Abstract Single crystal gallium nitride will produce subsurface damage during processing, and studying the total stress field during scratching gallium nitride is advantageous for predicting and controlling subsurface damage. The total stress field during scratching gallium nitride (0001) crystal plane is obtained by superimposing the elastic and residual stress field. Thus the distribution of the stress field under the indenter can be acquired. It was found that the median crack nucleated at the elastoplastic interface of the front of the indenter, and the extension angle of the median crack is linearly related to half-angle of the conical indenter. Next the anisotropic model in this paper and the method simplified to isotropic materials are used for calculating the total stress field, and the consequences of the two are obviously different. The ratio between the stresses obtained by the two methods under different indenter half-angle has been obtained. Then by introducing the corresponding ratio into the traditional equation of the median crack depth and the lateral crack depth, the results considering the anisotropy can be obtained by the isotropic method.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · GaN-based semiconductor devices and materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Microwave performance of a 0.25 mu-m gate AlGaN/GaN heterostructure field effect transistor10.1063/1.112116 ↗
2. High-brightness InGaN blue, green and yellow light-emitting diodes with quantum well structures10.1143/JJAP.34.L797 ↗
3. Fabrication of 3-in GaN substrates by hydride vapor phase epitaxy using void-assisted separation method10.1016/j.jcrysgro.2007.10.014 ↗
4. A GaN bulk crystal with improved structural quality grown by the ammonothermal method10.1038/nmat1955 ↗
5. Chemical mechanical polishing of gallium nitride with colloidal silica10.1149/2.024112jes ↗
6. GaN: processing, defects, and devices10.1063/1.371145 ↗
7. Evaluation of subsurface damage in GaN substrate induced by mechanical polishing with diamond abrasives10.1016/j.apsusc.2013.12.005 ↗
8. Ultra-precision grinding10.1016/j.cirp.2010.05.001 ↗
9. Processing characteristics in scratching and indentation test of single crystal gallium nitride10.2493/jjspe.74.282 ↗
10. Nanotribological properties of Ga- and N-faced bulk gallium nitride surfaces determined by nanoscratch experiments10.3390/ma12172653 ↗
11. Nanoscratch characterization of GaN epilayers on c- and a-Axis sapphire substrates10.1007/s11671-010-9717-8 ↗
12. Material removal mechanism of 6H-SiC studied by nano-scratching with Berkovich indenter10.1007/s00339-016-9802-7 ↗
13. Role of cracks, pores, and absorbing inclusions on laser induced damage threshold at surfaces of transparent dielectrics10.1364/AO.12.000661 ↗
14. Subsurface damage measurement of ground fused silica parts by HF etching techniques10.1364/OE.17.020448 ↗
15. Evaluation of subsurface damage inherent to polished GaN substrates using depth-resolved cathodoluminescence spectroscopy10.1016/j.tsf.2018.07.002 ↗
16. Cathodoluminescence evaluation of subsurface damage in GaN substrate after polishing
17. Subsurface damage in polishing process of silicon carbide ceramic10.3390/ma11040506 ↗
18. Effect of wire speed on subsurface cracks in wire sawing process of single crystal silicon carbide10.1016/j.engfracmech.2017.09.002 ↗
19. Elastic stress fields caused by indenting brittle materials10.1080/01418618208236917 ↗
20. An analytical expression for the stress field around an elastoplastic indentation/contact10.1016/j.actamat.2006.12.030 ↗
21. Elastic/plastic indentation damage in ceramics: the median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
22. Sliding microindentation fracture of brittle materials: role of elastic stress fields10.1016/S0167-6636(98)00012-X ↗
23. Experimental study on abrasive waterjet polishing for hard-brittle materials10.1016/j.ijmachtools.2009.02.005 ↗
24. Stress analysis in scratching of anisotropic single-crystal silicon carbide10.1016/j.ijmecsci.2018.03.042 ↗
25. Anisotropic elasticity in hexagonal crystals10.1016/j.tsf.2007.01.045 ↗
26. First-principles study on electronic and elastic properties of BN, AlN, and GaN10.1063/1.368739 ↗
27. Study on nucleation and propagation of median cracks generated by scratching single crystal silicon10.1016/j.mssp.2019.104691 ↗
28. Elastostatic Green's function for advanced materials subject to surface loading10.1023/B:ENGI.0000031191.64358.a8 ↗
29. Displacement field of a point force acting on the surface of an elastically anisotropic half-space10.1088/0305-4470/27/23/033 ↗
30. Residue approach for evaluating the 3D anisotropic elastic Green's function: multiple roots10.1016/j.enganabound.2004.12.012 ↗
31. Elastic stress field model and micro-crack evolution for isotropic brittle materials during single grit scratching10.1016/j.ceramint.2017.05.054 ↗
32. Nucleation location and propagation direction of radial and median cracks for brittle material in scratching10.1016/j.ceramint.2019.01.046 ↗
33. A quantitative analysis for the stress field around an elastoplastic indentation/contact10.1557/jmr.2009.0097 ↗
34. Deformation of silicon - insights from microcompression testing at 25-500 degrees C10.1016/j.ijplas.2011.05.009 ↗
35. Microfracture beneath point indentations in brittle solids10.1007/BF00541038 ↗
36. Strength or toughness? A criterion for crack onset at a notch10.1016/S0997-7538(01)01184-6 ↗
37. Insight into physical processes controlling the mechanical properties of the wurtzite group-III nitride family10.1016/j.jcrysgro.2018.08.001 ↗
38. Elastic and plastic properties of GaN determined by nano-indentation of bulk crystal10.1063/1.124919 ↗
39. Material removal mechanisms from grinding to polishing
40. Indentation-induced dislocations and cracks in (0001) freestanding and epitaxial GaN10.1088/1742-6596/281/1/012007 ↗
41. Relationship between subsurface damage and surface roughness of optical materials in grinding and lapping processes10.1016/j.jmatprotec.2007.11.118 ↗