journal article·2024-05

A review on the wettability and residual stress of AMB AlN/metal joints

Lin Cheng, Shaohong Liu, Bowen Jiang, Limin Zhou, Hao Cui, Manmen Liu, Ming Wen, Chuanjun Wang, Wei Wang, Song Li, Xudong Sun

Publisher page

Abstract

Aluminum nitride (AlN) ceramics possess exceptional comprehensive properties in terms of thermal, electrical, and mechanical aspects. The joining of AlN ceramics with metals enables the full exploitation of the advantages offered by AlN ceramics. Brazing is the most employed method for joining AlN ceramics with metals. However, brazing AlN ceramics to metals is challenging due to the differences in chemical bonding and coefficient of thermal expansion (CTE) between these two materials. This review provides a summary of methods that enhance the wettability and alleviate the residual stress of active metal brazing (AMB) AlN/metal joints. Additionally, it discusses the causes of residual stress and various methods to detect and evaluate the magnitude and distribution of residual stress, with a focus on finite element method (FEM). Finally, it identifies the existing challenges and future directions for further enhancing the wettability and reliability of AMB AlN/metal joints.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Thermal management on IGBT power electronic devices and modules10.1109/ACCESS.2018.2793300 ↗
2. Studies on the Al2OC mesophase in synthesized AlN powder and its effects on properties of AlN ceramic substrates10.1016/j.ceramint.2020.05.195 ↗
3. Enhanced adhesion strength of silver paste on AlN ceramic substrate via sintered nano-CuO10.1016/j.ceramint.2020.12.080 ↗
4. Effect of Ti content on the wetting behavior of Sn0.3Ag0.7Cu/AlN system10.1016/j.matdes.2016.11.041 ↗
5. Brazing ZrB2-SiC ceramics to Ti6Al4V alloy with TiCu-based amorphous filler10.1016/j.jmapro.2017.10.021 ↗
6. Forming mechanism of the repairing process on clinched joint10.1016/j.jmapro.2019.12.025 ↗
7. Brazing ZrO2 ceramic to Ti–6Al–4V alloy using NiCrSiB amorphous filler foil: interfacial microstructure and joint properties10.1016/j.matchar.2013.04.009 ↗
8. Interfacial microstructure of diffusion-bonded SiC and Re with Ti interlayer10.1016/j.jallcom.2017.01.081 ↗
9. Characterization of fusion welded ceramics in the SiC-ZrB2-ZrC system10.1016/j.jeurceramsoc.2020.10.067 ↗
10. Microstructure and shear strength of the brazed joint of Ti(C,N)-based cermet to steel10.1007/s12598-010-0013-7 ↗
11. The brazing of Al2O3 ceramic and other materials10.1007/s00170-022-08789-x ↗
12. Research advances in joining processes of sapphire10.1007/s00170-022-09199-9 ↗
13. Microstructure evolution and mechanical properties of titanium/alumina brazed joints for medical implants
14. Wetting of SiC by Al-Ti alloys and joining by in-situ formation of interfacial Ti3Si (Al) C210.1016/j.jeurceramsoc.2018.04.025 ↗
15. Interfacial microstructure and joining properties of TiAl/Si3N4 brazed joints10.1016/j.msea.2011.05.079 ↗
16. Development of light composite materials with low coefficients of thermal expansion10.1179/026708300101508568 ↗
17. Interfacial microstructure and strengthening mechanism of BN-doped metal brazed Ti/SiO2-BN joints10.1016/j.jeurceramsoc.2012.10.017 ↗
18. The effect of Mo particles addition in Ag-Cu-Ti filler alloy on Ti (C, N)-based cermet/45 steel-brazed joints10.1007/s11665-018-3339-1 ↗
19. Wetting and spreading10.1103/RevModPhys.81.739 ↗
20. Adamson · 1990
21. Atkinson · 1998 · 1675
22. Liquid metal wettability and advanced ceramic brazing10.1016/j.jeurceramsoc.2007.07.021 ↗
23. Wetting under chemical equilibrium and nonequilibrium conditions10.1021/j100605a009 ↗
24. Dynamics of wetting in reactive metal/ceramic systems
25. Joining of SiO2 ceramic and TC4 alloy by nanoparticles modified brazing filler metal10.1016/j.cja.2019.03.040 ↗
26. Kassam · 2018
27. Constructing a heterogeneous interlayer in relieving the residual stresses for the AlN/Cu brazed joint used in IGBT
28. Reactions and microstructure at selected ceramic/metal interfaces10.1080/10426919408934924 ↗
29. Microstructure and mechanical properties of AlN/Cu brazed joints10.1007/s11665-014-1120-7 ↗
