7010.1016/S1359-6454(98)00136-0 ↗
67. A.W. Loginow, E.H. Phelps: Corrosion, 1975, vol. 31, pp. 404–1210.5006/0010-9312-31.11.404 ↗