Analysis of LPCVD process conditions for the deposition of low stress silicon nitride. Part I: preliminary LPCVD experiments
Source abstract
Abstract
Abstract A wide range of process conditions were investigated to optimize conditions for the deposition of low stress silicon nitride films by low-pressure chemical vapor deposition. Experiments carried out in a standard, multi-wafer batch system generated films with an index of refraction ranging from about 2.04 to 2.82 and residual stress ranging from about 700 MPa tensile to –90 MPa compressive. The relationship between residual stress and index of refraction was characterized and results compared to those presented in the technical literature. Increase in the index of refraction beyond about 2.3 by means of increasing the gas flow did not reduce the residual stress appreciably but had a significant detrimental impact on the thickness uniformity and deposition rate. In contrast to results reported by other researchers, uniformity was not observed to increase with increasing DCS/NH3 ratio in this study. Efforts to minimize thickness non-uniformity by suppressing deposition rate at the gas inlet region of the deposition system while increasing deposition rate at the rear were not successful. While increasing the temperature at the exhaust end of the system was intended to improve thickness non-uniformity, significant thickness and index of refraction uniformity was not realized. The reduction in deposition rate and corresponding increase in index of refraction at the exhaust end of the system indicated a variation in gas species from inlet to exhaust of the system. These experimental results revealed that the index of refraction decreased while the deposition rate decreased with increasing partial pressure of DCS. This suggests that the inhomogeneity observed within the repeatability runs is due to ammonia depletion along the length of the load.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced Surface Polishing Techniques · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Hiraki S, Yasuda S, Ajima T, Yonezawa T. The electrochemical society extended abstracts, abstract 175, Vol. 80–1, St. Louis, MO, May 11–16, 1980. p. 461.
2. Local oxidation of silicon and its applications in semiconductor device technology
3. Bhattacharyya A, Selleck JE. The electrochemical society extended abstracts, abstract 51, vol. 80–1, St. Louis, MO, May 11–16, 1980. p. 144.
4. Sun JYC. Foundry technology for the next decade. Tech Dig EIDM 1998;321.10.1109/IEDM.1998.746364 ↗
5. Habermehl · J App Phys · 1998 · 83 · 910.1063/1.367253 ↗
6. Optimization of a low-stress silicon nitride process for surface-micromachining applications10.1016/S0924-4247(96)01397-0 ↗
7. Residual stress in silicon nitride films10.1007/BF02663273 ↗
8. Composition and structure control by source gas ratio in LPCVD SiNx10.1149/1.2119729 ↗
9. The composition and physical properties of LPCVD silicon nitride deposited with different NH3/SiH2Cl2 gas ratios10.1149/1.2113711 ↗
10. Generation of dislocations induced by chemical vapor deposited Si3N4 films on silicon10.1143/JJAP.11.1097 ↗
11. Ultralow-stress silicon-rich nitride films for microstructure fabrication
12. Mechanical stress of CVD-dielectrics10.1149/1.2069141 ↗
13. Optimization of the polycrystalline silicon-on-silicon dioxide characterization using spectroscopic ellipsometry10.1016/0040-6090(93)90092-4 ↗
14. An analysis of LPCVD system parameters for polysilicon, silicon nitride and silicon dioxide deposition