journal article·2013-01Open access

Influence of Gas Atmosphere Dew Point on the Selective Oxidation and the Reactive Wetting During Hot Dip Galvanizing of CMnSi TRIP Steel

Lawrence Cho, Seok Jae Lee, Myung Soo Kim, Young Ha Kim, Bruno C. De Cooman

Abstract

The selective oxidation and reactive wetting of intercritically annealed Si-bearing CMnSi transformation-induced plasticity steels were investigated by high-resolution transmission electron microscopy. In a N2 + 10 pct H2 gas atmosphere with a dew point (DP) ranging from 213 K to 278 K (−60 °C to 5 °C), a continuous layer of selective oxides was formed on the surface. Annealing in a higher DP gas atmosphere resulted in a thinner layer of external oxidation and a greater depth of internal oxidation. The hot dipping was carried out in a Zn bath containing 0.22 mass pct Al, and the bath temperature was 733 K (460 °C). Coarse and discontinuous Fe2Al5−x Zn x grains and Fe-Zn intermetallics (ζ and δ) were observed at the steel/coating interface after the hot dip galvanizing (HDG) of panels were annealed in a low DP atmosphere 213 K (−60 °C). The Fe-Zn intermetallics were formed both in areas where the Fe2Al5−x Zn x inhibition layer had not been formed and on top of non-stoichiometric Fe-Al-Zn crystals. Poor wetting was observed on panels annealed in a low DP atmosphere because of the formation of thick film-type oxides on the surface. After annealing in higher DP gas atmospheres, i.e., 263 K and 278 K (−10 °C and 5 °C), a continuous and fine-grained Fe2Al5−x Zn x layer was formed. No Fe-Zn intermetallics were formed. The small grain size of the inhibition layer was attributed to the nucleation of the Fe2Al5−x Zn x grains on small ferrite sub-surface grains and the presence of granular surface oxides. A high DP atmosphere can therefore significantly contribute to the decrease of Zn-coating defects on CMnSi TRIP steels processed in HDG lines.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. A.R. Marder: Prog. Mater. Sci., 2000, vol. 45, pp. 191–271.10.1016/S0079-6425(98)00006-1 ↗
2. B. Mintz: Int. Mater. Rev, 2001, vol. 46, pp. 169–97.10.1179/095066001771048754 ↗
3. L. Chen, H.S. Kim, S.K. Kim, and B.C. De Cooman: ISIJ Int., 2007, vol. 47, pp. 1804–12.10.2355/isijinternational.47.1804 ↗
4. J. Mahieu, S. Claessens, and B.C. De Cooman: Metall. Mater. Trans. A, 2001, vol. 32A, pp. 2905–08.10.1007/s11661-001-1042-5 ↗
5. X.V. Eynde, J.P. Servais, and M. Lamberigts: Surf. Interface Anal., 2003, vol. 35, pp. 1004–14.10.1002/sia.1639 ↗
6. J. Mahieu, S. Claessens, B.C. De Cooman, and F. Goodwin: The 6th International Conference on Zinc and Zinc Alloy Coated Steel Sheet (GALVATECH 2004), Chicago, IL, Association for Iron and Steel Technology, 2004, pp. 529–38.
7. Y.F. Gong, H.S. Kim, and B.C. De Cooman: ISIJ Int., 2008, vol. 48, pp. 1745–51.10.2355/isijinternational.48.1745 ↗
