Tin–lead (SnPb) solder reaction in flip chip technology
Source abstract
Abstract
Solder reactions between SnPb and one of the four metals, Cu, Ni, Au, and Pd have been reviewed on the basis of the available data of morphology, thermodynamics, and kinetics. The reactions on both bulk and thin film forms of these metals have been considered and compared. Also the two kinds of reactions, above and below the melting point of the solder, have been considered and compared. The rate of intermetallic compound formation in wetting reactions between the molten solder and the metals is three to four orders of magnitude faster than those between the solid state solder and the metals. The rate is controlled by the morphology of intermetallic compound formation. In the wetting reaction between molten SnPb and Cu or Ni, the intermetallic compound formation has a scallop-type morphology, but in solid state aging, it has a layer-type morphology. There are channels between the scallops, which allow rapid diffusion and rapid rate of compound formation. In the layer-type morphology, the compound layer itself becomes a diffusion barrier to slow down the reaction. Similar morphological changes occur between SnPb and Au or Pd. The stability of scallop-type morphology in wetting reaction and layer-type morphology in solid state aging have been explained by minimization of surface and interfacial energies. The unusually high rate of scallop-type intermetallic compound formation has been explained by the gain of rate of free energy change rather than free energy change. Also included in the review is the use of a stack of thin films as under-bump-metallization, such as Cr/Cu/Au, Al/Ni(V)/Cu, and Cu/Ni alloyed thin films.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. International Roadmap for Semiconductor Technology, Semiconductor Industry Association, San Jose, CA, 1999.
2. Solid logic technology: versatile, high performance microelectronics10.1147/rd.441.0056 ↗
3. Controlled collapse reflow chip joining10.1147/rd.133.0239 ↗
4. SLT device metallurgy and its monolithic extensions10.1147/rd.133.0226 ↗
5. K. Puttlitz, P. Totta, Area Array Technology Handbook for Microelectronic Packaging, Kluwer Academic Publishers, Norwell, MA, 2001.10.1007/978-1-4615-1389-6 ↗
6. L.F. Miller, Silver palladium fired electrodes, in: Proceedings of the IEEE Electronic Compound Conference, IEEE, New York, NY, 1968, p. 52.
7. V.C. Marcotte, N.G. Koopman, Palladium depletion of 80Ag20Pd thick film electrodes, in: Proceedings of the IEEE 31st Electronic Compound Conference, IEEE, New York, NY, 1981, pp. 157–164.
8. Thin film reactions of Pb with AgAu and AgPd alloys10.1063/1.322047 ↗
9. G. DiGiacomo, J. Gniewek, J. Rizzto, W. Rosenberg, AuAgPd ternary alloy for thick film electrodes, in: Proceedings of the IEEE 32nd Electronic Compound Conference, IEEE, New York, 1982, pp. 354–356.10.1109/TCHMT.1982.1136012 ↗
10. Kinetics of thin film reactions between Pb and AgPd alloys10.1063/1.324182 ↗
11. Y. Taguma, T. Uda, H. Ishida, T. Kobayashi, K. Nakada, Application of dc magnetron sputtered Cr–Cu–Au thin film for flip chip solder terminal contacts, in: Proceedings of the 1991 International Electronic Packaging Conference, Vol. 1, International Electronic Packaging Society, Wheaton, IL, 1991, pp. 619–633.
12. Microstructure of phase-in Cr–Cu/Cu/Au bump-limiting-metallization and its soldering behavior with high Pb and eutectic SnPb solders10.1063/1.120224 ↗
13. Three-dimensional morphology of a very rough interface formed in the soldering reaction between eutectic SnPb and Cu10.1063/1.113975 ↗
14. Kinetic analysis of the soldering reaction between eutectic SnPb alloy and Cu accompanied by ripening10.1103/PhysRevB.53.16027 ↗
15. Spalling of Cu6Sn5 spheroids in the soldering reaction of eutectic SnPb on Cr/Cu/Au thin films10.1063/1.363728 ↗
16. Ripening-assisted asymmetric spalling of Cu–Sn compound spheroids in solder joints on Si wafers10.1063/1.116013 ↗
17. Size dependent dewetting and sideband reaction of eutectic SnPb on Au/Cu/Cr multilayered thin film10.1557/JMR.1998.0152 ↗
18. Metastable structures in metallurgy10.1007/BF02648333 ↗
19. Metastable phase formation in thin film reactions10.1016/0921-5093(91)90965-P ↗
20. Studies of SLT chip terminal metallurgy10.1147/rd.133.0286 ↗
21. Direct correlation between mechanical failure and metallurgical reaction in flip chip solder joints10.1063/1.369779 ↗
22. Interfacial morphology and shear deformation of flip chip solder joints10.1557/JMR.2000.0242 ↗
23. Microstructure–electromigration correlation in a thin stripe of eutectic SnPb solder stressed between Cu electrodes10.1063/1.124276 ↗
24. S. Brandenburg, S. Yeh, Electromigration studies of flip chip bump solder joints, in: Proceedings of the Surface Mount International Conference and Exposition, SMTA, Edina, MN, 1998, pp. 337–344.
