journal article·2011-12

Crack Propagation During Sustained-Load Cracking of Al-Zn-Mg-Cu Aluminum Alloys Exposed to Moist Air or Distilled Water

N. J. Henry Holroyd, G. M. Scamans

Publisher page

Abstract

Intergranular sustained-load cracking of Al-Zn-Mg-Cu (AA7xxx series) aluminum alloys exposed to moist air or distilled water at temperatures in the range 283 K to 353 K (10 °C to 80 °C) has been reviewed in detail, paying particular attention to local processes occurring in the crack-tip region during crack propagation. Distinct crack-arrest markings formed on intergranular fracture faces generated under fixed-displacement loading conditions are not generated under monotonic rising-load conditions, but can form under cyclic-loading conditions if loading frequencies are sufficiently low. The observed crack-arrest markings are insensitive to applied stress intensity factor, alloy copper content and temper, but are temperature sensitive, increasing from ~150 nm at room temperature to ~400 nm at 313 K (40 °C). A re-evaluation of published data reveals the apparent activation energy, E a for crack propagation in Al-Zn-Mg(-Cu) alloys is consistently ~35 kJ/mol for temperatures above ~313 K (40 °C), independent of copper content or the applied stress intensity factor, unless the alloy contains a significant volume fraction of S-phase, Al2CuMg where E a is ~80 kJ/mol. For temperatures below ~313 K (40 °C) E a is independent of copper content for stress intensity factors below ~14 MNm−3/2, with a value ~80 kJ/mol but is sensitive to copper content for stress intensity factors above ~14 MNm−3/2, with E a , ranging from ~35 kJ/mol for copper-free alloys to ~80 kJ/mol for alloys containing 1.5 pct Cu. The apparent activation energy for intergranular sustained-load crack initiation is consistently ~110 kJ/mol for both notched and un-notched samples. Mechanistic implications are discussed and processes controlling crack growth, as a function of temperature, alloy copper content, and loading conditions are proposed that are consistent with the calculated apparent activation energies and known characteristics of intergranular sustained-load cracking. It is suggested, depending on the circumstances, that intergranular crack propagation in humid air and distilled water can be enhanced by the generation of aluminum hydride, AlH3, ahead of a propagating crack and/or its decomposition after formation within the confines of the nanoscale volumes available after increments of crack growth, defined by the crack arrest markings on intergranular fracture surfaces.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. M.O. Speidel: Metall. Trans. A, 1975, vol. 6A, pp. 631–51.10.1007/BF02672284 ↗
2. M.O. Speidel: in The Theory of Stress Corrosion Cracking in Alloys, J.C. Scully, ed., NATO, Brussels, Belgium, 1971, pp. 289–344.
3. N. Behnood, H. Cai, J.T. Evans, and N.J.H. Holroyd: Mater. Sci. Eng., 1989, vol. A119, pp. 23–32.10.1016/0921-5093(89)90520-0 ↗
4. G.A. Young and J.R. Scully: Metall. Mater. Trans. A, 2002, vol. 33A, pp. 101–15.10.1007/s11661-002-0009-5 ↗
5. S. Knight: Ph.D. Thesis, Monash University, Melbourne, 2008.
6. W. Thomson (Lord Kelvin): Philos. Mag., 1871, vol. 42, pp. 443–52.
7. R.H. Dean and J.W. Hutchinson: Fracture Mechanics: Twelfth Conf., ASTM STP-700, ASTM, Philadelphia, PA, 1980, pp. 383–405.10.1520/STP36982S ↗