8. Y.F. Gong, H.S. Kim, and B.C. De Cooman: ISIJ Int., 2009, vol. 49, pp. 557–63.10.2355/isijinternational.49.557 ↗
9. L. Cho, M.S. Kim, Y.H. Kim, S.J. Lee, and B.C. De Cooman: Proceedings of the 8th International Conference on Zinc and Zinc Alloy Coated Steel Sheet (GALVATECH 2011), Genova, Italy, Associazione Italiana di Metallurgia, Milan, 2011, pp. 145–52.
10. X.S. Li, S.I. Baek, C.S. Oh, S.J. Kim, and Y.W. Kim: Scripta Mater., 2007, vol. 57, pp. 113–16.10.1016/j.scriptamat.2007.03.040 ↗
11. Y.I. Choi, W.J. Beom, C.J. Park, D. Paik, and M.H. Hong: Metall. Mater. Trans. A, 2010, vol. 41A, pp. 3379–85.10.1007/s11661-010-0427-8 ↗
12. R. Sanguanmoo, E. Nisaratanaporn, and Y. Boonyongmaneerat: Corros. Sci., 2011, vol. 53, pp. 122–26.10.1016/j.corsci.2010.09.031 ↗
13. T. Matsumoto: CAMP-ISIJ, 1991, vol. 4, p. 1632.
14. R. Nakanishi, H. Irie, M. Nakamura, K. Okamoto, and M. Shimizu: European Patent, 2007. EP 1829 983 (A1).
15. L. Bordignon, X.V. Eynde, and R. Franssen: Revue de Métallurgie, 2004, vol. 101, pp. 559–68.10.1051/metal:2004124 ↗
16. M. Blumenau, M. Norden, F. Friedel, and K. Peters: Surf. Coat. Technol., 2011, vol. 206, pp. 559–67.10.1016/j.surfcoat.2011.07.088 ↗
17. Y.F. Gong and B.C. De Cooman: ISIJ Int., 2011, vol. 51, pp. 630–37.10.2355/isijinternational.51.630 ↗
18. D. Huin, P. Flauder, and J.B. Leblond: Oxid. Met., 2005, vol. 64, pp. 131–67.10.1007/s11085-005-5718-x ↗
19. K.K. Wang, L. Chang, D. Gan, and H.P. Wang: Thin Solid Films, 2010, vol. 518, pp. 1935–42.10.1016/j.tsf.2009.07.154 ↗
20. E.M. Bellhouse and J.R. McDermid: Metall. Mater. Trans. A, 2010, vol. 41A, pp. 1539–53.10.1007/s11661-010-0192-8 ↗
21. C. Wagner: Zeitschrift für Elektrochemie, Berichte der Bunsengesellschaft für physikalische Chemie, 1959, vol. 63, pp. 772–82.
22. H.J. Grabke, V. Leroy, and H. Viefhaus: ISIJ Int., 1995, vol. 35, pp. 95–113.10.2355/isijinternational.35.95 ↗
23. Y.D. He, J. Ma, Z.W. Li, and W. Gao: Mater. Sci. Forum, 2006, vol. 522, pp. 45–52.10.4028/www.scientific.net/MSF.522-523.45 ↗
24. Y. Kim, M. Shin, C. Tang, and J. Lee: Metall. Mater. Trans. B, 2010, vol. 41B, pp. 872–75.10.1007/s11663-010-9366-4 ↗
25. R. Khondker, A. Mertens, and J.R. McDermid: Mater. Sci. Eng. A, 2007, vol. 463, pp. 157–65.10.1016/j.msea.2006.09.116 ↗
26. Y.F. Gong, T.J. Song, H.S. Kim, J.H. Kwak, and B.C. De Cooman: Proceedings of the Asia Pacific Galvanizing Conference, Jeju, Korea, The Corrosion Science Society of Korea, 2009, paper no. B-15.
27. R. Kavitha and J.R. McDermid: Proceedings of the 8th International Conference on Zinc and Zinc Alloy Coated Steel Sheet (GALVATECH 2011), Genova, Italy, Associazione Italiana di Metallurgia, Milan, 2011, pp. 1243–53.
28. N. Gao, D.Y.H. Liu, N. Tang, R.B. Park, and M.S. Kim: Proceedings of the 8th International Conference on Zinc and Zinc Alloy Coated Steel Sheet (GALVATECH 2011), Genova, Italy, Associazione Italiana di Metallurgia, Milan, 2011, pp. 123–30.