25. Interface diffusion in eutectic Pb–Sn solder10.1016/S1359-6454(98)00348-6 ↗
26. Electric current effects upon the Sn/Cu and Sn/Ni interfacial reactions10.1007/s11664-998-0068-5 ↗
27. The growth of Cu–Sn intermetallics at a pretinned copper/solder interface10.1007/BF02665064 ↗
28. The formation of Cu3Sn intermetallic on the reaction of copper with 95Pb5Sn solder10.1007/BF02661885 ↗
29. L. Kaufman, H. Bernstein, Computer Calculation of Phase Diagrams, Academic Press, New York, 1970.
30. Algebraic representation of thermodynamic properties and the classification of solutions10.1021/ie50458a036 ↗
31. W.J. Boettinger, C.A. Handwerker, U.R. Kattner, Reactive wetting and intermetallic formation, in: F.G. Yost, F.M. Hosking, D.R. Frear (Eds.), The Mechanics of Solder Alloy Wetting and Spreading, Van Nostrand Reinhold, New York, 1993, pp. 103–140.10.1007/978-1-4684-1440-0_4 ↗
32. Thermodynamic study of phase equilibria in the Pb–Sn–Sb system10.1007/BF02645349 ↗
33. Thermodynamic assessment of the Cu–Sn system
34. A. Bolcavage, C.R. Kao, S.L. Chen, Y.A. Chang, Thermodynamic calculation of phase stability between copper and lead–indium solder, in: P. Nash, B. Sundman (Eds.), Proceedings of the Applications of Thermodynamics in the Synthesis and Processing of Materials, 2–6 October 1994, Rosemont, IL, USA, TMS, Warrendale, PA, 1995, pp. 171–185.
35. V.C. Marcotte, K. Schroeder, CuSnPb phase diagram, in: A.R. McGhie (Ed.), Proceedings of the 13th North American Thermal Analysis Society, North American Thermal Analysis Society, 1984, p. 294.
36. J.S. Kirkaldy, D.J. Young, Diffusion in the Condensed State, The Institute of Metals, London, 1987.
37. Thermodynamic considerations in the analysis of phase stability: the role of interfacial equilibrium in the determination of phase diagrams by X-ray microanalytical techniques10.1007/BF02869262 ↗
38. Second phase dissolution10.1007/BF02663326 ↗
39. A.D. Romig, Y.A. Chang, J.J. Stephens, D.R. Frear, V. Marcotte, C. Lea, Physical metallurgy of solder–substrate reactions, in: D.R. Frear, W.B. Jones, K.R. Kinsman (Eds.), EMPMD Monograph Series, Solder Mechanics — A State of the Art Assessment, Vol. 1, TMS, Santa Fe, New Mexico, 1991, pp. 29–104.
