Influence of Weld Cooling Rate on Microstructure and Mechanical Properties of Alloy 718 Weldments
Source abstract
Abstract
Even though alloy 718 is the best for welding among all nickel-base superalloys, the formation of the Laves phase in welds is a major concern. The presence of this phase drastically degrades mechanical properties of the welds. To study the influence of weld cooling rate on microstructure and mechanical properties of alloy 718 weldments, two distinct welding processes were adopted—gas tungsten arc (GTA) and electron beam (EB) welding. The EB welding resulted in finer and relatively discrete Laves phase in lower quantity due to higher cooling rates prevailing in this process. On the other hand, due to lower cooling rates, GTA weld fusion zones exhibited coarse Laves with higher niobium. Depletion of the primary strengthening element niobium in the surrounding regions of Laves promoted crack propagation. Because EB welds had finer and lower amount of Laves, EB weldments exhibited superior mechanical properties compared with GTA weldments.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Temperature Alloys and Creep · Welding Techniques and Residual Stresses · Additive Manufacturing Materials and Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. D.D. Krueger: Proc. Conf. Superalloy 718—Metallurgy and Applications, E.A. Loria, ed., TMS, Warrendale, PA, 1989, pp. 279–9610.7449/1989/Superalloys_1989_279_296 ↗
2. G.A. Knorovsky, M.J. Cieslak, T.J. Headley, A.D. Romig, Jr. W.F. Hammetter: Metall. Trans. A, 1989, vol. 20A, pp. 2149–5810.1007/BF02650300 ↗
3. J. Gordine: Weld. J., 1971, vol. 50, pp. 480s–484s
4. W.J. Mills: Weld. J., 1984, vol. 63, pp. 237s–245s
5. A. Lingenfelter: Proc. Conf. Superalloy 718—Metallurgy and Applications, E.A. Loria, ed., TMS, Warrendale, PA, 1989, pp. 673–8310.7449/1989/Superalloys_1989_673_683 ↗
6. G.R. Evers, H.H. Smith, D.J. Michel: Metallography, 1978, vol. 11, pp. 441–5710.1016/0026-0800(72)90069-9 ↗
7. G.D. Janaki Ram: Ph.D. Thesis, Indian Institute of Technology Madras, Chennai, India, 2004
8. S.A. David, J.M. Vitek: Int. Mater. Rev., 1989, vol. 34, pp. 213–4510.1179/imr.1989.34.1.213 ↗
9. C. Radhakrishna, K. Prasad Rao: J. Mater. Sci., 1997, vol. 32, pp. 1–810.1023/A:1018541915113 ↗
10. S. Kou, Y. Le: Weld. J., 1986, vol. 65, pp. 305s–13s
11. K. Sivaprasad, S. Ganesh Sundara Raman: Mater. Sci. Eng. A, 2007, vol. 448, pp. 120–2710.1016/j.msea.2006.10.048 ↗
12. K. Sivaprasad, S. Ganesh Sundara Raman, C.V. Srinivasa Murthy, G. Madhusudhan Reddy: Sci. Technol. Weld. Join., 2006, vol. 11, pp. 127–3410.1179/174329306X84337 ↗
13. H. Tada, P.C. Paris, G.R. Irwin: The Stress Analysis of Cracks Handbook, 3rd ed., Professional Engineering Publishing, London, 2000.10.1115/1.801535 ↗
14. J.F. Radavich: J. Met., 1988, vol. 40, pp. 42–43
15. G.D. Janaki Ram, A. Venugopal Reddy, K. Prasad Rao, G. Madhusudhan Reddy: Sci. Technol. Weld. Join., 2004, vol. 9, pp. 390–9810.1179/136217104225021788 ↗
16. L.A. James, W.J. Mills: Eng. Fract. Mech., 1985, vol. 22, pp. 797–81710.1016/0013-7944(85)90109-2 ↗
17. J.J. Schirra, R.H. Caless, and R.W. Hatala: Proc. Conf. Superalloys 718, 625, and Various Derivatives, E.A. Loria, ed., TMS, Warrendale, PA, 1991, pp. 375–8810.7449/1991/Superalloys_1991_375_388 ↗
18. L. Xiao, D.L. Chen, M.C. Chaturvedi: Mater. Sci. Eng. A, 2006, vol. 428, pp. 1–1110.1016/j.msea.2005.08.206 ↗
19. R.B. Scarlin: Metall. Trans. A, 1976, vol. 7A, pp. 1535–4110.1007/BF02656396 ↗
20. D.L. Chen, M.C. Chaturvedi: Metall. Mater. Trans. A, 2000, vol. 31A, pp. 1531–4110.1007/s11661-000-0164-5 ↗