8. K. Komai, K. Minoshima, and T. Miyawaki: J. Phys. IV, Coll. C6, suppl. J. Phys. III, 1996, vol. 6, pp. 413–20.
9. D.L. Davidson and J. Lankford: Fat. Eng. Struct., 1983, vol. 6 (3), pp. 241–56.10.1111/j.1460-2695.1983.tb00340.x ↗
10. M. Ciccotti, M. George, V. Ranieri, L. Wondraczek, and C. Marliere: J. Non-Cryst. Solids, 2008, vol. 354, pp. 564–68.10.1016/j.jnoncrysol.2007.06.090 ↗
11. A. Grimaldi, M. George, G. Pallares, C. Marliere, and M. Ciccotti: Physical Review Letters, Apr. 25, 2008, PRL 100, 165505, The American Physical Society, College Park, MD.10.1103/PhysRevLett.100.165505 ↗
12. H.A. Al-Abadleh and V.H. Grassian: Langmuir, 2003, vol. 19, pp. 341–47.10.1021/la026208a ↗
13. K.C. Hass, W.F. Schneider, A. Curioni, and W. Andreoni: Science, 1998, vol. 282, pp. 265–68.10.1126/science.282.5387.265 ↗
14. R.P. Wei: in Hydrogen Effects in Metals, I.M. Bernstein and A.W. Thompson, eds., AIME, Warrendale, PA, 1981, pp. 677–89.
15. M. Watanabe: J. Phys. Chem. Solids, 2010, vol. 71, pp. 1251–58.10.1016/j.jpcs.2010.05.002 ↗
16. M. Watanabe, X. Jiang, and R. Saito: U.S. Patent 7,235,226, June 26, 2007.
17. S.W. Ciaraldi, J.L. Nelson, R.A. Yeske, and E.N. Pugh: in Hydrogen Effects in Metals, I.M. Bernstein and A.W. Thompson, eds., AIME, Warrendale, PA, 1981, pp. 437–47.
18. M.V. Hyatt: Corrosion, 1970, vol. 26, pp. 487–503.10.5006/0010-9312-26.11.487 ↗
19. R. Hermann and N.J.H. Holroyd: Mater. Sci. Technol., 1986, vol. 2, pp. 1238–44.10.1179/mst.1986.2.12.1238 ↗
20. S.P. Lynch: Acta Metall., 1988, vol. 36, pp. 2639–61.10.1016/0001-6160(88)90113-7 ↗
21. M.O. Speidel and M.V. Hyatt: Advanced Corrosion Science Technology, 1972, vol. 2, Plenum Press, New York, NY, pp. 115–335.10.1007/978-1-4615-8255-7_3 ↗
22. S. Pyun, M. Hong, and H. Kim: Br. Corros. J., 1991, vol. 26, pp. 260–6410.1179/000705991798269053 ↗
23. G.M. Scamans: Aluminium, 1982, vol. 58, pp. 332–34.
24. R.G. Song, M.K. Tseng, B.J. Zhang, J. Lui, Z.H. Jin, and K.S. Shin: Acta Mater., 1996, vol. 44 (8), pp. 3241–48.10.1016/1359-6454(95)00406-8 ↗
25. R.G. Song, W. Dietzel, B.J. Zhang, W.J. Liu, M.K. Tseng, and A. Atrens: Acta Mater., 2004, vol. 52, pp. 4727–43.10.1016/j.actamat.2004.06.023 ↗
26. G.M. Scamans, N.J.H. Holroyd, and C.D.S. Tuck: Corros. Sci., 1987, vol. 27, pp. 329–47.10.1016/0010-938X(87)90076-X ↗
27. S. Bovard: Master’s Thesis, University of Pittsburgh, Pittsburgh, PA, 2005.
28. A.H. Lee and R.T. Foley: Corrosion, 1984, vol. 40 (4), pp. 195–97.10.5006/1.3581939 ↗
29. P. Martin, J.I. Dickson, and J.P. Bailon: Mater. Sci. Eng., 1985, vol. 69, pp. L9–L13.10.1016/0025-5416(85)90402-1 ↗
30. J. McEvily, J.B. Clark, and A.P. Bond: Trans. ASM, 1967, vol. 60, pp. 661–71.
31. G.M. Scamans: Scripta Metall., 1979, vol. 13, pp. 245–50.10.1016/0036-9748(79)90305-3 ↗
32. G.M. Scamans: in Hydrogen Effects in Metals, I.M. Bernstein and A.W. Thompson, eds., AIME, Warrendale, PA, 1981, pp. 467–75.
