Advanced characterizations of fluorine-free tungsten film and its application as low resistance liner for PCRAM
Source abstract
Abstract
Using a metal-organic tungsten based precursor, a fluorine-free tungsten thin film has been obtained. The process deposition recipe includes a plasma-enhanced CVD (PECVD) step and atomic layer deposition (ALD) cycles. A set of physicochemical characterizations including X-ray reflectivity (XRR), in-plane X-ray diffraction (XRD), wavelength dispersive X-ray fluorescence (WDXRF), plasma profiling time of flight mass spectrometry (PPTOFMS) and microscope observations has been realized in order to study the W thin film structure and properties. The film is perfectly conformal whatever the structure size investigated (from tens of nanometers to micrometers wide). It was also highlighted that the F-free W film exhibits the lowest electrical resistivity phase (α-W) but is not pure. Indeed, in addition to a top surface oxidation, a layer located at the W film / substrate interface is present. This interface layer (IL) contains impurities, including carbon and oxygen, due to ligand decomposition. This IL might be deposited during the soak step or during the PECVD step. The W liner with thicknesses ranging from 3 to 4 nm has been implemented on PCRAM structures in order to evaluate its impact on contact plug resistivity. First electrical results are promising and demonstrate the interest of using a F-free low resistance W liner. At the aspect ratio studied, the gain in terms of contact plug resistivity is about 20% compared to the process of reference using a TiN liner. Modeling shows that this benefit is mainly due to the reduction of interface resistances.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and devices · Metal and Thin Film Mechanics · Copper Interconnects and Reliability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. L. Carbonell, H. Volders, N. Heylen, K. Kellens, R. Caluwaerts, K. Devriendt, E.A. Sanchez, J. Wouters, V. Gravey, K. Shah, Q. Luo, A. Sundarrajan, J. Lu, J. Aubuchon, P. Ma, M. Narasimhan, A. Cockburn, Z. Tökei, G.P. Beyer, Metallization of sub-30nm interconnects: Comparison of different liner/seed combinations, in: Proceedings of the 2009 IEEE International Interconnect Technology Conference, 2009, pp. 200–202. 〈http://dx.doi.org/10.1109/IITC.2009.5090387〉.10.1109/IITC.2009.5090387 ↗
2. Evaluation of metallization options for advanced Cu interconnects application10.1149/1.3567629 ↗
3. Z. Tökei, End of Cu roadmap and beyond Cu, in: Proceedings of the 2016 IEEE International Interconnect Technology Conference / Advanced Metallization Conference (IITC/AMC), 2016, pp. 1–58. 〈http://dx.doi.org/10.1109/IITC-AMC.2016.7507738〉.10.1109/IITC-AMC.2016.7507738 ↗
4. T. Nogami, M. He, X. Zhang, K. Tanwar, R. Patlolla, J. Kelly, D. Rath, M. Krishnan, X. Lin, O. Straten, H. Shobha, J. Li, A. Madan, P. Flaitz, C. Parks, C.K. Hu, C. Penny, A. Simon, T. Bolom, J. Maniscalco, D. Canaperi, T. Spooner, D. Edelstein, CVD-Co/Cu(Mn) integration and reliability for 10nm node, in: Proceedings of the 2013 IEEE International Interconnect Technology Conference, 2013, pp. 1–3. 〈http://dx.doi.org/10.1109/IITC.2013.6615592〉.10.1109/IITC.2013.6615592 ↗
