Investigation on critical crack-free cutting depth for single crystal silicon slicing with fixed abrasive wire saw based on the scratching machining experiments
Source abstract
Abstract
Abstract The experimental research of single crystal silicon scratching machining is crucial for micro component machining, precision grinding and fixed abrasive wire saw precision slicing of single crystal silicon. The fixed abrasive wire saw slicing is the main slicing technology of large diameter single crystal silicon slicing process. During the fixed abrasive wire saw slicing process, the brittle material removal mode results in micro crack damage in wafer surface layer, which reduces the strength of sliced silicon wafer, and restricts silicon wafer thinner. The crack-free slicing surface could be obtained while the material is in ductile removal mode. In this study, the scratching machining experiments with the Nano Indenter and Berkovich diamond indenter scratching on single crystal silicon (100) plane along [010] orientation is conducted. The constant normal force 20 mN, 100 mN, and varied normal force from 0 mN to 50 mN are applied on the Berkovich indenter. The material removal mode is mainly in ductile regime while 20 mN constant normal force, and the material removal mode is mainly in brittle regime and cleavage fracture emerge while 100 mN constant normal force. The tangential friction force of scratching machining process changes from smooth to fluctuate when the varied normal force from 0 mN to 50 mN, and material removal mode from ductile regime to brittle regime. The critical normal force of ductile transition to brittle is 26 mN. However, the scratching machining experimental results near the ductile regime removal mode show that the scratch exists obvious elastic recovery. The elastic recovery of scratch affects the material removal amount and machining accuracy. Based on the scratching machining experimental results, the critical crack-free cutting depth per abrasive for single crystal silicon slicing with fixed abrasive wire saw is analyzed. The results in this paper are useful for the single crystal silicon micro component machining and slicing process parameters selection of fixed abrasive wire saw.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Surface Polishing Techniques · Advanced machining processes and optimization · Tunneling and Rock Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. 450mm silicon wafers challenges-wafer thickness scaling10.1149/1.2980288 ↗
2. A scratching force model of diamond abrasive particles in wire sawing of single crystal SiC10.1016/j.mssp.2017.05.032 ↗
3. Prediction of sawing force for single-crystal silicon carbide with fixed abrasive diamond wire saw10.1016/j.mssp.2017.01.014 ↗
4. Experiment study on electroplated diamond wire saw slicing single- crystal silicon10.1016/j.mssp.2016.08.003 ↗
5. On the nature and removal of saw marks on diamond wire sawn multicrystalline silicon wafers10.1016/j.mssp.2014.06.049 ↗
6. Depth of cut per abrasive in fixed diamond wire sawing10.1007/s00170-015-7089-z ↗
7. Deformation and removal characteristics in nanoscratching of 6H-SiC with Berkovich indenter10.1016/j.mssp.2014.11.034 ↗
8. Subsurface damage properties of nano scratches in fused silica optics
9. Material removal mechanism and grinding force modelling of ultrasonic vibration assisted grinding for SiC ceramics10.1016/j.ceramint.2016.11.066 ↗
10. Subsurface crack damage in silicon wafers induced by resin bonded diamond wire sawing10.1016/j.mssp.2016.10.021 ↗
11. Experimental study of surface performance of monocrystalline 6H-SiC substrates in plane grinding with a metal-bonded diamond wheel10.1007/s00170-016-9095-1 ↗
12. Surface characterization of 6H-SiC (0001) substrates in indentation and abrasive machining10.1016/j.ijmachtools.2003.12.006 ↗
13. Nanogrinding of SiC wafers with high flatness and low subsurface damage10.1016/S1003-6326(11)61566-5 ↗
14. An experimental and theoretical investigation on the brittle ductile transition and cutting force anisotropy in cutting KDP crystal10.1016/j.ijmachtools.2016.04.009 ↗
15. Crystallographic effect on subsurface damage formation in silicon microcutting10.1016/j.cirp.2012.03.070 ↗
16. Surface integrity and removal mechanism of silicon wafers in chemo-mechanical grinding using a newly developed soft abrasive grinding wheel10.1016/j.mssp.2017.02.001 ↗
17. Burghartz · 2011
18. Research on the factors limiting to reduce the thickness of silicon wafers
19. Manufacturing 100-µm-thick silicon solar cells with efficiencies greater than 20% in a pilot production line10.1002/pssa.201431241 ↗
20. Integrated process for silicon wafer thinning
21. Raman microspectroscopy study of processing-induced phase transformations and residual stress in silicon10.1088/0268-1242/14/10/310 ↗
22. Three-dimensional shape modeling of diamond abrasive grains measured by a scanning laser microscope10.4028/www.scientific.net/KEM.238-239.131 ↗
23. Depth of cut for single abrasive and cutting force in resin bonded diamond wire sawing10.1007/s00170-016-8896-6 ↗
24. A finite element analysis of sawing stress in fixed-abrasive wiresaw slicing KDP crystal10.1007/s00170-016-9916-2 ↗