33. G.M. Scamans: Metall. Trans. A, 1980, vol. 11A, pp. 846–50.10.1007/BF02661215 ↗
34. R. Hermann: Corrosion, 1988, vol. 44, pp. 685–90.10.5006/1.3584929 ↗
35. R.C. Dorward and K.R. Hasse: Final NASA Report Contract No. NAS8-30890, Oct. 1976.
36. N.J.H. Holroyd, G.M. Scamans, and R. Hermann: in Embrittlement by the Localized Environment , R.P. Gangloff, ed., AIME, Warrendale, PA, 1984, pp. 327–47.
37. Wu-Yang Chu, Y.B. Wang, and C.M. Hsiao: Corrosion, 1982, vol. 38, pp. 561–70.10.5006/1.3577303 ↗
38. M.S. Domack: in Corrosion Cracking, V.S. Groel, ed., ASM, Metals Park, OH, 1986, pp. 191–96.
39. A.H. Le, B.F. Brown, and R.T. Foley: Corrosion, 1980, vol. 36, pp. 673–79.10.5006/0010-9312-36.12.673 ↗
40. C.J. Newton and N.J.H. Holroyd: in New Methods for Corrosion Testing Aluminum Alloys, ASTM-STP 1134, V.S. Agarwala and G.M. Ugiansky, eds., 1992, pp. 153–79.10.1520/STP19588S ↗
41. C.A. Loto and R.A. Cottis: Corrosion, 1989, vol. 45, pp. 136–41.10.5006/1.3577831 ↗
42. M.S. Domack: in Environmentally Assisted Cracking: Science and Engineering, ASTM-STP 1049, W.B. Lisagor, T.W. Crooker, and B.N. Leis, ASTM, Philadelphia, PA, 1990, pp. 391–409.
43. K. Welpmann, A. Gysler, and G. Lutjering: Z. Metallkd., 1980, vol. 71, pp. 7–14.
44. N.J.H. Holroyd and D. Hardie: in Hydrogen Effects in Metals, I.M. Bernstein and A.W. Thompson, eds., AIME, Warrendale, PA, 1980, pp. 449–57.
45. N.J.H. Holroyd and D. Hardie: Corros. Sci., 1981, vol. 21, pp. 129-44.10.1016/0010-938X(81)90097-4 ↗
46. G.M. Scamans, R. Alani, and P.R. Swann: Corros. Sci., 1976, vol. 16, pp. 443–59.10.1016/0010-938X(76)90065-2 ↗
47. D. Hardie, N.J.H. Holroyd, and R.N. Parkins: Met. Sci., 1979, vol. 13, pp. 603–10.10.1179/msc.1979.13.11.603 ↗
48. M. Abe, K Ouchi, K Asano, and A. Fujiwara: J. Jpn. Inst. Met., 1981, vol. 45, pp. 1161–69.10.2320/jinstmet1952.45.11_1161 ↗
49. R.S. Pathania and D. Tromans: Metall. Trans. A, 1981, vol. 12A, pp. 607–12.10.1007/BF02649735 ↗
50. M.O. Speidel: in Hydrogen in Metals, A.W. Thompson, ed., ASM, Metals Park, OH, 1974, pp. 249–76.
51. S. Lee, S. Pyun, and Y. Chun: Metall. Trans. A, 1991, vol. 22A, pp. 2407–14.10.1007/BF02665007 ↗
52. H. Vogt and M.O. Speidel: Corros. Sci., 1998, vol. 40, pp. 251–70.10.1016/S0010-938X(97)00132-7 ↗
53. H.F. de Jong: Aluminium, 1981, vol. 58, pp. 526–31.
54. D.G. Anltenpohl: Corrosion, 1962, vol. 18, pp. 143–53.10.5006/0010-9312-18.4.143 ↗
55. R. Rungta, R.R. Ahrens, and M. Zu: U.S. Patent 5,601,663, Feb. 11, 1997.
56. N.J.H. Holroyd: in Environmental Effects on Engineered Materials, Russell H. Jones, ed., Marcel Dekker, Inc., New York, NY, 2000, pp. 173–251.