40. Use of multicomponent phase diagrams for predicting phase evolution in solder/conductor systems10.1007/s11664-001-0212-y ↗
41. The rule of Cu–Sn intermetallics in wettability degradation10.1007/BF02655460 ↗
42. Effect of solid state intermetallic growth on the fracture toughness of Cu/63Sn–37Pb solder joints
43. V.C. Marcotte K. Schroder, Cu–Pb–Sn ternary system: low Cu additions to Pb–Sn binary system, in: L.H. Bennett, T.B. Massalski, B.C. Giessen (Eds.), Proceedings of the Alloy Phase Diagrams, Vol. 19, November 1982, Boston, USA, Elsevier, New York, 1983, pp. 403–410.10.1557/PROC-19-403 ↗
44. Growth kinetics of planar binary diffusion couples: thin film case versus bulk cases10.1063/1.331028 ↗
45. Some aspects of the growth of diffusion layers in binary systems10.1016/0022-3115(61)90175-1 ↗
46. A theory of multiphase binary diffusion10.1016/0001-6160(76)90023-7 ↗
47. Analysis of thin film structures with nuclear backscattering and X-ray diffraction10.1116/1.1318668 ↗
48. Structure and growth kinetics of Ni2Si on silicon10.1016/0040-6090(75)90058-9 ↗
49. Thermal and ion-induced dissociation of NiSi and NiSi2 in contact with nickel10.1016/0040-6090(83)90033-0 ↗
50. First phase nucleation in silicon–transition metal planar interface10.1063/1.88590 ↗
51. R. Pretorius, Prediction of silicide first phase and phase sequence from heats of formation, in: Proceedings of the Thin Film and Interfaces II, November 1983, Boston, MA, USA, Elsevier, New York, USA, 1984, pp. 15–20.10.1557/PROC-25-15 ↗
52. Formation of an amorphous alloy by solid state reaction of the pure polycrystalline metals10.1103/PhysRevLett.51.415 ↗
53. Formation of an amorphous RhSi alloy by interfacial reaction between amorphous Si and crystalline Rh thin films10.1063/1.94014 ↗
54. Solid phase amorphization and crystallization in multilayer and bilayer RhSi thin films10.1016/0254-0584(93)90047-P ↗
55. Transmission electron microscopic observations of amorphous NiZr alloy formation by solid state reaction10.1063/1.96881 ↗
56. Interfacial reaction and wetting behavior in eutectic SnPb solder on Ni/Ti thin films and Ni foils10.1063/1.371751 ↗
57. Wetting reaction vs. solid state aging of eutectic SnPb on Cu10.1063/1.1357469 ↗
58. A study of solute diffusion in liquid tin10.1016/0001-6160(60)90008-0 ↗
59. T. Young, in: G. Peacock (Ed.), Miscellaneous Works, Vol. 1, Murray, London, 1855, p. 418.
60. Flow of simple liquids down narrow V grooves10.1103/PhysRevE.52.3967 ↗
61. Reactive flow of molten Pb(Sn) alloys in Si grooves coated with Cu film10.1103/PhysRevE.58.6308 ↗
62. Morphology of instability of the wetting tips of eutectic SnBi, eutectic SnPb, and pure Sn on Cu10.1557/JMR.1995.0497 ↗
63. Rapid soldering reactions of eutectic SnPb and eutectic SnBi on palladium surfaces10.1016/0956-716X(95)00095-D ↗
64. Fast dissolution and soldering reactions on Au foils10.1016/S0254-0584(97)02076-2 ↗
65. Thermodynamic modeling of the Ni–Pb–Sn system10.1007/s11661-999-0085-x ↗
66. P.W. Dehaven, The reaction kinetics of liquid 60/40 Sn/Pb solder with copper and nickel: a high temperature X-ray diffraction study, in: Proceedings of the Electronic Packaging Materials Science, 27–29 November 1984, Boston, MA, USA, Materials Research Society, USA, 1984, pp. 123–128.10.1557/PROC-40-123 ↗
67. R.J.K. Wassink, Soldering in Electronics, 2nd Edition, Electrochemical Publications Limited, Isle of Man, British Isles, 1989.
68. The interaction kinetics and compound formation between electroless Ni–P and solder10.1016/0040-6090(94)90761-7 ↗
69. C.-Y. Lee, K.-L. Lin, Bonding fracture mechanism between SnPb solder and electroless nickel alloy deposits, in: Proceedings of the International Intersociety Electronic Packaging Conference (INTERpack 95), Vol. 2, 26–30 March 1995, Maui, USA, American Society of Mechanical Engineers, New York, 1995, pp. 1081–1099.
70. Preparation of solder bumps incorporating electroless nickel–boron deposit and investigation on the interfacial interaction behavior and wetting kinetics10.1023/A:1018599609177 ↗
71. Solder reaction-assisted crystallization of electroless Ni–P under bump metallization in low cost flip chip technology10.1063/1.370627 ↗
72. Kinetics of interfacial reaction between eutectic SnPb solder and Cu/Ni/Pd metallizations10.1007/s11664-999-0163-2 ↗
73. D. Frear, F. Hosking, P. Vianco, Mechanical behavior of solder joint interfacial intermetallics, in: Proceedings of the Materials Developments in Microelectronic Packaging: Performance and Reliability, 19–22 August 1991, Montreal, Que., Canada, ASM International, Materials Park, OH, USA, 1991, pp. 229–240.
74. Dissolution of Au, Ag, Pd, Pt, Cu, and Ni in a molten tin–lead solder
75. Solder bump formation using electroless plating and ultrasonic soldering10.1109/33.52858 ↗
76. A.C. Harman, Rapid tin–nickel intermetallic growth: some effects on solderability, in: Proceeding of the InterNepcon, Brighton, UK, 1978, pp. 42–49.
