Creep Behavior and Degradation of Subgrain Structures Pinned by Nanoscale Precipitates in Strength-Enhanced 5 to 12 Pct Cr Ferritic Steels
Source abstract
Abstract
Creep behavior and degradation of subgrain structures and precipitates of Gr. 122 type xCr-2W-0.4Mo-1Cu-VNb (x = 5, 7, 9, 10.5, and 12 pct) steels were evaluated during short-term and long-term static aging and creep with regard to the Cr content of steel. Creep rupture life increased from 5 to 12 pct Cr in the short-term creep region, whereas in the long-term creep region, it increased up to 9 pct Cr and then decreased with the addition of Cr from 9 to 12 pct. Behavior of creep rupture life was attributed to the size of elongated subgrains. In the short-term creep region, subgrain size decreased from 5 to 12 pct Cr, corresponding to the longer creep strength. However, in the long-term creep region after 104 hours, subgrain size increased up to 9 pct Cr and then decreased from 9 to 12 pct, corresponding to the behavior of creep rupture life. M23C6 and MX precipitates had the highest number fraction among all of the precipitates present in the studied steels. Cr concentration dependence of spacing of M23C6 and MX precipitates exhibited a V-like shape during short-term as well as long-term aging at 923 K (650 °C), and the minimum spacing of precipitates belonged to 9 pct Cr steel, corresponding to the lowest recovery speed of subgrain structures. In the short-term creep region, subgrain coarsening during creep was controlled by strain and proceeded slower with the addition of Cr, whereas in long-term creep region, subgrain coarsening was controlled by the stability of precipitates rather than due to the creep plastic deformation and took place faster from 9 to 12 pct and 9 to 5 pct Cr. However, M23C6 precipitates played a more important role than MX precipitates in the control of subgrain coarsening, and there was a closer correlation between spacing of M23C6 precipitates and subgrain size during static aging and long-term creep region.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Temperature Alloys and Creep · Fatigue and fracture mechanics · Fire effects on concrete materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. A. Aghajani, C. Somsen, and G. Eggeler: Acta Mater., 2009, vol. 57, pp. 5093–5106.10.1016/j.actamat.2009.07.010 ↗
2. K. Maruyama, K. Sawada, and J. Koike: ISIJ Int., 2001, vol. 41, pp. 641–53.10.2355/isijinternational.41.641 ↗
3. F. Abe: Creep-Resistant Steels, Woodhead Publishing, Cambridge, United Kingdom, 2008, pp. 279–304.10.1533/9781845694012 ↗
4. R. Agamennone, W. Blum, C. Gupta, and J.K. Chakravartty: Acta Mater., 2006, vol. 54, pp. 3003–14.10.1016/j.actamat.2006.02.038 ↗
5. G. Eggeler: Acta Metall., 1989, vol. 37, pp. 3225–34.10.1016/0001-6160(89)90194-6 ↗
6. M. Yoshizawa and M. Igarashi: Int. J. Press. Vess. Pip., 2007, vol. 84, pp. 37–43.10.1016/j.ijpvp.2006.09.005 ↗
7. M. Igarashi and M. Yoshizawa: Proc. 4th Int. Conf. on Advances in Materials Technology in Fossil Power Plants, Hilton Head Island, South Carolina, ASM International, Materials Park, OH, 2004, pp. 1124–35.10.31399/asm.cp.am-epri-2004p1124 ↗
8. F. Abe: Sci. Technol. Adv. Mater., 2008, vol. 9, pp. 1–15.
9. F. Abe and S. Nakazawa: Mater. Sci. Technol., 1992, vol. 8, pp. 1063–69.10.1179/mst.1992.8.12.1063 ↗
10. H. Ghassemi Armaki, K. Maruyama, M. Yoshizawa, and M. Igarashi: Mater. Sci. Eng. A, 2008, vol. 490, pp. 66–71.10.1016/j.msea.2008.01.072 ↗
11. K. Maruyama, H. Ghassemi Armaki, and K. Yoshimi: Int. J. Press. Vess. Pip., 2007, vol. 84, pp. 171–76.10.1016/j.ijpvp.2006.09.015 ↗
12. J.S. Lee, H. Ghassemi Armaki, K. Maruyama, T. Muraki, and H. Asahi: Mater. Sci. Eng. A, 2006, vol. 428, pp. 270–75.10.1016/j.msea.2006.05.010 ↗
13. K. Maruyama, H. Ghassemi Armaki, R.P. Chen, K. Yoshimi, M. Yoshizawa, and M. Igarashi: Int. J. Press. Vess. Pip., 2010, vol. 87, pp. 276–81.10.1016/j.ijpvp.2010.03.012 ↗
14. H. Kushima, K. Kimura, and F. Abe: Tetsu-to-Hagané, 1999, vol. 85, pp. 841–47.10.2355/tetsutohagane1955.85.11_841 ↗
15. K. Kimura, H. Kushima, F. Abe, K. Suzuki, S. Kumai, and A. Satoh: Proc. 5th Int. Charles Parsons Turbine Conf., Cambridge, United Kingdom, 2000, pp. 590–602.
16. H. Ghassemi Armaki, R.P. Chen, K. Maruyama, and M. Igarashi: Mater. Sci. Eng. A, 2010, vol. 527, pp. 6581–88.10.1016/j.msea.2010.07.037 ↗
17. A. Strang and V. Vodarek: Mater. Sci. Technol., 1996, vol. 12, pp. 552–56.10.1179/mst.1996.12.7.552 ↗
18. V. Sklenicka, K. Kucharova, M. Svoboda, L. Kloc, J. Bursik, and A. Kroupa: Mater. Character., 2003, vol. 51, pp. 35–48.10.1016/j.matchar.2003.09.012 ↗
19. A. Strang, V. Foldyna, J. Lenert, V. Vodarek, and K.-H. Mayer: Proc. 6th Int. Charles Parsons Turbine Conf., Dublin, Ireland, Sept. 16–18, 2003, pp. 427–41.