57. R.S. Alwitt: J. Electrochem. Soc., 1974, vol. 121, pp. 1322–28.10.1149/1.2401679 ↗
58. G. Kostikos, J.M. Sutcliffe, and N.J.H. Holroyd: Br. Corros. J., 1995, vol. 30, pp. 302–08.10.1179/bcj.1995.30.4.302 ↗
59. N.J.H. Holroyd and D. Hardie: Corros. Sci., 1983, vol. 23, pp. 527–46.10.1016/0010-938X(83)90117-8 ↗
60. R. Guest and A.R. Troiano: in L’Hydrogene dans les Metaux, Editions Science et Industrie, Paris, France, 1972, pp. 427–32.
61. R.E. Ricker and D.J. Duquette: Metall. Trans. A, 1988, vol. 19A, pp. 1775–83.10.1007/BF02645146 ↗
62. K.R. Cooper, L.M. Young, R.P. Gangloff, and R.G. Kelly: Mater. Sci. Forum, 2000, vols. 331–337, pp. 1625–34.10.4028/www.scientific.net/MSF.331-337.1625 ↗
63. J.W. Hutchinson: Int. J. Sol. Struct., 2000, vol. 37, pp. 225–38.10.1016/S0020-7683(99)00090-6 ↗
64. L.M. Young and R.P. Gangloff: in Advances in Metallurgy of Aluminum Alloys, Murat Tiryakioglu, ed., ASM International, Metals Park, OH, 2001, pp. 135–40.
65. F.P. Ford: Corrosion, 1979, vol. 35, pp. 281–89.10.5006/0010-9312-35.7.281 ↗
66. N. Lampeas and P.G. Koutoukos: Corros. Sci., 1994, vol. 36, pp. 1011–25.10.1016/0010-938X(94)90200-3 ↗
67. M. Metikos-Hukovic, R. Babic, Z. Grubac, and S. Brinic: J. Appl. Chem., 1994, vol. 24, pp. 325–31.
68. M. Metikos-Hukovic, R. Babic, and Z. Grubac: J. Appl. Chem., 1998, vol. 28, pp. 433–39.
69. Y.A. Aleksandrov, E.I. Tsyganova, and A.L. Pisarev: Russ. J. Gen. Chem., 2003, vol. 73 (5), pp. 729–34.10.1023/A:1026114331597 ↗
70. A.Z. Zhuk, A.E. Sheindlin, B.V. Kleymenov, E.I. Shkolnikov, and M.Y. Lopatin: J. Power Sources, 2006, vol. 157, pp. 921–26.10.1016/j.jpowsour.2005.11.097 ↗
71. T. Hiraki, M. Takeuchi, M. Hisa, and T. Akiyama: Mater. Trans., 2005, vol. 46 (5), pp. 1052–57.10.2320/matertrans.46.1052 ↗
72. L.C. Rowe and M.S. Walker: Corrosion, 1961, vol. 17, pp. 353t–356t.10.5006/0010-9312-17.7.105 ↗
73. B. Bavarian, L. Reiner, H. Youssefpour, and I. Juraga: in Corrosion, NACE, Houston, TX, 2005.
74. T. Ishikawa and R.B. McLellan: Acta Metall., 1986, vol. 34, pp. 1091–95.10.1016/0001-6160(86)90219-1 ↗
75. G.A. Young and J.R. Scully: Acta Mater., 1998, vol. 18, pp. 6337–49.10.1016/S1359-6454(98)00333-4 ↗
76. J.R. Scully, G.A. Young, and S.W. Smith: Mater. Sci. Forum, 2000, vols. 331–337, pp. 1583–1600.10.4028/www.scientific.net/MSF.331-337.1583 ↗
77. O.D. Sherby, J.L. Lytonn, and J.E. Dorn: Acta Metall., 1957, vol. 5, pp. 219–27.10.1016/0001-6160(57)90169-4 ↗
78. A.L. Goodman, E.T. Barnard, and V.H. Grassian: J. Phys. Chem. A, 2001, vol. 105, pp. 6443–75.10.1021/jp003722l ↗
79. J.P. Nordin, D.J. Sullivan, B.L. Phillips, and W.H. Casey: Inorg. Chem., 1998, vol. 37, pp. 4760–63.10.1021/ic980333l ↗
80. D.J. Sullivan, J.P. Nordin, B.L. Phillips, and W.H. Casey: Geochimica Cosmochimica Acta, 1999, vol. 63, pp. 1471–80.10.1016/S0016-7037(99)00113-1 ↗
81. N.J.H. Holroyd: in Environment-Induced Cracking of Metals, R.P. Gangloff and M.B. Ives, eds., NACE, Houston, TX, 1990, pp. 311–45.
