journal article·2002-06

Tensile and fatigue properties of 17-4 PH stainless steel at high temperatures

Jui-Hung Wu, Chih-Kuang Lin

Publisher page

Abstract

The tensile and high-cycle fatigue properties for 17-4 PH* stainless steels in three different conditions were investigated at temperatures ranging from room temperature to 400 °C. Results indicated that the yield strength and fatigue strength for the three conditions at a given temperature took the following order: condition H900 > condition A> condition H1150. The yield strength of each condition decreased with increasing temperature except for condition A, which was tested at 400 °C with longer hold times, where a precipitation-hardening effect took place. The S-N curves showed that the fatigue strengths of each condition in the short-life regime were decreased with an increase in temperature. In the long-life regime, the fatigue strengths of condition A at 400 °C were greater than those at lower temperatures as a result of an in-situ precipitation-hardening effect. The fatigue strengths of condition H900 in the long life regime at 300 °C were superior to those at lower temperatures, due to the mechanisms of surface oxidation and thermal activation of dislocations. Fractography observations indicated that a shift of fatigue fracture from surface to internal crack initiation occurred at higher temperatures (300 °C and 400 °C) with long fatigue lives.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Temperature Alloys and Creep · Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. W.F. Smith: Structure and Properties of Engineering Alloys, 2nd ed., McGraw-Hill, Inc., New York, NY, 1993.
2. U.K. Viswanathan, S. Banerjee, and R. Krishnan: Mater. Sci. Eng., 1988, vol. A104, pp. 181–89.10.1016/0025-5416(88)90420-X ↗
3. H.J. Rack and D. Kalish: Metall. Trans., 1974, vol. 5, pp. 1595–1605.10.1007/BF02646331 ↗
4. C.-K. Lin and W.-J. Tsai: Fatigue Fract. Eng. Mater. Struct., 2000, vol. 23, pp. 489–97.10.1046/j.1460-2695.2000.00313.x ↗
5. F.B. Pickering: Int. Met. Rev., 1976, vol. 21, pp. 227–68.
6. R.D.K. Misra, G.Y. Prasad, T.V. Balasubramanian, and P.R. Rao: Scripta Metall., 1986, vol. 20, pp. 713–16.10.1016/0036-9748(86)90497-7 ↗
7. R.D.K. Misra, G.Y. Prasad, T.V. Balasubramanian, and P.R. Rao: Scripta Metall., 1987, vol. 21, pp. 1067–70.10.1016/0036-9748(87)90251-1 ↗
8. K.C. Antony: J. Met., 1963, vol. 15, pp. 922–27.
9. U.K. Viswanathan, P.K.K. Nayar, and R. Krishnan: Mater. Sci. Technol., 1989, vol. 5, pp. 346–49.10.1179/mst.1989.5.4.346 ↗
10. X. Zang: Trans. Met. Heat Treatment, 1991, vol. 12, pp. 23–29 (in Chinese).
11. G. Huang: Iron and Steel, 1998, vol. 33, pp. 44–46 (in Chinese).
12. F.J. Heymann, V.P. Swaminathan, and J.W. Cunningham: Report No. CS-1967, Electrical Power Research Institute, Palo Alto, CA, 1981.
13. B.C. Syrett, R. Viswanathan, S.S. Wing, and J.E. Wittig: Corrosion, 1982, vol. 38, pp. 273–82.10.5006/1.3577350 ↗
14. M. Murayama, Y. Katayama, and K. Hono: Metall. Mater. Trans. A, 1999, vol. 30A, pp. 345–53.10.1007/s11661-999-0323-2 ↗
15. T. Isomoto and N.S. Stoloff: Mater. Sci. Eng., 1990, vol. A124, pp. 171–81.10.1016/0921-5093(90)90147-U ↗
16. J. Botella, C. Merino, and E. Otero: Oxid. Met., 1998, vol. 49, pp. 297–324.10.1023/A:1018830424480 ↗
17. G.R. Leverant and M. Gell: Metall. Trans. A, 1975, vol. 6A, pp. 367–71.10.1007/BF02667291 ↗
18. D.J. Duquette and M. Gell: Metall. Trans., 1972, vol. 3, pp. 1899–1905.10.1007/BF02642576 ↗
19. J.A. Bannantine, J.J. Comer, and J.L. Handrock: Fundamentals of Metal Fatigue Analysis, Prentice-Hall, Inc., Englewood Cliffs, NJ, 1990.