Optimization of Cu protrusion of wafer-to-wafer hybrid bonding for HBM packages application
Source abstract
Abstract
This work focuses on the effect of Cu protrusion on the reliability of High Bandwidth Memory (HBM) fabricated by wafer-to-wafer hybrid bonding (W2W-HB) process. The thermal stress induced by large coefficient of thermal expansion (CTE) mismatch between different materials could seriously deteriorate the device performance, and even lead to failure. Different manufacturing and service conditions could greatly affect the microstructure and deformation behavior of the through silicon via (TSV). In this paper, a new process was designed to realize the self-compensation of the surface topology by rationally utilizing the dishing defects caused by CMP . The influence of dielectric materials (dielectric layer thickness and CTE) on Cu protrusion height was systematically explored. A finite element analysis (FEA) model was proposed to provide insight into the Cu protrusion mechanism under different operating conditions. Annealing tests were carried out to identify how the microstructure affects protrusion and to verify the accuracy of the model. During the test, the extruded TSV was observed using scanning electron microscopy (SEM) and atomic force microscopy (AFM). Mechanisms of Cu protrusion in TSVs during heat treatment were analyzed, and possible factors involving thermal stress were discussed through the model. In addition, debonding risk was evaluated by comparing the peak interfacial peeling stress and the protrusion height for various scenarios. The conclusions can be used to understand and solve the key issues in the reliability challenges of HBM W2W-HB stacking process by enabling high-throughput TSV fabrication.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: 3D IC and TSV technologies · Electronic Packaging and Soldering Technologies · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. 21-Layer 3-D chip stacking based on Cu-Sn bump bonding10.1109/TCPMT.2015.2418274 ↗
2. Three-dimensional hybrid integration technology of CMOS, MEMS, and photonics circuits for optoelectronic heterogeneous integrated systems10.1109/TED.2010.2099870 ↗
3. Wafer-to-Wafer hybrid bonding development by advanced finite element modeling for 3-D IC packages10.1109/TCPMT.2020.3035652 ↗
4. A reliable Cu-Sn bonding technology for 3D-TSV packaging10.1088/0268-1242/29/2/025003 ↗
5. The experimental analysis and the mechanical model for the debonding failure of TSV-Cu/Si interface
6. Effect of Cu TSV annealing on via protrusion for TSV wafer fabrication10.1007/s11664-012-2117-3 ↗
7. Characterization of thermal stresses in through-silicon vias for three-dimensional interconnects by bending beam technique10.1063/1.3678020 ↗
8. Cu anisotropy effects in three-dimensional integrated circuits using through-silicon vias10.1109/TDMR.2012.2189401 ↗
9. Modeling stress in silicon with TSVs and its effect on mobility10.1109/TCPMT.2011.2158002 ↗
10. Failure analysis of through-silicon vias in free-standing wafer under thermal-shock test10.1016/j.microrel.2012.06.140 ↗
11. Protrusion of electroplated Cu filled in through silicon vias during annealing process10.1016/j.microrel.2016.04.005 ↗
12. Measurement and analysis of thermal stresses in 3D integrated structures containing through-silicon-vias10.1016/j.microrel.2012.05.008 ↗
13. Optimization for warpage and residual stress due to reflow process in IGBT modules based on pre-warped substrate10.1016/j.mee.2015.04.019 ↗
14. Reliability challenges in 3D IC packaging technology10.1016/j.microrel.2010.09.031 ↗
15. Reliability of TSV interconnects: electromigration, thermal cycling, and impact on above metal level dielectric10.1016/j.microrel.2012.06.021 ↗
16. Analysis of the electrical characteristics and structure of Cu-filled TSV with thermal shock test10.1007/s13391-013-3260-6 ↗
17. Evaluation of interfacial fracture toughness of a flip-chip package and a bimaterial system by a combined experimental and numerical method10.1016/S0013-7944(99)00078-8 ↗
18. Rebhan · 2015 · 2
19. Kim · 2016 · 1179
20. Interface and reliability analysis of Au-passivated Cu–Cu fine-pitch thermocompression bonding for 3-D IC applications10.1109/TCPMT.2019.2912891 ↗
21. Study on Cu protrusion of through-silicon via10.1109/TCPMT.2013.2252955 ↗
22. Reliability challenges related to TSV integration and 3-D stacking10.1109/MDAT.2015.2501302 ↗
23. Interfacial effects during thermal cycling of Cu-filled through-silicon vias (TSV)10.1007/s11664-011-1726-6 ↗
24. Overview and outlook of through-silicon via (TSV) and 3D integrations10.1108/13565361111127304 ↗
25. Study on Cu protrusion of through-silicon via in a 3D integrated circuit10.1016/j.msea.2019.03.130 ↗
26. The effect of the diffusion creep behavior on the TSV-Cu protrusion morphology during annealing
27. Characterizing interfacial sliding of through-silicon-via by nano-indentation10.1109/TDMR.2017.2681580 ↗
28. Jourdon · 2018 · 1
29. Dishing-radius model of Cu CMP dishing effects10.1109/TSM.2005.845110 ↗
30. Thermomechanical finite element modeling of Cu–SiO2 direct hybrid bonding with a dishing effect on Cu surfaces10.1016/j.ijsolstr.2016.02.041 ↗
31. Shames · 2014
32. Stress analysis in silicon die under different types of mechanical loading by finite element method (FEM)10.1109/TADVP.2002.807561 ↗
33. Idris · 2017
34. Initiation of free-edge delamination in composite laminates10.4028/www.scientific.net/KEM.37.103 ↗
35. Surface action mechanism and design considerations for the mechanical integrity of Cu/lowK BEOL interconnect during chemical mechanical polishing process10.1016/j.microrel.2022.114565 ↗
36. A view on annealing behavior of Cu-filled through-silicon vias (TSV)
37. Cu protrusion of different through-silicon via shapes under annealing process10.1007/s11665-021-05775-4 ↗