30. Wettability and interfacial reactions for AlN/CuTi and AlN/SnTi systems10.1016/j.ceramint.2011.08.037 ↗
31. Active brazing of C/C composite to copper by AgCuTi filler metal10.1007/s11661-016-3340-y ↗
32. Investigation on viscosity, surface tension and non-reactive wettability of melting Ag-Cu-Xwt% Ti active filler metals10.1016/j.jallcom.2018.09.186 ↗
33. First-principles calculations of the effects of the interface microstructure on the wettability of a Cu–Ti/AlN system10.1016/j.ceramint.2021.03.188 ↗
34. Reaction kinetics and mechanical properties in the reactive brazing of copper to aluminum nitride10.1007/s10853-006-0920-z ↗
35. Investigation on wetting behavior and mechanism of AgCu-Xwt.% Ti filler metal/AlN ceramic reactive wetting system: experiments and first-principles calculations10.1016/j.jallcom.2021.159323 ↗
36. Review of non-reactive and reactive wetting of liquids on surfaces10.1016/j.cis.2007.04.009 ↗
37. The role of reactivity in wetting by liquid metals: a review10.1007/s10853-015-9331-3 ↗
38. Wetting transition in a molten metal and solid substrate system in high magnetic fields10.1007/s11661-020-05706-3 ↗
39. Wetting of TiN by liquid copper
40. Ru · 2011 · 311
41. Investigation of the direct plating copper (DPC) on Al2O3, BeO or AlN ceramic substrates for high power density applications10.4071/isom-2016-TP43 ↗
42. High thermal conductive AlN substrate for heat dissipation in high-power LEDs10.1016/j.ceramint.2018.09.171 ↗
43. Disclosing AlN ceramic substrate process failure mode and effect analysis10.1016/j.microrel.2019.113508 ↗
44. Yuan · 2013 · 3
45. Metal-ceramic interfaces: wetting and joining processes10.1504/IJMPT.2004.004780 ↗
46. Reactive wetting behavior and mechanism of AlN ceramic by CuNi-Xwt%Ti active filler metal10.1016/j.ceramint.2019.10.150 ↗
47. Wetting-bond strength relationship in Al-AlN system
48. Resistance of solid surfaces to wetting by water10.1021/ie50320a024 ↗
49. The spreading of a liquid over a rough solid10.1039/df9480300016 ↗
50. Some effects of substrate roughness on wettability10.1007/BF02402789 ↗
51. Effects of roughness on the wettability of high temperature wetting system10.1016/j.surfcoat.2015.12.092 ↗
52. Effect of temperature and surface roughness on the wettability of boron nitride by molten Al10.1007/s10853-007-1561-6 ↗
53. Wettability of aluminium nitride based ceramics of different porosity by two active silver based brazing alloys10.1016/j.msea.2004.02.021 ↗
54. Contact angle of 63Sn–37Pb and Pb-free solder on Cu plating10.1016/S0169-4332(03)00342-8 ↗
55. Nalagatla · 2007
56. Machine learning of metal-ceramic wettability10.1016/j.jmat.2021.03.014 ↗
57. Thermal properties and Young's modulus of Al-AlN composites10.1023/A:1010964430269 ↗
58. The regulation strategy for releasing residual stress in ceramic-metal brazed joints10.1016/j.jmapro.2022.12.022 ↗
59. Research advances in residual thermal stress of ceramic/metal brazes10.1016/j.ceramint.2021.04.220 ↗
60. Recent advances in active metal brazing of ceramics and process10.1007/s12540-019-00536-4 ↗
61. Thermal residual stress analysis of epoxy bi-material laminates and bonded joints10.1016/j.ijadhadh.2010.03.009 ↗
62. Fabrication of reliable ZTA composite/Ti6Al4V alloy joints via vacuum brazing method: microstructural evolution, mechanical properties and residual stress prediction10.1016/j.jeurceramsoc.2021.02.043 ↗
63. Methods of measuring residual stresses in components10.1016/j.matdes.2011.08.022 ↗
64. Residual stress analysis and measurement in multi-layer bellows10.1016/j.jmapro.2021.10.021 ↗
65. Measurement of residual stress in arc welded lap joints by cosα X-ray diffraction method10.1016/j.jmatprotec.2016.12.021 ↗
66. Experimental methods in chemical engineering: X‐ray diffraction spectroscopy—XRD10.1002/cjce.23747 ↗
67. Investigation of the residual stress in UO2-Mo composites via a neutron diffraction method10.1016/j.ceramint.2020.03.137 ↗
68. Feasibility of early fatigue damage evaluation using the Neutron diffraction method10.1016/j.engfailanal.2022.106603 ↗
