The impact of silicon brick polishing on thin (120 μm) silicon wafer sawing yields and fracture strengths in diamond-wire sawing
Source abstract
Abstract
Abstract The present study recommends sawing thin (120 μm) silicon (Si) wafers using thin (120 μm) diamond wire with higher throughputs and sawing yields (>96%). In a multi-wire saw, an improved type of diamond wire (100 d/M6-12) is employed to saw ground (g) and mirror-polished (p) Si bricks into thin (120 μm) Si wafers. Improvements in both diamond wire and Si brick surface allow us to saw thin (120 μm) Si wafers with higher fracture strengths and sawing yields of over 96%. The wafers sawn from g and p Si bricks are labeled as g- Si wafers and p- Si wafers. Depending on wire wear position, sawn wafers are labeled as fresh-wire and worn-wire sides. In a three-line bending test, mechanical loads were applied perpendicular to the wire saw marks on the middle of each wafer to measure its fracture strength. Two fundamental differences are observed in the fracture strengths of g- and p- Si wafers. The g- Si wafers fractured at lower strengths compared with the p- Si wafers. Both g- and p- Si wafers from the fresh-wire side fractured at lower strengths compared with worn-wire-side wafers. To address the fracture strength difference, edge chipping and fractographic studies were carried out. The wafer edges were observed at wire entrance and wire exit sides in the Si brick. At the wire exit side, the wafer surface contains a large number of pits followed by longer chipping lengths and widths compared with the wire entrance side. The fractographic studies were performed on fractured samples collected from the middle of the wafer by observing its cross-sections. The wafers fractured at low-strength samples follow mirror mechanisms, and the wafers fractured at intermediate- and higher-strength samples follow any one of mirror–mist, mist, hackle, branching or a mixture of these mechanisms.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Surface Polishing Techniques · Diamond and Carbon-based Materials Research · Force Microscopy Techniques and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Review of CMOS integrated circuit technologies for high-speed photo-detection10.3390/s17091962 ↗
2. 2019
3. High-efficiency heterojunction crystalline Si solar cells10.7567/JJAP.57.08RB20 ↗
4. Challenges associated with diamond wire sawing when generating reduced thickness mono-crystalline silicon wafers
5. Crack detection in crystalline silicon solar cells using dark-field imaging10.1016/j.egypro.2017.09.252 ↗
6. A review of crystalline silicon bifacial photovoltaic performance characterisation and simulation10.1039/C8EE02184H ↗
7. Edge chipping of silicon wafers in diamond grinding10.1016/j.ijmachtools.2012.08.002 ↗
8. Review of new technology for preparing crystalline silicon solar cell materials by metallurgical method10.1088/1755-1315/94/1/012016 ↗
9. Wafer slicing by internal diameter sawing10.1016/0141-6359(88)90092-X ↗
10. Grinding of silicon wafers: a review from historical perspectives10.1016/j.ijmachtools.2008.05.009 ↗
11. Silicon crystal growth and wafer technologies10.1109/JPROC.2012.2189786 ↗
12. The effect of cut depth and distribution for abrasives on wafer surface morphology in diamond wire sawing of PV polycrystalline silicon10.1016/j.mssp.2018.12.004 ↗
13. Mechanisms of wafer sawing and impact on wafer properties10.1002/pip.972 ↗
14. Two-body and three-body abrasion: a critical discussion10.1016/S0043-1648(97)00188-9 ↗
15. Wire sawing technology: a state-of-the-art review10.1016/j.precisioneng.2015.08.008 ↗
16. Effects of mirror polishing brick surface on process yield of multi-wire slicing for thin single-crystalline silicon solar cells10.1016/j.solener.2015.10.022 ↗
17. The impact of subsurface damage on the fracture strength of diamond-wire-sawn monocrystalline silicon wafers10.7567/JJAP.57.08RB08 ↗
18. The impact of saw mark direction on the fracture strength of thin (120 μm) monocrystalline silicon wafers for photovoltaic cells10.7567/JJAP.57.095501 ↗
19. The impact of damage etching on fracture strength of diamond wire sawn monocrystalline silicon wafers for photovoltaics use10.7567/JJAP.57.126501 ↗
20. On the cracks self-healing mechanism at ductile mode cutting of silicon10.1016/j.triboint.2014.07.003 ↗
21. Subsurface crack damage in silicon wafers induced by resin bonded diamond wire sawing10.1016/j.mssp.2016.10.021 ↗
22. Fundamental investigation of subsurface damage in single crystalline silicon caused by diamond machining10.1016/j.precisioneng.2008.10.008 ↗
23. Development of a high-speed manufacturing method for electroplated diamond wire tools10.1016/S0007-8506(07)60584-8 ↗
24. Experiment study on electroplated diamond wire saw slicing single- crystal silicon10.1016/j.mssp.2016.08.003 ↗
25. Experimental investigation of tool wear in electroplated diamond wire sawing of silicon10.1016/j.procir.2018.09.038 ↗
26. Diamond wire sawing of solar silicon wafers: a sustainable manufacturing alternative to loose abrasive slurry sawing10.1016/j.promfg.2018.02.156 ↗
27. Mechanics prediction of the fracture pattern on scratching wafers of single crystal silicon10.1016/j.actamat.2012.04.040 ↗
28. Investigation on critical crack-free cutting depth for single crystal silicon slicing with fixed abrasive wire saw based on the scratching machining experiments10.1016/j.mssp.2017.10.027 ↗
29. Grinding induced subsurface cracks in silicon wafers10.1016/S0890-6955(98)00079-0 ↗
30. Directional anisotropy in the cleavage fracture of silicon10.1103/PhysRevLett.84.5347 ↗
31. Klute · 2014 · 753
32. Aspects of rapid crack propagation in silicon10.1111/j.1460-2695.2006.01054.x ↗
33. Dislocations deflect and perturb dynamically propagating cracks10.1103/PhysRevLett.93.265501 ↗
34. Energy considerations in crack deflection phenomenon in single crystal silicon10.1007/s10704-006-0048-9 ↗
35. From crack defection to lattice vibrations-macro to atomistic examination of dynamic cleavage fracture10.1016/j.jmps.2004.02.004 ↗
36. Hackle or textured mirror? Analysis of surface perturbation in single crystal silicon
37. Fractography of dynamic crack propagation in silicon crystal10.4028/www.scientific.net/KEM.409.55 ↗
38. Crack plane deflection and shear wave effects in the dynamic fracture of silicon single crystal10.1016/j.jmps.2018.09.031 ↗