Investigation of soldering process and interfacial microstructure evolution for the formation of full Cu3Sn joints in electronic packaging
Source abstract
Abstract
Abstract Within electronic products, solder joints with common interfacial structure of Cu/IMCs/Sn-based solders/IMCs/Cu cannot be used under high temperature for relatively low melting points of Sn-based solders (200–300 °C). However, there is a trend for solder joints to service under high temperature because of the objective for achieving multi-functionality of electronic products. With the purpose of ensuring that solder joints can service under high temperature, full Cu3Sn solder joints with the interfacial structure of Cu/Cu3Sn/Cu can be a substitute due to the high melting point of Cu3Sn (676 °C). In this investigation, soldering process parameters were optimized systematically in order to obtain such joints. Further, interfacial microstructure evolution during soldering was analyzed. The soldering temperature of 260 °C, the soldering pressure of 1 N and the soldering time of 5 h were found to be the optimal parameter combination. During soldering of 260 °C and 1 N, the Cu6Sn5 precipitated first in a planar shape at Cu-Sn interfaces, which was followed by the appearance of planar Cu3Sn between Cu and Cu6Sn5. Then, the Cu6Sn5 at opposite sides continued to grow with a transition from a planar shape to a scallop-like shape until residual Sn was consumed totally. Meanwhile, the Cu3Sn grew with a round-trip shift from a planar shape to a wave-like shape until the full Cu3Sn solder joint was eventually formed at 5 h. The detailed reasons for the shape transformation in both Cu6Sn5 and Cu3Sn during soldering were given. Afterwards, a microstructure evolution model for Cu-Sn-Cu sandwich structure during soldering was proposed. Besides, it was found that no void appeared in the interfacial region during the entire soldering process, and a discuss about what led to the formation of void-free joints was conducted.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Humpston · 2004
2. Intermetallic growth study on SnAgCu/Cu solder joint interface during thermal aging
3. Cu6Sn5 morphology transition and its effect on mechanical properties of eutectic Sn-Ag solder joints10.1007/s11664-010-1430-y ↗
4. Interfacial reaction and morphology between molten Sn base solders and cu substrate10.2320/matertrans.45.646 ↗
5. Microstructural evolution and tensile properties of Sn-Ag-Cu mixed with Sn-Pb solder alloys10.1016/j.jallcom.2008.10.141 ↗
6. The microstructure parameters and microhardness of dorectionally solidified Sn-Ag-Cu eutectic10.1016/j.jallcom.2009.06.067 ↗
7. Interrelation of wettability-microstructure-tensile strength of lead-free Sn-Ag and Sn-bi solder alloys10.1080/13621718.2015.1124176 ↗
8. Effect of trace platinum additions on the interfacial morphology of Sn-3.8Ag-0.7Cu alloy aged for long hours10.1016/j.microrel.2014.06.014 ↗
9. Effect of In on microstructure, thermodynamic characteristic and mechanical properties of Sn-Bi based lead-free solder10.1016/j.jallcom.2015.01.219 ↗
10. Wetting and microstructure evolution of the Sn-Zn-Ag/Cu interface10.1007/s11665-014-0929-4 ↗
11. Effects of thermal annealing in the post-reflow in microstructure, tin crystallography, and impact reliability of Sn-Ag-Cu solder joints10.1016/j.msea.2014.06.102 ↗
12. Low temperature epoxy bonding for wafer level MEMS packaging10.1016/j.sna.2007.10.048 ↗
13. Effect of isothermal aging and low density current on intermetallic compound growth rate in lead-free solder interface10.1016/j.microrel.2013.09.005 ↗
14. Evolution of intermetallic compounds between Sn-0.3Ag-0.7Cu low-silver lead-free solder and Cu substrate during thermal aging10.1016/S1005-0302(12)60023-1 ↗
15. Effect of Isothermal aging and thermal cycling on interfacial IMC growth and fracture behavior of SnAgCu/Cu joints10.1007/s11664-010-1401-3 ↗
16. Study of interfacial reactions between Sn3.5Ag0.5Cu composite alloys and Cu substrate10.1016/j.mee.2011.04.034 ↗
