Water stress corrosion at wafer bonding interface during bond strength evaluation
Source abstract
Abstract
Wafer-to-wafer bonding is becoming a critical unit process step with the increase in the demand for 3D integration. The widely used bonding method is plasma activated bonding, where it is essential to ensure sufficient bond strength to withstand the stresses generated during subsequent processes and achieve multi-layer stacking or layer transfer. Although the double cantilever beam method is widely used to evaluate wafer bond strength, significant variation occurs due to water stress corrosion at the bonding interface. These factors have not been adequately addressed, and precise measurement conditions have yet to be established. In this study, a semi-auto tool was introduced to conduct measurements under an inert atmosphere, whereby the influence of water stress corrosion was eliminated. Furthermore, the study elucidated the effects of the crystal orientation and blade insertion conditions. The impacts of interfacial voids and the annealing conditions on bond strength were revealed. Observation of the progress of delamination during measurements under an inert atmosphere enabled the effective estimation of the moisture content that remained inside the wafers, which then contributed to the selection of appropriate annealing conditions. • Accurate bond strength via Double Cantilever beam method for direct wafer bonding was investigated. • Controlled environment ensured consistent measurements with minimal variation by eliminating water stress corrosion. • Water stress corrosion is caused by moisture in the atmosphere, interface voids, and residual moisture, affecting delamination length. • Evaluating delamination under inert atmosphere aids in estimating proper annealing conditions.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: 3D IC and TSV technologies · Electronic Packaging and Soldering Technologies · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Buried power rails and nano-scale TSV: technology boosters for backside power delivery network and 3D heterogeneous integration
2. Future logic scaling: towards atomic channels and deconstructed chips10.1109/IEDM13553.2020.9372023 ↗
3. Enabling logic with backside connectivity via n-TSVs and its potential as a scaling booster
4. 3-D sequential stacked planar devices featuring low-temperature replacement metal gate junctionless top devices with improved reliability10.1109/TED.2018.2871265 ↗
5. First Demonstration of 3D stacked Finfets at a 45nm fin pitch and 110nm gate pitch technology on 300mm wafers
6. 3D sequential stacked planar devices on 300 mm wafers featuring replacement metal gate junction-less top devices processed at 525°C with improved reliability
7. The Complementary FET (CFET) for CMOS scaling beyond N3
8. Fabrication of vertically stacked nanosheet junctionless field-effect transistors and applications for the CMOS and CFET inverters10.1109/TED.2020.3007134 ↗
9. Inorganic temporary direct bonding for collective die to wafer hybrid bonding
10. Area-selective electroless deposition of Cu for hybrid bonding10.1109/LED.2021.3124960 ↗
11. Novel stacked CMOS image sensor with advanced Cu2Cu hybrid bonding10.1109/IEDM.2016.7838375 ↗
12. Novel Cu/SiCN surface topography control for 1 μm pitch hybrid wafer-to-wafer bonding10.1109/ECTC32862.2020.00046 ↗
13. Exploring bond strength for an advanced chiplet with hybrid bonding
14. Atomic diffusion bonding in air using oxide films10.1149/11203.0173ecst ↗
15. Influence of composition of SiCN as interfacial layer on plasma activated direct bonding10.1149/2.0241906jss ↗
16. Film characterization of low-temperature silicon carbon nitride for direct bonding applications10.1149/2162-8777/abd260 ↗
17. Influence of Si wafer thinning processes on (sub) surface defects10.1016/j.apsusc.2017.01.259 ↗
18. Modified SAB methods for hybrid and all-Cu bonding for 3D integration below 200°C10.1149/11203.0103ecst ↗
19. 300 mm wafer-level hybrid bonding for Cu/interlayer dielectric bonding in vacuum10.7567/1347-4065/ab4b2b ↗
20. Characterization of bonding activation sequences to enable ultra-low Cu/SiCN wafer level hybrid bonding
21. K. Onishi, H. Kitagawa, S. Teranishi, A. Uedono, F. Inoue, “Temporary Direct Bonding by Low Temperature Deposited SiO2 for Chiplet Applications” DOI 10.1021/acsaelm.4c00114 (Accepted in ACS Applied Electronic Materials).
22. Bonding of silicon wafers for silicon‐on‐insulator10.1063/1.342443 ↗
23. Accurate characterization of wafer bond toughness with the double cantilever specimen10.1063/1.2828156 ↗
24. Analysis of crack propagation in double cantilever beam tests of multidirectional laminates10.1016/S0167-6636(02)00289-2 ↗
25. Quantification of wafer bond strength under controlled atmospheres10.35848/1347-4065/ac5e49 ↗
26. Steady-state measurement of wafer bonding cracking resistance10.1016/j.sna.2003.09.004 ↗
27. Measurement of bonding energy in an anhydrous nitrogen atmosphere and its application to silicon direct bonding technology10.1063/1.4716030 ↗
28. Robust measurement of bonding strength for wafer-to-wafer 3D integration
29. Double‐cantilever cleavage mode of crack propagation10.1063/1.1713430 ↗
30. Measuring the surface bonding energy: a comparison between the classical double-cantilever beam experiment and its nanoscale analog10.1063/1.5143843 ↗
31. Evaluation of GIC of a DCB specimen usin an anisotropic solution10.1520/CTR10278J ↗
32. Water stress corrosion in bonded structures10.1149/2.0031505jss ↗
33. Mechanisms for room temperature direct wafer bonding10.1063/1.4794319 ↗
34. Water stress corrosion study during bonding energy measurement
35. Young's modulus, shear modulus, and Poisson's ratio in silicon and germanium10.1063/1.1713863 ↗
36. What is the young's modulus of silicon?10.1109/JMEMS.2009.2039697 ↗
37. Void Formation mechanism related to particles during wafer-to-wafer direct bonding10.1149/2162-8777/ac7662 ↗
38. Origin of voids at the SiO2/SiO2 and SiCN/SiCN bonding interface using positron annihilation spectroscopy and Electron spin resonance
39. Adhesion energy and bonding wave velocity measurements10.1149/07509.0145ecst ↗