journal article·2004-11

Double loop electrochemical potentiokinetic reactivation test optimization in checking of duplex stainless steel intergranular corrosion susceptibility

T. Amadou, H. Sidhom, C. Braham

Publisher page

Abstract

The double loop electrochemical potentiokinetic reactivation (DL-EPR) test using an electrolyte of 33 pct H2SO4 solution with 0.3 pct HCl, at room temperature and at a potential scan rate dE/dt of about 2.5 mV/s, was chosen to evaluate the sensitization of austeno-ferritic duplex stainless steels (DSS). Reproducible and optimal test responses and high test selectivity in detecting integranular corrosion (IGC) susceptibility were verified for four DSS differing in their method of fabrication (cast or wrought) and their ferrite phase content (44 to 57 pct). The test was successfully used to analyze the interactions between precipitation, chromium depletion, and IGC sensitization of the UNS S31250 steel, which was aged between 6 minutes and 120 hours at temperatures varying from 500 °C to 900 °C. The eutectoid decomposition of the ferrite, at different aging temperatures, was investigated using various techniques. The chromium depletion was analyzed qualitatively by X-ray mapping in a scanning transmission electronic microscope (STEM) and quantitatively by analytical calculation based on the chromium diffusion in the ferrite. It was shown that the chromium content in the ferrite can decrease from 30 to 7.5 pct by weight during aging before total decomposition occurs. The interactions between precipitation and IGC sensitization during DSS aging were clearly shown by superimposing the time-temperature-start of precipitation (TTP) and time-temperature-sensitization (TTS) diagrams obtained from the DL-EPR tests performed for various levels of sensitization.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. P. Combrade and J.P. Audouard: Duplex Stainless Steels ’91, Proc. Conf., Beaune Bourgogne, France, 1991. J. Charles and S. Bernhardsson, eds., Les Edition de Physique, Paris, 1991, vol. 1, pp. 257–81.
2. J. Charles: Duplex Stainless Steels ’91, Proc. Conf., Beaune Bourgogne, France, 1991, J. Charles and S. Bernhardsson, eds., Les Editions de Physique, Paris, 1991, vol. 1, pp. 151–68.
3. S. Azuma and K. Ogawa: Appl. Thermal Eng., 1998, vol. 18 (6), p. XXIV.10.1016/S1359-4311(97)84446-8 ↗
4. N. Lopez, M. Cid, M. Puiggali, I. Azkarate, and A. Pelayo: Mater. Sci. Eng. A, 1997, vol. 229 (1–2), pp. 123–28.10.1016/S0921-5093(97)00008-7 ↗
5. T. Amadou, A. Ben Rhouma, H. Sidhom, C. Braham, and J. Lédion: Metall. Mater. Trans. A, 2000, vol. 31A (8), pp. 2015–24.10.1007/s11661-000-0229-5 ↗
6. B. Josefsson, J.O. Nilsson, and A. Wilson: Duplex Stainless Steels ’91, Proc. Conf., Beaune Bourgogne, France, 1991, J. Charles and S. Bernhardsson, eds., Les Editions de Physique, Paris, 1991, vol. 1, pp. 67–78.
7. M. Guttmann: Duplex Stainless Steels ’91, Proc. Conf., Beaune Bourgogne, France, 1991, J. Charles and S. Bernhardsson, eds., Les Editions de Physique, Paris, 1991, vol. 1, pp. 79–92.
8. Report No. NF EN ISO 3651-2, AFNOR, Cedex, France, 1998.
9. NF EN ISO 3651-1, AFNOR, Cedex, France, 1998.
10. Practice A262-98, Standard Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels, ASTM, New York, NY, 1998.
11. Test Method G28-97, Standard Test Methods of Detecting Susceptibility to Intergranular Corrosion in Wrought, Nickel-Rich, Chromium-Bearing Alloys, ASTM, New York, NY, 1997.
