Abstract
We report promising results regarding the possible use of AlN or Al2O3 as a gate dielectric in 4H-SiC MISFETs. The crystalline AlN films are grown by hot wall metal organic chemical vapor deposition (MOCVD) at 1100 °C. The amorphous Al2O3 films are grown by repeated deposition and subsequent low temperature (200 °C) oxidation of thin Al layers using a hot plate. Our investigation shows a very low density of interface traps at the AlN/4H-SiC and the Al2O3/4H-SiC interface estimated from capacitance-voltage (CV) analysis of MIS capacitors. Current-voltage (IV) analysis shows that the breakdown electric field across the AlN or Al2O3 is ∼ 3 MV/cm or ∼ 5 MV/cm respectively. By depositing an additional SiO2 layer by plasma enhanced chemical vapor deposition at 300 °C on top of the AlN or Al2O3 layers, it is possible to increase the breakdown voltage of the MIS capacitors significantly without having pronounced impact on the quality of the AlN/SiC or Al2O3/SiC interfaces.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Silicon Carbide Semiconductor Technologies · Semiconductor materials and devices · Copper Interconnects and Reliability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Jia · Appl. Surf. Sci. · 2017 · 397 · 17510.1016/j.apsusc.2016.11.142 ↗
2. Kodigala · Appl. Surf. Sci. · 2015 · 330 · 46510.1016/j.apsusc.2014.12.116 ↗
3. Kimoto · Jpn. J. Appl. Phys. · 2015 · 54 · 04010310.7567/JJAP.54.040103 ↗
4. Nawaz · 2015 · 1
5. Aboelfotoh · Appl. Phys. Lett. · 1996 · 69 · 287310.1063/1.117347 ↗
6. Vispute · MRS Online Proc. Libr. · 1999 · 59510.1557/PROC-595-F99W11.3 ↗
7. Choi · Appl. Phys. Lett. · 2005 · 86 · 19210110.1063/1.1923187 ↗
8. Afanasev · J. Phys. Condens. Matter. · 2004 · 16 · 183910.1088/0953-8984/16/17/019 ↗
9. Zheng · J. Appl. Phys. · 2013 · 113
10. Wongchotigul · Mater. Lett. · 1996 · 26 · 22310.1016/0167-577X(95)00225-1 ↗
11. Tanner · Appl. Phys. Lett. · 2007 · 91 · 20351010.1063/1.2805742 ↗
12. Horita · IEEE Trans. Electron Dev. · 2014 · 35 · 33910.1109/LED.2014.2299557 ↗
13. Onojima · Mater. Sci. Forum · 2004 · 457–460 · 156910.4028/www.scientific.net/MSF.457-460.1569 ↗
14. Onojima · Appl. Phys. Lett. · 2002 · 80 · 7610.1063/1.1428620 ↗
15. Zetterling · Appl. Phys. Lett. · 1997 · 70 · 354910.1063/1.119229 ↗
16. Zetterling · J. Appl. Phys. · 1997 · 82 · 299010.1063/1.366136 ↗
17. Feng · Carbon · 2014 · 75 · 24910.1016/j.carbon.2014.03.060 ↗
18. Badmaev · ACS Nano · 2012 · 6 · 337110.1021/nn300393c ↗
19. Avice · J. Appl. Phys. · 2007 · 10210.1063/1.2778289 ↗
20. Suvanam · Appl. Surf. Sci. · 2018 · 433 · 10810.1016/j.apsusc.2017.10.006 ↗
21. Usman · Mater. Sci. Semicond. Process. · 2018 · 81 · 11810.1016/j.mssp.2018.02.036 ↗
22. Yoshioka · AIP Adv. · 2016 · 6 · 10520610.1063/1.4966041 ↗
23. Hatayama · IEEE Trans. Electron Devices · 2008 · 55 · 204110.1109/TED.2008.926647 ↗
24. Chen · J. Cryst. Growth · 2015 · 428 · 5410.1016/j.jcrysgro.2015.07.021 ↗
25. Khosa · AIP Adv. · 2018 · 810.1063/1.5021411 ↗
26. Allerstam · Semicond. Sci. Technol. · 2007 · 22 · 30710.1088/0268-1242/22/4/002 ↗
27. Nicollian · 1982
28. Cooper · Phys. Status Solidi · 1997 · 162 · 30510.1002/1521-396X(199707)162:1<305::AID-PSSA305>3.0.CO;2-7 ↗
29. Sadeghi · Microelectron. Eng. · 1997 · 36 · 18310.1016/S0167-9317(97)00044-0 ↗
30. Berberich · Solid-State Electron. · 1998 · 42 · 91510.1016/S0038-1101(98)00122-1 ↗
31. Gordon · Phys. Rev. B · 2014 · 89 · 08520410.1103/PhysRevB.89.085204 ↗
32. Yu · Chin. Phys. B · 2015 · 24 · 08730410.1088/1674-1056/24/8/087304 ↗