17. Kinetics of intermetallic compound formation at the interface between Sn-3.0Ag-0.5Cu solder and Cu-Zn alloy substrates10.1007/s11664-010-1379-x ↗
18. Prediction of interface reaction products between Cu and various solder alloys by thermodynamic calculation10.1016/S1359-6454(96)00325-4 ↗
19. Early stages of soldering reactions10.1063/1.2058186 ↗
20. Nucleation kinetics of Cu6Sn5 by reaction of molten tin with a copper substrate10.1007/s11664-002-0010-1 ↗
21. Intermetallic growth kinetics for Sn-Ag, Sn-Cu, and Sn-Ag-Cu lead-free solders on Cu, Ni, and Fe-42Ni substrates10.1007/s11664-006-0152-7 ↗
22. Theory for intermetallic phase growth between Cu and liquid Sn-Pb solder based on grain boundary diffusion control10.1007/s11664-998-0066-7 ↗
23. Effects of Ag content on the interfacial reactions between liquid Sn-Ag-Cu solders and Cu substrates during soldering10.1016/j.jallcom.2016.03.177 ↗
24. Growth behaviors of intermetallic compounds at Sn-3Ag-0.5Cu/Cu interface during isothermal and non-isothermal aging10.1016/j.jallcom.2013.05.156 ↗
25. Microstructural evolution at Cu/Sn-Ag-Cu and Cu/Sn-Ag-Cu/Ni-Au ball grid array interfaces during thermal aging10.1016/j.jallcom.2014.05.200 ↗
26. The effect of reflow time on reactive,evolution of interfacial IMCs and shear strength of eutectic Sn-Cu solder alloy
27. Murr · 1975
28. Kinetics analysis of the soldeing reaction between eutectic SnPb alloy and Cu accompanied by ripening10.1103/PhysRevB.53.16027 ↗
29. Kinetics theory of flux-driven ripening10.1103/PhysRevB.66.115403 ↗
30. Dissolution and interfacial reactions of thin-film Ti/Ni/Ag metallizations in solder joints10.1016/S1359-6454(01)00187-2 ↗
31. Interfacial reactions between lead-free solders and common base metals10.1016/j.mser.2005.03.001 ↗
32. Properties of lead-free solder alloys with rare earth element additions10.1016/j.mser.2004.01.001 ↗
33. Impact of Thermal Cycling on Sn-Ag-Cu Solder Joints and Board-Level Drop Reliability10.1007/s11664-008-0400-0 ↗
34. Kirkendall void formation in eutectic SnPb solder joints on bare Cu and its effect on joint reliability10.1063/1.1839637 ↗
35. On the root cause of Kirkendall voiding in Cu3Sn10.1557/jmr.2010.47 ↗
36. EBSD investigation of Cu-Sn IMC microstructural evolution in Cu/Sn-Ag/Cu microbumps during isothermal annealing10.1007/s11664-013-2675-z ↗
37. Acceleration of the growth of Cu3Sn voids in solder joints10.1016/j.microrel.2011.12.005 ↗
38. Assessing the risk of "Kirkendall voiding" in Cu3Sn10.1016/j.microrel.2010.11.014 ↗
39. L. Yin, P. Kondos, P. Kondos, Y. H. Liu, S. Bliznakov, F. Wafula, N. Dimitrov, D. W. Henderson, C. Parks, M. Gao, J. Therriault, J. Wang, E. Cotts: Controlling Cu Electroplating to Prevent Sporadic Voiding in Cu3Sn, in: Proceedings of the 59th Electronic Components and Technology Conference, San Diego, California, May 2009,pp. 406–414.10.1109/ECTC.2009.5074046 ↗
40. Kirkendall voids formation in the reaction between Ni-doped SnAg lead-free solders and different Cu substrates10.1016/j.microrel.2008.09.010 ↗
41. A study on the thermal reliablity of Cu/SnAg double-bump flip-chip assemblies on organic substrates'10.1007/s11664-008-0498-0 ↗
42. Intermetallic growth and Kirkendall effect manifestations in Cu/Sn and Au/Sn diffusion couples10.1515/ijmr-2004-0169 ↗
43. Critical concerns in soldering reactions arising from space confinement in 3-D IC packages10.1109/TDMR.2012.2185239 ↗
44. Elimination of voids in reactions between Ni and Sn: a novel effect of solver10.1016/j.scriptamat.2011.10.032 ↗
45. Calculating the diffusivity of Cu and Sn in Cu3Sn intermetallic by molecular dynamics simulations10.1016/j.matlet.2012.01.014 ↗
46. Cavity formation and metallurgical changes induced by growth of oxide scale10.1179/mst.1988.4.12.1089 ↗
47. The role of interface dislocations and ledges as sources/sinks for point defects in scaling reactions10.1016/0956-7151(94)00296-T ↗
48. Structure and migration of (112) step on (111) twin boundaries in nanocrystalline copper10.1063/1.3035944 ↗