12. V. Cihal, A. Desestret, M. Froment, and G.-H. Wagner: 5th Eur. Conf. on Corrosion, Proc. Conf., Paris, 1973, pp. 249–54.
13. T. Wu, T. Cheng and W. Tsai: J. Nucl. Mater., 2001, vol. 295 (2–3), pp. 233–43.10.1016/S0022-3115(01)00558-X ↗
14. V. Cíhal and R. Ctefec: Electrochimica Acta, 2001, vol. 46 (24–25), pp. 3867–77.10.1016/S0013-4686(01)00674-0 ↗
15. M. Verneau, C. Lojewski, and J. Charles: Duplex Stainless Steels ’91, Proc. Conf., Beaune Bourgogne, France, 1991, J. Charles and S. Bernhardsson, eds., Les Editions de Physique, Paris, 1991, vol. 2, pp. 863–70.
16. M. Verneau, F. Dupoiron, and J. Charles: 12th Int. Corrosion Conf., Proc. Conf., Houston, TX, 1993.
17. M. Verneau and J.M. Scarabello: Corrosion in Chemical and Parachemical Industries, 2nd Eur. Conf. on corrosion, Proc. Conf., Grenoble, France, 1994, CEFRACOR, Paris, France, 1994, pp. 181–82.
18. I. Chattoraj, A.K. Bhattamishra, S. Jana, S.K. Das, S.P. Chakraborty, and P.K. De: Corr. Sci., 1996, vol. 38 (6), pp. 957–69.10.1016/0010-938X(96)00181-3 ↗
19. Y. Cetre, P. Eichner, G. Sibaud, and J.M. Scarabello: Corrosion in Chemical and Parachemical Industries 3rd Eur. Conf. on Corrosion, Proc. Conf., Lyon, France, 1997, CEFRACOR, Paris, France, 1997, pp. C4.1-C4.12.
20. M. Verneau, J. Charles, and J. Lojewski: Corrosion in Chemical and Parachemical Industries, 1st Eur. Conf. on corrosion, Proc. Conf., Lyon, France, 1991, CEFRACOR, Paris, France, 1991, pp. P17.1-P17.6.
21. N. Lopez: Ph.D. Thesis, University of Bordeaux I, Bordeaux, France, 1997.
22. F. Mazaudier, G. Sanchez, and P. Fauvet: Corrosion in Chemical and Parachemical Industries, 3rd Eur. Conf. on Corrosion, Proc. Conf., Lyon, France, 1997, CEFRACOR, Paris, France, 1997, pp. 12.1–12.6.
23. A.P. Majidi and M.A. Streicher: Corr. Nace, 1984, vol. 40 (8), pp. 393–408.10.5006/1.3593944 ↗
24. A.P. Majidi and M.A. Streicher: Corr. Nace, 1984, vol. 40 (11), pp. 584–93.10.5006/1.3581921 ↗
25. M. Verneau and B. Bonnefois: Corrosion in Chemical and Parachemical Industries, 3rd Eur. Conf. on Corrosion, Proc. Conf., Lyon, France, 1997, CEFRACOR, Paris, France, 1997, C5.1-C5.6.
26. U. Kamachi Mudali, R.K. Dayal, J.B. Gnanamoorthy, and P. Rodriguez: Metall. Mater. Trans. A, 1996, vol. 27A, pp. 2881–87.10.1007/BF02663836 ↗
27. S.J. Goodwin, B. Quayle, and F.W. Noble: Corr. Nace, 1987, vol. 43 (12), pp. 743–47.10.5006/1.3583863 ↗
28. David L. Reichert and Glenn E. Stoner: Electrochem Soc., 1990, vol. 137 (2), pp. 411–13.10.1149/1.2086454 ↗
29. J.R. Scully and R.G. Kelly: Corr. Nace, 1986, vol. 42 (9), pp. 537–42.10.5006/1.3583064 ↗
30. H. Sidhom and R. Portier: Phil. Mag. Lett., 1989, vol. 59 (3), pp. 131–39.10.1080/09500838908206334 ↗
31. H. Sidhom, S. Bonnet, and R. Portier: 3rd Int. Meeting on Quasicrystals and Incommensurate Structures, Proc. Conf., Vista Hermosa, Mexico, 1989, M. Morelos, ed., World Scientific Pub. Co., New York, 1990.
32. H. Sahlaoui, H. Sidhom, and J. Philibert: Acta Mater., 2002, vol. 50 (6), pp. 1383–92.10.1016/S1359-6454(01)00444-X ↗
33. H. Sidhom: Ph.D. Thesis, University of Paris XI, Paris, 1990.
34. I. Trigui, H. Sidhom, C. Braham, and J. Lédion: Mater. Technol., 1996, June, pp. 23–30.10.1051/mattech/199684060023s ↗
35. A. Roelandt and J. Vereecken: Corr. Nace, 1986, vol. 42 (5), pp. 289–98.10.5006/1.3584906 ↗
36. C. Stawström and M. Hillert: J. Iron Steel Inst., 1969, Jan., pp. 77–85.
37. A. Borello and S. Casadio: Corr. Nace, 1981, vol. 37 (9), pp. 498–505.10.5006/1.3580797 ↗