82. T. Magnin, A. Chambreuil, and B. Bayle: Acta Mater., 1996, vol. 44, pp. 1457–70.10.1016/1359-6454(95)00301-0 ↗
83. J.J. Lewandowski, V. Kohler, and N.J.H. Holroyd: Mater. Sci. Eng., 1978, vol. 96, pp. 185–95.10.1016/0025-5416(87)90552-0 ↗
84. P. Singh, J.T. Evans, and N.J.H. Holroyd: Mater. Sci. Eng., 1992, vol. A157, pp. 1–8.10.1016/0921-5093(92)90091-E ↗
85. V. Rosenband and A. Gany: Int. J. Hydrogen Energy, 2010, vol. 35, pp. 10898–10904.10.1016/j.ijhydene.2010.07.019 ↗
86. E. Czech and T. Troczynski: Int. J. Hydrogen Energy, 2010, vol. 35, pp. 1029–37.10.1016/j.ijhydene.2009.11.085 ↗
87. R.G. Buchheit, L.P. Montes, M.A. Martinez, J. Michael, and P.F. Hlava: J. Electrochem. Soc., 1999, vol. 146, pp. 4424–28.10.1149/1.1392654 ↗
88. R.G. Buchheit, M.A. Martinez, and L.P. Montes: J. Electrochem. Soc., 2000, vol. 147, pp. 119–24.10.1149/1.1393164 ↗
89. F.C. Porter and S.E. Hadden: J. Appl. Chem., 1953, vol. 3, pp. 385–409.10.1002/jctb.5010030809 ↗
90. H.P. Goddard: in Corrosion of Light Metals, John Wiley, New York, 1967, pp. 65–67.
91. R.S. Allwitt: in Oxide and Oxide Films, J.W. Diggle, ed., Marcel Decker, New York, NY, 1976, pp. 169–254.
92. R.S. Allwitt and L.C. Archibald: Corros. Sci., 1973, vol. 13, pp. 687–88.10.1016/S0010-938X(73)80039-3 ↗
93. G.M. Scamans and A.S. Rehal: J. Mater. Sci., 1979, vol. 14, pp. 2459–70.10.1007/BF00737037 ↗
94. W. Vedder and D.A. Vermilyea: Trans. Faraday Soc., 1969, vol. 65, pp. 561–84.10.1039/tf9696500561 ↗
95. R.K. Hart: Trans. Faraday Soc., 1957, vol. 53, pp. 1020–27.10.1039/tf9575301020 ↗
96. L. Lepin and V. Kadek: Corros. Sci., 1966, vol. 6, pp. 177–81.10.1016/S0010-938X(66)80007-0 ↗
97. R.S. Alwitt and W.J. Barnard: J. Electrochem. Soc., 1974, vol. 121, pp. 1019–21.10.1149/1.2401970 ↗
98. T.H. Sanders and E.A. Starke: Metall. Trans. A, 1976, vol. 7A, pp. 1407–18.10.1007/BF02658827 ↗
99. E.A. Starke: Mater. Sci. Eng., 1977, vol. 29, pp. 99–115.10.1016/0025-5416(77)90114-8 ↗
100. F.S. Lin and E.A. Starke: Mater. Sci. Eng., 1979, vol. 39, pp. 27–41.10.1016/0025-5416(79)90167-8 ↗