5. R.H. Kim, B.H. Kim, J.N. Kim, J.J. Lee, J.M. Baek, J.H. Hwang, J. Hwang, J. Chang, S.Y. Yoo, T.J. Yim, K.M. Chung, K.H. Park, T. Oszinda, I.S. Kim, E.B. Lee, S.D. Nam, S. Jung, Y.W. Cho, H.J. Choi, J.S. Kim, S.H. Ahn, S.H. Park, B.U. Yoon, J.H. Ku, S.S. Paak, N.I. Lee, S. Choi, H.K. Kang, E.S. Jung, High performance Cu/low-k interconnect strategy beyond 10nm logic technology, in: Proceedings of the 2015 IEEE International Interconnect Technology Conference and 2015 IEEE Materials for Advanced Metallization Conference (IITC/MAM), 2015, pp. 1–4. 〈http://dx.doi.org/10.1109/IITC-MAM.2015.7325599〉.10.1109/IITC-MAM.2015.7325599 ↗
6. Y.K. Siew, N. Jourdan, Y. Barbarin, J. Machillot, S. Demuynck, K. Croes, J. Tseng, H. Ai, J. Tang, M. Naik, P. Wang, M. Narasimhan, M. Abraham, A. Cockburn, J. Bömmels, Z. Tökei, CVD Mn-based self-formed barrier for advanced interconnect technology, in: Proceedings of the 2013 IEEE International Interconnect Technology Conference, 2013, pp. 1–3. 〈http://dx.doi.org/10.1109/IITC.2013.6615551〉.10.1109/IITC.2013.6615551 ↗
7. M.H. van der Veen, K. Vandersmissen, D. Dictus, S. Demuynck, R. Liu, X. Bin, P. Nalla, A. Lesniewska, L. Hall, K. Croes, L. Zhao, J. Bömmels, A. Kolics, Z. Tökei, Cobalt bottom-up contact and via prefill enabling advanced logic and DRAM technologies, in: Proceedings of the 2015 IEEE International Interconnect Technology Conference and 2015 IEEE Materials for Advanced Metallization Conference (IITC/MAM), 2015, pp. 25–28. 〈http://dx.doi.org/10.1109/IITC-MAM.2015.7325605〉.10.1109/IITC-MAM.2015.7325605 ↗
8. Scalability of RuTiN barriers deposited by plasma-enhanced atomic layer deposition for advanced interconnects10.1016/j.mee.2013.08.008 ↗
9. Atomic layer deposition of ruthenium with TiN interface for sub-10nm advanced interconnects beyond copper10.1021/acsami.6b07181 ↗
10. High aspect ratio contacts10.1016/S0040-6090(96)09557-0 ↗
11. Advanced tungsten plug process for beyond nanometer technology10.1016/j.mee.2008.04.030 ↗
12. Influence of line dimensions on the resistance of Cu interconnections10.1109/55.735762 ↗
13. Classical size effect in oxide-encapsulated Cu thin films: Impact of grain boundaries versus surfaces on resistivity10.1116/1.2938395 ↗
14. Dominant role of grain boundary scattering in the resistivity of nanometric Cu films10.1103/PhysRevB.79.041402 ↗
15. Surface and grain-boundary scattering in nanometric Cu films10.1103/PhysRevB.81.155454 ↗
16. Phase transformation of thin sputter-deposited tungsten films at room temperature10.1116/1.1506905 ↗
17. Phase, grain structure, stress, and resistivity of sputter-deposited tungsten films10.1116/1.3622619 ↗
18. Copper interconnection integration and reliability10.1016/0040-6090(94)05807-5 ↗
19. Copper interconnections and reliability10.1016/S0254-0584(98)80000-X ↗
20. Reliability challenges for copper interconnects10.1016/j.microrel.2003.11.004 ↗
21. An introduction to Cu electromigration10.1016/j.microrel.2003.10.020 ↗
22. J. Bakke, Y. Lei, Y. Xu, K. Daito, X. Fu, G. Jian, K. Wu, R. Hung, R. Jakkaraju, N. Breil, Fluorine-free tungsten films as low resistance liners for tungsten fill applications, in: Proceedings of the 2016 IEEE International Interconnect Technology Conference / Advanced Metallization Conference (IITC/AMC), 2016, pp. 108–110. 〈http://dx.doi.org/10.1109/IITC-AMC.2016.7507699〉.10.1109/IITC-AMC.2016.7507699 ↗
23. X. Fu, G. Jian, J. Zhou, R. Jakkaraju, N. Yoshida, P. Ma, A conformal low resistivity fluorine free tungsten for FinFET metal gate and 3D memory applications, in: Proceedings of the 2016 China Semiconductor Technology International Conference (CSTIC), 2016, pp. 1–4. 〈http://dx.doi.org/10.1109/CSTIC.2016.7464018〉.10.1109/CSTIC.2016.7464018 ↗
24. Phase transformation of tungsten films deposited by diode and inductively coupled plasma magnetron sputtering10.1116/1.1642651 ↗