69. A neutron diffraction study of residual stress due to welding10.1016/j.jmatprotec.2005.02.092 ↗
70. Numerical study of the effect of yield strain and stress ratio on the measurement accuracy of biaxial residual stress in steels using indentation10.1016/j.jmrt.2020.02.021 ↗
71. Investigation of surface residual stress distribution in deformation machining process for aluminum alloy10.1016/j.jmatprotec.2015.05.025 ↗
72. Residual strains of aluminum alloy characterized by nanoindentation10.1016/S1003-6326(10)60148-3 ↗
73. Recent advances in brazing fillers for joining of dissimilar materials10.3390/met11071037 ↗
74. Improvement and validation of residual stress measurement in composite laminates using the incremental hole-drilling method10.1016/j.mechmat.2020.103715 ↗
75. Measurement of residual stress in thermal spray coatings by the incremental hole drilling method10.1016/j.surfcoat.2006.04.056 ↗
76. Novel residual stress measurement technique to evaluate through thickness residual stress fields10.1016/j.matlet.2020.128347 ↗
77. Cross-sectional mapping of residual stresses by measuring the surface contour after a cut10.1115/1.1345526 ↗
78. Evaluation of residual stresses relaxation by post weld heat treatment using contour method and X-ray diffraction method10.1007/s11340-015-0040-2 ↗
79. Measurement of residual stresses in submerged arc welded P91 steel using surface deformation10.1016/j.matpr.2019.12.049 ↗
80. Thermal ratchetting effect of AMB-AlN ceramic substrate: experiments and calculations10.1016/j.ceramint.2019.04.186 ↗
81. Microstructure and mechanical properties of Si3N4/42CrMo joints brazed with TiNp modified active filler10.1016/j.ceramint.2013.12.008 ↗
82. The dependence of microstructure and mechanical properties on substrate heat treatment in AlN ceramics/AgCuTi/316 stainless steel brazed joints10.1016/j.vacuum.2023.112094 ↗
83. Finite element analysis of the effect of TiC or graphite modified composite fillers on the thermal residual stress of AMB ceramic substrates10.1016/j.ceramint.2019.06.155 ↗
84. Characterization of the residual stresses and strength of ceramic-metal braze joints10.1115/1.3078305 ↗
85. Thermo-mechanical reliability assessment of AlN power substrates subjected to severe aging tests10.1166/mat.2017.1413 ↗
86. Residual stress and warpage of AMB ceramic substrate studied by finite element simulations10.1016/j.microrel.2019.04.025 ↗
87. Numerical analysis on the residual stress distribution and its influence factor analysis for Si3N4/42CrMo brazed joint10.1016/j.simpat.2019.04.007 ↗
88. Effect of additional elements in Ag-Cu based filler metal on brazing of aluminum nitride to metals10.2355/isijinternational.30.1135 ↗
89. Bonding of aluminum nitride to copper for reducing thermal stress10.2320/matertrans1989.35.910 ↗
90. Joining of AlN to Cu using In-base active brazing fillers10.1557/JMR.1997.0146 ↗
91. Fabrication of 3D metal-ceramic (Al-AlN) architectures using laser-powder bed fusion process
92. AlN/Cu composite ceramic substrate fabricated using a novel TiN/AgCuTi composite brazing alloy10.1016/j.jeurceramsoc.2020.07.060 ↗
93. Vacuum brazing of AlON and Ti2AlNb with LiAlSiO4 enhanced Ag–Cu–Ti composite fillers: microstructure, mechanical properties and measurement of residual stress10.1016/j.msea.2022.143277 ↗
94. Microstructures and properties of Ag–Cu–Ti–In composite fillers for electronic packaging applications10.1007/s10854-019-01507-6 ↗
95. Brazing SiO2-BN diphase ceramic with Nb by using multilayer Ti-Ni composite foils10.1016/j.vacuum.2017.09.022 ↗
96. Strain energy release in ceramic-to-metal joints with patterned interlayers10.1016/j.scriptamat.2003.09.055 ↗
97. Brazing of doped graphite to Cu using stress relief interlayers10.1016/j.jmatprotec.2008.06.021 ↗
98. Active brazing carbon/carbon composite to TC4 with Cu and Mo composite interlayers10.1016/j.msea.2009.06.049 ↗
99. High shear strength Kovar/AlN joints brazed with AgCuTi/Cu/AgCuTi sandwich composite filler10.1016/j.msea.2022.144435 ↗
100. Active brazed Invar-SiO2f/SiO2 joint using a low-expansion composite interlayer10.1016/j.jmatprotec.2017.11.058 ↗