journal article·2024-03

Investigating surface wear characteristics of single-crystal SiC based on metal electrochemical corrosion

Da Hu, Jiabin Lu, Qiusheng Yan, Yingrong Luo, Ziyuan Luo

Publisher page

Abstract

Aiming at the environmental pollution of the polishing solution in chemical mechanical polishing, this study introduces a chemical mechanical polishing technique for single-crystal SiC based on metal electrochemical corrosion. The wear properties of the SiC C-surface, as influenced by different materials on grinding balls (Cu, Fe, Al, and Al 2O 3), and different solutions (KCl, Na 2SO 4 , Fenton, and H 2 O), were examined through wear experiments to elucidate the material removal mechanisms involved. The experiments demonstrated that the most significant wear marks, with a peak cross-sectional area of 46.89 μm 2, were obtained when the C-face of SiC was ground with Al-paired grinding balls in an Na 2SO 4 electrolyte solution. Energy dispersive spectroscopy analysis of the wear debris revealed an O elemental content of 11 %, and X-ray photoelectron spectroscopy analysis indicated the existence of SiO 2 and Al 2O 3 oxides. Subsequently, the effects of Na 2SO 4 solution concentration and pH on the wear pattern of the C-surface were investigated. The largest wear cross-sectional area (approximately 50 μm 2) was observed when using an Na 2SO 4 electrolyte solution with a concentration of 1.25 mol/L at a pH of 9 in an alkaline solution. The proposed mechanism of material removal in single-crystal SiC via metal electrochemical corrosion involves the Al metal acting as a cathode. This causes galvanic coupling corrosion, generating a corrosion current, which subsequently induces oxidation of the SiO 2 oxide layer on the anode SiC surface. The oxidized layer is then mechanically removed.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Semiconductor materials and devices · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Challenges of overcoming defects in wide bandgap semiconductor power electronics10.3390/electronics11010010 ↗
2. Electrical and optical control of single spins integrated in scalable semiconductor devices10.1126/science.aax9406 ↗
3. A Review: inductively coupled plasma reactive Ion etching of silicon carbide10.3390/ma15010123 ↗
4. Power electronics based on wide-bandgap semiconductors: opportunities and challenges10.1109/ACCESS.2021.3118897 ↗
5. Ultraprecision CMP for sapphire, GaN, and SiC for advanced optoelectronics materials10.1016/j.cap.2012.02.016 ↗
6. A review on chemical and mechanical phenomena at the wafer interface during chemical mechanical planarization10.1557/s43578-020-00060-x ↗
7. Mechanical aspects of the chemical mechanical polishing process: a review10.1007/s12541-016-0066-0 ↗
8. A review: green chemical mechanical polishing for metals and brittle wafers10.1088/1361-6463/ac0c4a ↗
9. Formulation of sodium hypochlorite based slurry for copper-cobalt chemical mechanical planarization process10.1149/2162-8777/ab682a ↗
10. Influence of slurry components on copper CMP performance in alkaline slurry10.1016/j.mee.2017.10.002 ↗
11. Synergistic action mechanism and effect of ammonium dodecyl sulfate and 1,2,4-triazole in alkaline slurry on step height reduction for Cu CMP10.1149/2162-8777/ab80b3 ↗
12. Environment friendly chemical mechanical polishing of copper10.1016/j.apsusc.2018.10.133 ↗
13. A novel approach of chemical mechanical polishing for a titanium alloy using an environment-friendly slurry10.1016/j.apsusc.2017.08.064 ↗
14. Green chemical mechanical polishing of sapphire wafers using a novel slurry
15. Chemical mechanical polishing for sapphire wafers using a developed slurry10.1016/j.jmapro.2021.01.004 ↗
16. The effect of surface polarity on the CMP behavior of 6H-SiC substrates10.1134/S1070427220060099 ↗
17. The influence of concentration of hydroxyl radical on the chemical mechanical polishing of SiC wafer based on the Fenton reaction10.1016/j.precisioneng.2017.12.011 ↗
18. Planarization mechanism for 6H–SiC (0001) Si-faced surfaces using electrochemical reactions10.1088/2053-1591/ab0152 ↗
19. Preliminary study on highly efficient polishing of 4H-SiC by utilization of anodic oxidation10.4028/www.scientific.net/AMR.1017.509 ↗
20. A study on surface polishing of SiC with a tribochemical reaction mechanism10.1007/s00170-003-1873-x ↗
21. A novel approach to obtain near damage-free surface/subsurface in machining of single crystal 4H-SiC substrate using pure metal mediated friction10.1016/j.apsusc.2022.152963 ↗
22. Chemical mechanical polishing exploiting metal electrochemical corrosion of single-crystal SiC10.1016/j.mssp.2022.107067 ↗
23. XPS study of leached glass surfaces10.1016/0022-3093(90)91029-Q ↗
24. Infrared and ESCA studies of a heterogenized rhodium carbonylation catalyst10.1016/S0021-9517(79)80003-2 ↗
25. XPS studies on SiOx thin films10.1016/0169-4332(93)90431-A ↗
26. Preparation and characterization of amorphous SiC:H thin films10.1116/1.577431 ↗
27. Compositional and structural analysis of aluminum oxide films prepared by plasma-enhanced chemical vapor deposition10.1016/0040-6090(94)90238-0 ↗
28. The interaction of thin NiO layers with single crystalline α-Al2O3(1120) substrates10.1016/0039-6028(95)00063-1 ↗
29. ESCA studies of aluminophosphate molecular sieves10.1021/j100153a045 ↗
30. Electrochemical behaviour and corrosion inhibition of Al, Al-6061 and Al–Cu in neutral aqueous solutions10.1016/S0010-938X(98)00145-0 ↗
31. Effects of 1,4-naphthoquinone on aluminum corrosion in 0.50M sodium chloride solutions10.1016/j.electacta.2005.06.018 ↗
32. Modeling the effects of individual layer thickness and orientation on the tribocorrosion behavior of Al/Cu nanostructured metallic multilayers10.1016/j.wear.2021.203849 ↗
33. Influence of milling route on the corrosion passivation of Al-2%SiC nanocomposites in chloride solutions10.3390/cryst11101231 ↗
34. Photoelectrochemical mechanical polishing method for n-type gallium nitride10.1016/j.cirp.2019.04.121 ↗
35. A review on precision polishing technology of single-crystal SiC10.3390/cryst12010101 ↗
36. Investigation of anodic oxidation mechanism of 4H-SiC (0001) for electrochemical mechanical polishing10.1016/j.electacta.2018.03.184 ↗
37. Electrochemistry of anodic etching of 4H and 6H–SiC in fluoride solution of pH 310.1016/j.electacta.2009.05.086 ↗
38. Effect of surface potential distribution on corrosion behavior of Cu/Al interface in Cu wire bonding applications10.1016/j.microrel.2020.113942 ↗
39. Evaluation of the modified extracted lignin from wheat straw as corrosion inhibitors for aluminum in alkaline solution10.20964/2018.05.49 ↗