77. Intermetallic compound growth in tin and tin–lead platings over nickel and its effects on solderability
78. Growth of intermetallic compounds on common basis material coated with tin or tin–lead alloys10.1080/00202967.1976.11870376 ↗
79. Morphology of interfacial reaction between Pb-free solders and electroless Ni(P) under-bump-metallization10.1063/1.1321787 ↗
80. Kinetic analysis of interfacial diffusion accompanied by intermetallic compound formation10.1063/1.370880 ↗
81. Ultrafast intermetallic compound formation between eutectic SnPb and Pd where the intermetallic is not a diffusion barrier10.1063/1.114467 ↗
82. T.B. Massalski, Binary Alloy Phase Diagrams, ASM International, OH, 1990.
83. Diffusion and phase transformations during interfacial reaction between lead–tin solders and palladium10.1007/s11664-998-0064-9 ↗
84. Interfacial microstructure and the kinetics of interfacial reaction in diffusion couples between SnPb solder and Cu/Ni/Pd metallization10.1016/S1359-6454(00)00165-8 ↗
85. Thermodynamic modeling of the Pd–Pb–Sn system10.1007/s11661-999-0191-9 ↗
86. Soldering reaction between eutectic SnPb and plated Pd/Ni thin films on Cu leadframe10.1063/1.120434 ↗
87. Time- and temperature-dependent wetting behavior of eutectic SnPb on Cu leadframes plated with Pd/Ni and Au/Pd/Ni thin films10.1063/1.368136 ↗
88. J.K. Kivilahti, K. Kulojärvi, A new reliability aspect related to high density interconnections, in: R.K. Mahidhara, D.R. Fear, et al. (Eds.), Proceedings of the Design and Reliability of Solders and Solder Interconnections, 10–13 February 1997, Orlando, FL, USA, Minerals, Metals and Materials Society/AIME, Warrendale, USA, 1997, pp. 377–384.
89. The Au–Pb–Sn ternary system10.1016/0022-5088(67)90094-X ↗
90. Morphology of wetting reaction of eutectic SnPb solder on Au foils10.1063/1.363336 ↗
91. Constitution of Au–AuSn–Pb partial ternary system10.1179/mst.1987.3.8.621 ↗
92. Diffusion controlled reactions in Au/Pb–Sn solder system10.1179/mst.1992.8.9.817 ↗
93. Reaction kinetics of solder balls with pads in BGA packages during reflow soldering10.1007/s11664-999-0162-3 ↗
94. Constitution of AuSn–Pb–Sn partial ternary system10.1179/mst.1985.1.6.433 ↗
95. K. Banerji, R.F. Darveaux, Effect of aging on the strength and ductility of controlled collapse solder joints, in: Proceedings of the 1st International Conference on Microstructures and Mechanical Properties of Aging Materials, 2–5 November 1992, Chicago, IL, USA, The Minerals, Metals and Materials Society/AIME, Warrendale, USA, 1993, pp. 431–442.
96. Z. Mei, M. Kaufmann, A. Eslambolchi, P. Johnson, Brittle interfacial fracture of PBGA packages soldered on electroless nickel/immersion gold, in: Proceedings of the 48th Electronic Components and Technology Conference, 25–28 May 1998, Seattle, Washington, USA, IEEE, Piscataway, USA, 1998, pp. 952–961.
97. Z. Mei, P. Callery, D. Fisher, F. Hua, J. Glazer, Interfacial fracture mechanism of BGA packages on electroless Ni/Au, in: Proceedings of the Pacific Rim/ASME International Intersociety Electronic and Photonic Packaging Conference, Vol. 2, Advances in Electronic Packaging 1997, ASME, New York, USA, 1997, pp. 1543–1550.
98. S.C. Hung, P.J. Zheng, S.C. Lee, J.J. Lee, The effect of Au plating thickness of BGA substrates on ball shear strength under reliability tests, in: Proceedings of the 24th IEEE/CPMT International Electronics Manufacturing Technology Symposium, 18–19 October 1999, Austin, USA, IEEE, Piscataway, USA, 1999, pp. 7–15.10.1109/IEMT.1999.804790 ↗
99. R. Erich, R.J. Coyle, G. M. Wenger, A. Primavera, Shear testing and failure mode analysis for evaluation of BGA ball attachment, in: Proceedings of the 24th IEEE/CPMT International Electronics Manufacturing Technology Symposium, 18–19 October 1999, Austin, USA, IEEE, Piscataway, USA, 1999, pp. 16–22.10.1109/IEMT.1999.804791 ↗
100. Formation and resettlement of (AuxSn1−x)Sn4 in solder joints of ball-grid-array packages with the Au/Ni surface finish10.1007/s11664-000-0010-y ↗