journal article·2021-02Open access

The improvement of atomic layer deposited SiO2/4H-SiC interfaces via a high temperature forming gas anneal

A.B. Renz, O.J. Vavasour, P.M. Gammon, F. Li, T. Dai, M. Antoniou, G.W.C. Baker, E. Bashar, N.E. Grant, J.D. Murphy, P.A. Mawby, V.A. Shah

Abstract

This letter reports on the improvement of a SiO2 layer formed by atomic layer deposition on 4H-SiC, using a post-deposition anneal in forming gas ambient. Capacitance–voltage measurements revealed good electrical properties, compared to a thermal oxide which was grown in N2O, with flatband voltage values averaging at -0.29 V and a low positive mobile ion charge density in the order of 1010 cm−2. XPS analysis revealed the FG annealed sample to have the most Si rich interface comparatively to other PDAs, with a C:Si ratio of 0.72, allowing more Si bonds to be terminated. SIMS analysis identified an increase in hydrogen near the interface of the FG-annealed sample with a peak concentration of 2.12 × 1021 cm−3. It is concluded that the improvement in electrical performance is due to the hydrogen passivating trap states at the SiO2/4H-SiC interface.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicon Carbide Semiconductor Technologies · Semiconductor materials and devices · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Band offsets and electronic structure of SiC/SiO2 interfaces10.1063/1.361254 ↗
2. Dielectrics in silicon carbide devices: Technology and application
3. Bonding at the SiC-SiO2 interface and the effects of nitrogen and hydrogen10.1103/PhysRevLett.98.026101 ↗
4. Emerging trends in wide band gap semiconductors (SiC and GaN) technology for power devices10.1016/j.mee.2017.11.021 ↗
5. Comparison of thermal and atomic-layer-deposited oxides on 4H-SiC after post-oxidation-annealing in nitric oxide10.1063/1.3689766 ↗
6. Electrical characteristics of SiO2 deposited by atomic layer deposition on 4H–SiC after nitrous oxide anneal10.1109/TED.2016.2565665 ↗
7. Improved threshold voltage instability in 4H-SiC MOSFETs with atomic layer deposited SiO2
8. Densification of silicon dioxide formed by plasma-enhanced atomic layer deposition on 4h-silicon carbide using argon post-deposition annealing10.1016/j.ceramint.2018.04.190 ↗
9. Development of high-quality gate oxide on 4H-SiC using atomic layer deposition
10. A study of deep energy-level traps at the 4H-SiC/SiO2 interface and their passivation by hydrogen
11. Forming gas annealing of the carbon PbC center in oxidized porous 3C-and 4H-SiC: an EPR study
12. Microscopic structure and electrical activity of 4H-SiC/SiO2 interface defects: An EPR study of oxidized porous SiC
13. Effects of combined NO and forming gas annealing on interfacial properties and oxide reliability of 4H-SiC MOS structures10.1016/j.microrel.2015.11.022 ↗
14. Characterization of the effects of nitrogen and hydrogen passivation on SiO2/4H-SiC interface by low temperature conductance measurements
15. Investigation of unusual mobile ion effects in thermally grown SiO2 on 4H-SiC (0001) at high temperatures10.1063/1.4729780 ↗
16. Understanding and controlling bias-temperature instability in SiC metal-oxide-semiconductor devices induced by unusual generation of mobile ions10.1063/1.4794942 ↗
17. Improved bias-temperature instability characteristics in SiC metal-oxide-semiconductor devices with aluminum oxynitride dielectrics10.1063/1.4870047 ↗
18. High temperature nitridation of 4H-SiC MOSFETs
19. Kimoto · 2014
20. Surface states at steam-grown silicon-silicon dioxide interfaces10.1109/T-ED.1966.15827 ↗
21. Schroder · 2015
22. Generation of very fast states by nitridation of the SiO2/SiC interface10.1063/1.4740068 ↗
23. Limitations of the high-low c-v technique for MOS interfaces with large time constant dispersion10.1109/TED.2013.2237777 ↗
24. Bias-stress induced threshold voltage and drain current instability in 4H–SiC DMOSFETs10.1016/j.sse.2007.07.031 ↗
25. Temperature-dependence of SiC MOSFET threshold-voltage instability
26. MOS characteristics of C-face 4H-SiC10.1007/s11664-010-1096-5 ↗
27. Negative charge trapping effects in Al2o3 films grown by atomic layer deposition onto thermally oxidized 4H-SiC10.1063/1.4960213 ↗
28. Improved interface and electrical properties of atomic layer deposited Al2o3/4H-SiC10.1016/j.apsusc.2017.10.006 ↗
29. The improvement of Mo/4H-SiC schottky diodes via a P2o5 surface passivation treatment10.1063/1.5133739 ↗
30. SiC MOS interface states: Difference between Si face and C face10.1149/05807.0055ecst ↗
31. Electron-spin-resonance and electrically detected-magnetic-resonance characterization on PbC center in various 4H-SiC (0001)/SiO2 interfaces10.1063/1.5134648 ↗
32. Theoretical models of hydrogen-induced defects in amorphous silicon dioxide10.1103/PhysRevB.92.014107 ↗