20. E. Lotofsky and H. Cerjak: Sci. Technol. Weld. Join., 2004, vol. 9, pp. 31–36.10.1179/136217104225017116 ↗
21. K. Kimura, K. Suzuki, Y. Toda, H. Kushima, and F. Abe: Proc. 7th Liege Conf. on Materials for Advanced Power Engineering 2002, Liege, Belgium, Woodhead Publishing, Cambridge, UK, 2002, pp. 1171–80.
22. K. Kimura, H. Kushima, and K. Sawada: Proc. 6th Int. Charles Parsons Turbine Conf., Dublin, Ireland, Sept. 16–18, Woodhead Publishing, Cambridge, UK, 2003, pp. 444–56.
23. K. Suzuki, S Kumai, H. Kushima, K. Kimura, and F. Abe: Tetsu-to-Hagané, 2003, vol. 89, pp. 691–98.10.2355/tetsutohagane1955.89.6_691 ↗
24. K. Sawada, M. Taneike, K. Kimura, and F. Abe: ISIJ Int., 2004, vol. 44, pp. 1243–49.10.2355/isijinternational.44.1243 ↗
25. F. Abe: Mater. Sci. Eng. A, 2001, vols. 319–321, pp. 770–73.10.1016/S0921-5093(00)02002-5 ↗
26. Y. Kadoya, B. Dyson, and M. McLean: Metall. Mater. Trans. A, 2002, vol. 33A, pp. 2549–57.10.1007/s11661-002-0375-z ↗
27. H. Semba and F. Abe: Symp. USC Steels for Fossil Power Plants, G. Yong, ed., Beijing, China, 2005, pp. 157–62.
28. K. Sawada, H. Kushima, K. Kimura, and M. Tabuchi: ISIJ Int., 2007, vol. 47, pp. 733–39.10.2355/isijinternational.47.733 ↗
29. C.G. Panait, W. Bendick, A. Fuchsmann, A.F. Gourgues-Lorenzon, and J. Besson: Int. J. Press. Vess. Pip., 2010, vol. 87, pp. 326–35.10.1016/j.ijpvp.2010.03.017 ↗
30. H. Cerjak, P. Hofer, and B. Schaffernak: ISIJ Int., 1999, vol. 39, pp. 874–88.10.2355/isijinternational.39.874 ↗
31. H. Ghassemi Armaki: Ph.D. Thesis, Tohoku University, Sendai, Japan, 2008.
32. R.P. Chen, H. Ghassemi Armaki, K. Maruyama, and M. Igarashi: Mater. Sci. Eng. A, 2011, vol. 528 (13–14), pp. 4390–94.10.1016/j.msea.2011.02.060 ↗
33. K. Maruyama, E. Baba, K. Yokokawa, H. Kushima, and K. Yagi: Tetsu-to-Hagané, 1994, vol. 80, pp. 336–41.10.2355/tetsutohagane1955.80.4_336 ↗
34. H. Ghassemi Armaki, K. Maruyama, M. Yoshizawa, and M. Igarashi: Key Eng. Mater., 2007, vols. 345–346, pp. 553–56.10.4028/www.scientific.net/KEM.345-346.553 ↗
35. H. Ghassemi Armaki, K. Yoshimi, K. Maruyama, M. Yoshizawa, and M. Igarashi: Mater. Sci. Forum, 2007, vols. 561–565, pp. 2217–20.10.4028/www.scientific.net/MSF.561-565.2217 ↗
36. K. Miki, T. Azuma, Y. Tanaka, and T. Ishiguro: 4th Int. Conf. on Advances in Materials Technology for Fossil Power Plants, Hilton Head Island, South Carolina, ASM International, Materials Park, OH, 2004, pp. 1115–23.10.31399/asm.cp.am-epri-2004p1115 ↗
37. H. Ghassemi Armaki, R.P. Chen, K. Maruyama, M. Yoshizawa, and M. Igarashi: Mater. Lett., 2009, vol. 63, pp. 2423–25.10.1016/j.matlet.2009.08.024 ↗
38. O.D. Sherby, R.H. Klunalt, and A.K. Miller: Metall. Trans. A, 1977, vol. 8A, pp. 843–50.10.1007/BF02661565 ↗
39. F. Abe: Metall. Mater. Trans. A, 2003, vol. 34A, pp. 913–25.10.1007/s11661-003-0222-x ↗
40. F. Abe, H. Araki, and T. Noda: Metall. Trans. A, 1991, vol. 22A, pp. 2225–35.10.1007/BF02664988 ↗
41. F. Abe and S. Nakazawa: Metall. Trans. A, 1992, vol. 23A, pp. 3025–34.10.1007/BF02646120 ↗
42. S. Kano: M.Sc. Thesis, Tohoku University, Sendai, Japan, 2010.
43. F.J. Humphreys and M. Hatherly: Recrystallization and Related Annealing Phenomena, 2nd ed., 2004, pp. 140–50.10.1016/B978-008044164-1/50016-5 ↗
44. T. Nishizawa, I. Ohnuma, and K. Ishida: Mater. Trans. JIM, 1997, vol. 38, pp. 950–56.10.2320/matertrans1989.38.950 ↗
45. T. Gladman: Scripta Metall. Mater., 1992, vol. 27, pp. 1569–73.10.1016/0956-716X(92)90146-6 ↗
46. T. Gladman: Proc. R. Soc., 298, vol. 294A, pp. 298–309.